Coupled growth behavior in the rapidly solidified Ti-Al peritectic alloys

被引:26
|
作者
Liu, YC
Yang, GC
Guo, XF
Huang, J
Zhou, YH
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
[2] Xian Inst Technol, Coll Mat Sci & Engn, Xian 710048, Peoples R China
基金
中国国家自然科学基金;
关键词
rapid solidification; coupled growth; peritectic reaction; phase selection; Ti-Al alloy;
D O I
10.1016/S0022-0248(00)00946-5
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
Laser melting technology, an ultra-high-temperature gradient direction solidification process, has been, adopted on near equal atomic percent Ti+Al peritectic alloys with an effort to achieve the two-phase coupled growth structure. Both the alloy composition range and its local solidification parameters were determined by means of mathematical calculation of local solidification parameters in the melt pool. X-ray, SEM, TEM and optical microscopy techniques were carried out to investigate the microstructure and identify the phase composition. The two-phase (alpha and gamma) coupled growth morphology under conditions of high growth velocity and high-temperature gradient was first detected in the laser resolidified Ti-Al peritectic alloys. The aluminum composition range appearing in the coupled growth of alpha and gamma phases, lies in Ti-(51.0-54.0)at% Al, a little shift towards the left direction of the hypoperitectic plateau. Microstructural analysis showed that the coupled growth morphology changed from regular lamellar, irregular blocks and equiaxed structures in sequence, with the temperature gradient decreasing during growth. Energy spectrum analysis results showed that not only the solute diffusion but also the dissolution of phase gamma played an important role in the coupled structure evolution. Rapid eutectic growth KT model (Kurz, Trivedi, Metall Trans. A 22(1991) 3051) could be used effectively to predict the characteristic lamellar spacing of two-phase coupled, structures in TI-AI peritectic alloys. The transformation from a peritectic, L + alpha --> gamma, to metastable eutectic reaction, L --> alpha + gamma, of near equal atomic percent Ti-Al peritectic alloys, induced the formation of two-phase coupled growth morphologies. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:645 / 654
页数:10
相关论文
共 50 条
  • [21] Structure and properties of rapidly solidified Al-Zr-Ti alloys
    P. Málek
    M. JaneČek
    B. Smola
    P. BartuŠka
    J. PleŠtil
    Journal of Materials Science, 2000, 35 : 2625 - 2633
  • [22] Combined Effects of High Undercooling and Large Cooling Rate on the Microstructure Evolution and Hardening Mechanism of Rapidly Solidified Ti-Al Alloys
    Z. C. Luo
    H. P. Wang
    Metallurgical and Materials Transactions A, 2020, 51 : 1242 - 1253
  • [23] Combined Effects of High Undercooling and Large Cooling Rate on the Microstructure Evolution and Hardening Mechanism of Rapidly Solidified Ti-Al Alloys
    Luo, Z. C.
    Wang, H. P.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2020, 51 (03): : 1242 - 1253
  • [24] MICROSTRUCTURES OF RAPIDLY SOLIDIFIED TI-AL-LI AND TI-MG ALLOYS
    SASTRY, SML
    ONEAL, JE
    PENG, TC
    JOURNAL OF METALS, 1985, 37 (11): : A98 - A98
  • [25] OXIDATION OF TI-AL ALLOYS
    KAHVECI, AI
    WELSCH, G
    WASIELEWSKI, GE
    JOURNAL OF METALS, 1988, 40 (07): : A49 - A49
  • [26] OXIDATION OF TI-AL ALLOYS
    KAHVECI, AI
    LIU, Z
    WELSCH, G
    WASIELEWSKI, G
    JOURNAL OF METALS, 1987, 39 (07): : A7 - A7
  • [27] Microstructure of rapidly solidified Ti-Al-V and Ti-Al-Si-V alloys
    Jazayeri-G, A
    Davies, HA
    Buckley, RA
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 375 : 512 - 515
  • [28] Electrical property of rapidly solidified Co-Cu peritectic alloys
    Xu, JF
    Wei, BB
    ACTA PHYSICA SINICA, 2005, 54 (07) : 3444 - 3450
  • [29] BEHAVIOR OF HYDROGEN IN ALPHA-PHASE TI-AL ALLOYS
    PATON, NE
    HICKMAN, BS
    LESLIE, DH
    METALLURGICAL TRANSACTIONS, 1971, 2 (10): : 2791 - &
  • [30] THE LOW-CYCLE FATIGUE BEHAVIOR OF TI-AL ALLOYS
    KIM, HM
    WILLIAMS, JC
    JOURNAL OF METALS, 1980, 32 (08): : 38 - 38