Long-term creep testing and microstructure evaluation of P91 steel weld joints

被引:0
|
作者
Jandova, Dagmar [1 ]
Kasl, Josef [1 ]
Kanta, Vaclav [1 ]
机构
[1] SKODA VYZKUM Sro, Plzen, Czech Republic
关键词
D O I
暂无
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Trial weld joints were made from wrought and cast modified Cr-1Mo-V steel using GTAW & SMAW methods. Creep testing was carried out at temperature range from 525 degrees C to 625 degrees C and stresses from 50 to 240 MPa. Time to rupture of welds made from tube segments and cast plates reached almost 30 000 hours and 20 000 hours respectively. Creep strength was evaluated according the Larson-Miller parametric equation and microstructure was investigated using both light and electron microscopy. Creep rupture strength of both weld joints tested at temperatures below 600 degrees C falls into the +/- 20% scatter band of the creep rupture strength of the parent material. At 600 degrees C and 625 degrees C the creep strength dropped by 27% and 30% for the plate weld and the tube weld respectively. All ruptures occurred in fine grain and intercritically reheated heat affected zones either in the parent material or in the weld metal. Observation of thin foils prepared from selected regions of the weld joints revealed differences in precipitation processes and the structure recovery causing decrease of dislocation density in some regions. Fine ferritic grains with low density of fine carbonitride precipitate occurred in critical localities. Soft grains were deformed and cavities at grain boundaries initiated the crack propagation.
引用
收藏
页码:143 / +
页数:2
相关论文
共 50 条
  • [21] A comparative study on the effect of GTAW processes on the microstructure and mechanical properties of P91 steel weld joints
    Arivazhagan, B.
    Vasudevan, M.
    JOURNAL OF MANUFACTURING PROCESSES, 2014, 16 (02) : 305 - 311
  • [22] Role of microstructures on heterogeneous creep behaviour across P91 steel weld joint assessed by impression creep testing
    Sakthivel, T.
    Sasikala, G.
    Vasudevan, M.
    MATERIALS CHARACTERIZATION, 2020, 159
  • [23] LONG TERM CREEP LIFE PREDICTION OF NEW AND SERVICE EXPOSED P91 STEEL
    Ejaz, Muneeb
    Ab Razak, Norhaida
    Morris, Andrew
    Lockyer, Scott
    Davies, Catrin M.
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2018, VOL 6A, 2019,
  • [24] Creep behavior of dissimilar metal weld joints between P91 and AISI 304
    Akram, Javed
    Kalvala, Prasad Rao
    Misra, Mano
    Charit, Indrajit
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 688 : 396 - 406
  • [25] Effect of Long-Term Aging on the Microstructural Evolution in a P91 Steel
    Zhao, Hongchang
    Wang, Zixi
    Han, Xi
    Wang, Mingjia
    MATERIALS, 2022, 15 (08)
  • [26] Evaluation of microstructure degradation during creep of P91 steel using electrochemical detection technique
    Zhu, Lin
    Liu, Xinbao
    Fan, Ping
    Yang, Yang
    Zhang, Kai
    Wang, Kai
    Wang, Lin
    MATERIALS TODAY COMMUNICATIONS, 2023, 34
  • [27] Creep deformation and rupture behaviour of service exposed P91 weld and base steel measured by miniature tensile creep testing
    Erten, Deniz Taygun
    Thanh Tuan Nguyen
    Jeong, Tae Min
    Yoon, Kee Bong
    MATERIALS AT HIGH TEMPERATURES, 2017, 34 (5-6) : 425 - 433
  • [28] Study of the microstructure of a weld bead P91 steel by transmission electron microscopy
    Lucia Marzocca, Ana
    Soldera, Flavio
    Zalazar, Monica
    Ines Luppo, Maria
    MATERIA-RIO DE JANEIRO, 2018, 23 (02):
  • [29] Analysis of creep behavior of welded joints of P91 steel at 600 °C
    El-Desoky, O. E.
    Abd El-Azim, M. E.
    ElKossy, M. R.
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2019, 171 : 145 - 152
  • [30] Thermomechanical modelling of weld microstructure and residual stresses in P91 steel pipe
    Yaghi, A.H.
    Hyde, T.H.
    Becker, A.A.
    Sun, W.
    Energy Materials: Materials Science and Engineering for Energy Systems, 2009, 4 (03): : 113 - 123