关键词
fracture toughness; strength; deformation; Al2O3/YAG composite; ultra high temperature;
D O I
10.1016/S0266-3538(01)00159-2
中图分类号
TB33 [复合材料];
学科分类号
摘要
The deformation and fracture behavior of a newly developed Al2O3/YAG composite, fabricated by the unidirectional solidification of a eutectic composition, was investigated by means of bending tests between room temperature and 2023 K, on specimens whose longitudinal directions were parallel (L specimen) and perpendicular (T specimen) to the direction of solidification. At low temperatures, the composite fractured in a brittle manner at all displacement speeds. At high temperatures, it fractured in a brittle manner at high displacement speed, but in a ductile manner with accompanying plastic deformation at low speed for both L and T specimens. The brittle-ductile transition temperature became higher at higher displacement speeds in both L and T specimens, while it was slightly higher in the latter specimen. The crack propagated dominantly through YAG with lower ductility than Al2O3, as a consequence of which the fraction of YAG in the fracture surface was higher than the structural value estimated from a polished surface. The strength at room temperature of both L and T specimens was maintained up to 2023 K at high displacement speeds. At low displacement speeds, the strength decreased beyond 1900 K as a result of the enhanced plastic deformation. The stress exponent for plastic deformation at high temperatures (1823-2023 K) was 5-6, suggesting that the plastic deformation is controlled by a dislocation mechanism during bending as well as in compressive and tensile loading. The fracture toughness tended to increase with increasing temperature and with decreasing displacement speed, especially in L specimens. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2117 / 2128
页数:12
相关论文
共 50 条
  • [22] Wear behavior of lanxide Al2O3/Al composite
    Zhang, J
    Zhu, DG
    Yang, L
    Li, SZ
    WEAR, 1998, 215 (1-2) : 34 - 39
  • [23] Tensile deformation behavior of a sub-micrometer Al2O3/6061Al composite
    Zhang, Qiang
    Wu, Gaohui
    Jiang, Longtao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 483-84 (281-284): : 281 - 284
  • [24] Microstructure and Tribocorrosion Behavior of Al2O3/Al Composite Coatings: Role of Al2O3 Addition
    Jiangbo Cheng
    Yunyun Ge
    Bishi Wang
    Lianhua Zhang
    Xianlong Hu
    Shen Hong
    Xiubing Liang
    Xiancheng Zhang
    Journal of Thermal Spray Technology, 2020, 29 : 1741 - 1751
  • [25] Crack healing behavior of monolithic Al2O3 and Al2O3-SiCw composite at high temperature
    Subiantoro
    Akatsu, T
    Tanabe, Y
    Yasuda, E
    TIME DEPENDENT MECHANICAL RESPONSE OF ENGINEERING CERAMICS: FROM PICO-SECOND TO MILLION YEARS, 1999, 4 : 125 - 130
  • [26] Crack healing behavior of monolithic Al2O3 and Al2O3-SiCw composite at high temperature
    Materials and Structures Laboratory, Tokyo Institute of Technology, 4259, Nagatsuta, Midori, Yokohama 226-8503, Japan
    Key Eng Mat, (125-130):
  • [27] Fracture behavior of laser zone-remelted metastable eutectic Al2O3/YAG/ZrO2 in-situ composite
    Su, Haijun
    Zhang, Jun
    Liu, Lin
    Fu, Hengzhi
    ENGINEERING STRUCTURAL INTEGRITY: RESEARCH, DEVELOPMENT AND APPLICATION, VOLS 1 AND 2, 2007, : 1074 - 1077
  • [28] High Temperature Internal Friction Behavior of Unidirectionally Solidified Al2O3/YAG Eutectic
    Ueno, Shunkichi
    Takata, Satoshi
    Tanabe, Yasuhiro
    Akatsu, Takashi
    Yasuda, Eiichi
    Waku, Yoshiharu
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 2482 - +
  • [29] Internal friction behavior of an unidirectionally solidified Al2O3/YAG eutectic at high temperature
    Takata, Satoshi
    Ueno, Shunkichi
    Tanabe, Yasuhiro
    Akatsua, Takashi
    Yasuda, Eiichi
    Waku, Yoshiharu
    CERAMICS INTERNATIONAL, 2007, 33 (08) : 1569 - 1571
  • [30] Acetone detection at room temperature by chemical sensors based on PVDF/Al2O3 composite
    Devikala, S.
    Kamaraj, P.
    Arthanareeswari, M.
    JOURNAL OF THE INDIAN CHEMICAL SOCIETY, 2019, 96 (01) : 131 - 132