Localised corrosion susceptibility of nitrogen-containing type 316LN stainless steel in cold work and thermally aged conditions

被引:1
|
作者
Mannepalli, Srinivas [1 ,2 ]
Shankar, A. Ravi [1 ,2 ]
Ningshen, S. [1 ,2 ]
Philip, John [1 ,2 ]
机构
[1] Indira Gandhi Ctr Atom Res, Corros Sci & Technol Div, Met & Mat Grp, Kalpakkam 603102, Tamil Nadu, India
[2] HomiBhaba Natl Inst, Kalpakkam 603102, Tamil Nadu, India
关键词
316LN SS; cold work; electrochemical impedance spectroscopy; DLEPR; pitting corrosion; PITTING CORROSION; SENSITIZATION; BEHAVIOR; PRECIPITATION;
D O I
10.1080/1478422X.2022.2126407
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present paper, an investigation was carried out to understand the microstructure or secondary phase changes formed during thermal ageing at nose temperature (where Cr diffusion was faster) and its influence on the pitting corrosion behaviour of type 316LN SS with marginally lower Cr in as-received (AR) and 10% cold work (CW). X-ray diffraction studies confirmed Cr23C6 and Cr2N in AR and CW conditions. On thermal ageing, AR material from 0 to 10 h and CW from 10 to 24 h, although with lower Cr, the degree of sensitisation (DOS) and pitting potential (E-pit) were insignificant due to nitrogen where as above 10 h in AR condition and below 10 h in CW condition resulted reductions in pitting potential (E-pit) in different chloride mediums. These results provide new insights on the interplay between pitting, microstructures, alloying elements.
引用
收藏
页码:762 / 773
页数:12
相关论文
共 50 条
  • [21] Fracture toughness of type 316LN stainless steel welded joints
    Gao, Wenhua
    Chen, Kai
    Guo, Xianglong
    Zhang, Lefu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 685 : 107 - 114
  • [22] Effect of Nitrogen and Sensitization on the Microstructure and Pitting Corrosion Behavior of AISI Type 316LN Stainless Steels
    Poonguzhali, A.
    Pujar, M. G.
    Mudali, U. Kamachi
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2013, 22 (04) : 1170 - 1178
  • [23] Effect of Nitrogen and Sensitization on the Microstructure and Pitting Corrosion Behavior of AISI Type 316LN Stainless Steels
    A. Poonguzhali
    M. G. Pujar
    U. Kamachi Mudali
    Journal of Materials Engineering and Performance, 2013, 22 : 1170 - 1178
  • [24] Clustering and ordering of nitrogen in nuclear grade 316LN austenitic stainless steel
    Shankar, P
    Sundararaman, D
    Ranganathan, S
    JOURNAL OF NUCLEAR MATERIALS, 1998, 254 (01) : 1 - 8
  • [25] Influence of Cold Work on Sensitization Kinetics and Evaluation of Degree of Sensitization in Type 316LN Stainless Steels
    Srinivas, M.
    George, R. P.
    Mallika, C.
    Mudali, U. Kamachi
    CORROSION, 2017, 73 (10) : 1213 - 1223
  • [26] Hot deformation behavior of a Nb-containing 316LN stainless steel
    Zhang Wenhui
    Sun Shuhua
    Zhao Deli
    Wang Baozhong
    Wang Zhenhua
    Fu Wantang
    MATERIALS & DESIGN, 2011, 32 (8-9): : 4173 - 4179
  • [27] Hydrogen effects on pitting corrosion and semiconducting properties of nitrogen-containing type 316L stainless steel
    Ningshen, S.
    Mudali, U. Kamachi
    ELECTROCHIMICA ACTA, 2009, 54 (26) : 6374 - 6382
  • [28] Electrolyte and temperature effects on pitting corrosion of type 316LN stainless steels
    Ningshen, S
    Mudali, UK
    Dayal, RK
    BRITISH CORROSION JOURNAL, 2001, 36 (01): : 36 - 41
  • [29] Effect of grain size on creep properties of type 316LN stainless steel
    Lee, YS
    Kim, DW
    Lee, DY
    Ryu, WS
    METALS AND MATERIALS-KOREA, 2001, 7 (02): : 107 - 114
  • [30] Effect of grain size on creep properties of type 316LN stainless steel
    Yo Seob Lee
    Dae Whan Kim
    Dok Yol Lee
    Woo Seog Ryu
    Metals and Materials International, 2001, 7 : 107 - 114