Effects of cooling rate on the microstructure and tensile behavior of a Sn-3.5wt.%Ag solder

被引:168
|
作者
Ochoa, F [1 ]
Williams, JJ [1 ]
Chawla, N [1 ]
机构
[1] Arizona State Univ, Dept Chem & Mat Engn, Tempe, AZ 85287 USA
关键词
lead-free solder; Sn-3.5Ag; cooling rates; microstructure; tensile behavior;
D O I
10.1007/s11664-003-0109-z
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The tensile behavior and microstructure of bulk, Sn-3.5Ag solders as a function of cooling rate were studied. Cooling rate is an important processing parameter that affects the microstructure of the solder and, therefore, significantly influences mechanical behavior. Controlled cooling rates were obtained by cooling specimens in different media: water, air, and furnace. Cooling rate significantly affected secondary dendrite-arm size and spacing of the Sn-rich phase, as well as the aspect ratio of Ag3Sn. The Sn-rich dendrite-arm size and spacing were smaller for water-cooled specimens than for air-cooled specimens. Furnace cooling yielded a nearly eutectic microstructure because the cooling rate approached equilibrium cooling. The morphology of Ag3Sn also changed from spherical, at a fast cooling rate, to a needlelike morphology for slower cooling. The changes in the microstructure induced by the cooling rate significantly affected the mechanical behavior of the solder. Yield strength was found to increase with increasing cooling rate, although ultimate tensile strength and strain-to-failure seemed unaffected by cooling rate. Cooling rate did not seem to affect Young's modulus, although a clear correlation between modulus and porosity was obtained. The mechanical behavior was correlated with the observed microstructure, and fractographic analysis was employed to elucidate the underlying damage mechanisms.
引用
收藏
页码:1414 / 1420
页数:7
相关论文
共 50 条
  • [11] The effect of strain rate and temperature on the tensile properties of Sn-3.5Ag solder
    Lang, FQ
    Tanaka, H
    Munegata, O
    Taguchi, T
    Narita, T
    MATERIALS CHARACTERIZATION, 2005, 54 (03) : 223 - 229
  • [12] Correlation between mechanical tensile properties and microstructure of eutectic Sn-3.5Ag solder
    Yeung, B
    Jang, JW
    JOURNAL OF MATERIALS SCIENCE LETTERS, 2002, 21 (09) : 723 - 726
  • [13] Effects of Cooling Rate on the Microstructure and Morphology of Sn-3.0Ag-0.5Cu Solder
    Lee, Hwa-Teng
    Huang, Kuo-Chen
    JOURNAL OF ELECTRONIC MATERIALS, 2016, 45 (01) : 182 - 190
  • [14] Effects of Cooling Rate on the Microstructure and Morphology of Sn-3.0Ag-0.5Cu Solder
    Hwa-Teng Lee
    Kuo-Chen Huang
    Journal of Electronic Materials, 2016, 45 : 182 - 190
  • [15] Effects of cooling rate and joint size on Sn grain features in Cu/Sn-3.5Ag/Cu solder joints
    Chang, Z. Y.
    Zhao, N.
    Wu, C. M. L.
    MATERIALIA, 2020, 14
  • [16] Effect of cooling rate on microstructure of Ag-Cu-Sn solder alloys
    Snugovsky, L
    Snugovsky, P
    Perovic, DD
    Rutter, JW
    MATERIALS SCIENCE AND TECHNOLOGY, 2005, 21 (01) : 61 - 68
  • [17] Ambient Temperature Ultrasonic Bonding of Si-Dice Using Sn-3.5wt.%Ag
    Jung-Mo Kim
    Jae-Pil Jung
    Y. Norman Zhou
    Jong-Young Kim
    Journal of Electronic Materials, 2008, 37 : 324 - 330
  • [18] The effects of temperature gradient and growth rate on the microstructure of directionally solidified Sn–3.5Ag eutectic solder
    Mevlüt Şahin
    Emin Çadirli
    Journal of Materials Science: Materials in Electronics, 2012, 23 : 484 - 492
  • [19] The effects of temperature gradient and growth rate on the microstructure of directionally solidified Sn-3.5Ag eutectic solder
    Sahin, Mevlut
    Cadirli, Emin
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2012, 23 (02) : 484 - 492
  • [20] Ambient temperature ultrasonic bonding of Si-dice using Sn-3.5wt.%Ag
    Kim, Jung-Mo
    Jung, Jae-Pil
    Zhou, Y. Norman
    Kim, Jong-Young
    JOURNAL OF ELECTRONIC MATERIALS, 2008, 37 (03) : 324 - 330