Change in the fracture surface pattern in the fracture process of SUS631 stainless steel fatigued by repeated bending

被引:2
|
作者
Tanaka, Manabu
Kato, Ryuichi
Sukegawa, Junpei
机构
[1] Akita Univ, Fac Engn & Resource Sci, Dept Mech Engn, Akita 0108502, Japan
[2] Akita Univ, Grad Sch Engn & Resource Sci, Akita 0108502, Japan
关键词
D O I
10.2355/isijinternational.47.1372
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Fractal dimension of the fracture surface has been calculated and displayed as a fracture surface pattern map (FPM) to examine the fracture process of SUS631 stainless steel fatigued by repeated bending. SUS631 steel plates of about 1 mm thickness with thermo mechanical heat treatment (ACH) treatment were used that had martensite structure with a small of retained austenite and delta ferrite. Quasi-cleavage fracture with microcracks was dominant in the fatigue fracture of the steel, while ductile fracture surface with dimples was also observed near the fracture surface. It was observed that the fracture surface near specimen surface formed in the earlier stage of fatigue was subjected to more damage by cyclic compressive load, and the fracture surface geometry became simpler than the fracture surface in the interior of specimen formed in the later stage. The geometrical analysis was found suitable to examine the fracture process of materials numerically and visually.
引用
收藏
页码:1372 / 1374
页数:3
相关论文
共 50 条
  • [31] Ductile Fracture Prediction of 316LN Stainless Steel in Hot Deformation Process
    Jian-li HE
    Juan LIU
    Zhen-shan CUI
    Chao-zhong YANG
    Fei CHEN
    Journal of Iron and Steel Research(International), 2014, 21 (10) : 923 - 930
  • [32] Ductile Fracture Prediction of 316LN Stainless Steel in Hot Deformation Process
    He, Jian-li
    Liu, Juan
    Cui, Zhen-shan
    Yang, Chao-zhong
    Chen, Fei
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2014, 21 (10) : 923 - 930
  • [33] Intergranular Brittle Fracture of SUS304 Stainless Steel with Residual Tensile Stress During Molten Chloride Attack
    Hayashi, K.
    Suzuki, H.
    Takemoto, M.
    1997, (46):
  • [34] Intergranular brittle fracture of SUS304 stainless steel with residual tensile stress during the molten chloride attack
    Graduate Sch of Aoyama Gakuin Univ, Tokyo, Japan
    Zairyo Kankyo, 1 (30-36):
  • [35] Carbon segregation and inclusions effects on surface fracture morphology of a 12% chromium stainless steel
    Souami, N
    Saidi, D
    Negache, M
    Ati, A
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2003, 12 (06) : 715 - 720
  • [36] Carbon segregation and inclusions effects on surface fracture morphology of a 12% chromium stainless steel
    N. Souami
    D. Saidi
    M. Negache
    A. Ati
    Journal of Materials Engineering and Performance, 2003, 12 : 715 - 720
  • [37] Fracture analysis procedure for cast austenitic stainless steel pipes with an axial surface crack
    Kamaya, M. (kamaya@inss.co.jp), 1600, Japan Society of Mechanical Engineers, Shinanomachi 35, Shinjuku-ku, Tokyo, 160-0016, Japan (78):
  • [38] Duplex stainless steel fracture surface analysis using x-ray fractography
    Rajanna, K
    Pathiraj, B
    Kolster, BH
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1997, 6 (01) : 35 - 40
  • [39] ANALYSIS OF FRACTURE SURFACE IN STRESS-CORROSION CRACKING OF AUSTENITIC STAINLESS-STEEL
    KUWANO, S
    OKI, T
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1981, 21 (05) : 345 - 351
  • [40] Correspondence of fracture surface features with mechanical properties in 304LN stainless steel
    Das, Arpan
    Sivaprasad, S.
    Chakraborti, P. C.
    Taraffler, S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 496 (1-2): : 98 - 105