Tribology in superplastic forming processing of 3Y-TZP/Al2O3 ceramic at elevated temperatures

被引:0
|
作者
Wang, F. [1 ]
Zhang, K. F. [1 ]
Han, W. B. [1 ]
机构
[1] Harbin Inst Technol, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
ceramic superplasticity; friction and lubrication; high-temperature lubricant; ring compressive test;
D O I
10.4028/www.scientific.net/MSF.551-552.507
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Superplastic forming processing of ceramic materials at high temperatures and high pressure puts forward very high requests to moulds and lubricants, at which conditions seeking for appropriate lubricants is one of important preconditions in the superplastic forming of ceramic materials. Using ring compressive testing, lubricities of hexagonal boron nitride in superplastic compressive forming processing of 3Y-TZP/Al2O3 ceramic composite at elevated temperatures were investigated. Theoretical curves of friction factor were drawn according to upper bound method. Ring compressive tests were adopted at temperature of 1400 degrees C-1600 degrees C. The results indicate that when BN is used, friction factor is about 0.4, meanwhile friction factor don't have great changes with higher temperature and increasing strain rate. X-ray diffraction shows that under high temperature and high pressure no boron nitride converts to cubic phase, which remains at room temperature.
引用
收藏
页码:507 / +
页数:2
相关论文
共 50 条
  • [41] Microstructure and toughening mechanism of the 3Y-TZP/Al2O3 composite reinforced by SiC whiskers
    Chinese Acad of Sciences, Shanghai, China
    J Mater Sci, 24 (6637-6643):
  • [42] Microstructure and toughening mechanism of the 3Y-TZP/Al2O3 composite reinforced by SiC whiskers
    Xu, FF
    Ma, LT
    Wen, SL
    JOURNAL OF MATERIALS SCIENCE, 1996, 31 (24) : 6637 - 6643
  • [43] Preparation of the Al2O3/3Y-TZP ceramics by microwave sintering under low temperature
    Luo, Junming
    Xu, Jilin
    Zuo, Hongyan
    Huang, Jun
    APPLIED MECHANICS AND MATERIALS II, PTS 1 AND 2, 2014, 477-478 : 1238 - 1241
  • [44] 3Y-TZP/γ-Al2O3复合粉体制备方法的探究
    韦薇
    陈亮维
    管春平
    陈应花
    天然气化工(C1化学与化工), 2007, (06) : 42 - 45
  • [45] Low temperature degradation of Al2O3-doped 3Y-TZP sintered at various temperatures
    Wu, Zhi-kai
    Li, Ning
    Jian, Chao
    Zhao, Wan-qian
    Yan, Jia-zhen
    CERAMICS INTERNATIONAL, 2013, 39 (06) : 7199 - 7204
  • [46] Characterization of tunneling cracks in Al2O3/Al2O3 +3Y-TZP multilayered composites by Raman and fluorescence piezo-spectroscopy
    Goffredo De Portu
    Lorenzo Micele
    Giuseppe Pezzotti
    Journal of Materials Science, 2005, 40 : 1505 - 1508
  • [47] Deformation of superplastic Al2O3/Y-TZP particulate and particulate laminate composites
    Wang, J
    Kovar, D
    Taleff, EM
    ADVANCES IN SUPERPLASTICITY AND SUPERPLASTIC FORMING, 2004, : 265 - 273
  • [48] Cavitation damage mechanisms in a superplastic zirconia(3Y-TZP)
    Hiraga, K
    Nakano, K
    SUPERPLASTICITY IN ADVANCED MATERIALS - ICSAM-97, 1997, 243-2 : 387 - 392
  • [49] Effect of the Al2O3 content on the mechanical properties and microstructure of 3Y-TZP ceramics for dental applications
    Tang, Dongxu
    Lee, Ki-Ju
    Xu, Jingwen
    Lim, Hyung-Bong
    Park, K.
    Cho, Won-Seung
    METALS AND MATERIALS INTERNATIONAL, 2012, 18 (03) : 545 - 551
  • [50] Effect of liquid-forming additives on the sintering and mechanical properties of Al2O3/3Y-TZP (30 vol.%) composite
    Huang, XW
    Wang, SW
    Zhao, SK
    Huang, XX
    MATERIALS RESEARCH BULLETIN, 2002, 37 (10) : 1709 - 1719