The effect of pre-straining and pre-ageing on a novel thermomechanical treatment for improving the mechanical properties of AA2139 aerospace aluminium alloys

被引:4
|
作者
Bakare, F. [1 ,2 ]
Alsubhi, Y. [1 ]
Ragkousis, A. [1 ]
Ebomwonyi, O. [2 ]
Damisa, J. [2 ]
Okunzuwa, S. [2 ]
机构
[1] Univ Manchester, Sch Mat, Manchester, Lancs, England
[2] Univ Benin, Phys Dept, Benin, Nigeria
来源
MATERIALS RESEARCH EXPRESS | 2017年 / 4卷 / 07期
关键词
aluminium alloys; cold-rolling; mechanical testing; thermomechanical processing; precipitation; STRENGTH; PRECIPITATION; BEHAVIOR;
D O I
10.1088/2053-1591/aa7bc0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The novel thermomechanical treatment employed by Wang Z et al (2014 Mater. Sci. Eng. A 607 313-7) in enhancing the mechanical and microstructure properties of 6000 series aluminium alloys has been replicated for AA2139 aerospace aluminium alloys. The novel route which involves underageing, cold-rolling reductions and re-ageing at a fixed temperature has been carried out focusing on the effect of pre-straining and pre-ageing on the alloy properties. The influence of varying coldrolling reductions and pre-ageing has been examined by tensile testing, hardness testing, differential scanning calorimetry, thermoelectric power measurements and scanning electron microscope (SEM). Further analyses were conducted with DSC and TEP measurements to check for precipitation sequence and solute retention respectively. On comparing the hardness and strength of the non pre-aged to the pre-aged samples, there is a remarkable increase in the hardness and strength of the aerospace alloy showing the huge influence of both pre-ageing and pre-straining stage of the novel thermomechanical treatment as observed in the 6000 series alloy, albeit at a higher rate. The treatments that exhibited the most promising mechanical properties (hardness, yield and ultimate tensile strength, elongation to failure) were found to be at a pre-ageing temperature of 175 degrees C for 1.5 h, 40% cold-rolling and re-ageing at 150 degrees C. The material was found to have yield strength of 590 MPa and 8.1% uniform elongation, which is well above the 5% acceptable value for structural applications and with strength levels adaptable for aerospace industries. The presence of higher volume fraction of well dispersed precipitates observed in the SEM further shows that intermediate cold-rolling reductions combines well with pre-ageing to give the best mechanical properties in this alloy.
引用
收藏
页数:9
相关论文
共 42 条
  • [21] The effect of tensile pre-straining on fatigue crack initiation mechanisms and mechanical behavior of AA7050 friction stir welds
    White, B. C.
    White, R. E.
    Jordon, J. B.
    Allison, P. G.
    Rushing, T.
    Garcia, L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 736 : 228 - 238
  • [22] Effects of Pre-ageing on Microstructure and Mechanical Properties of T9I6 Treated 2519A Aluminium Alloy
    Ye, Lingying
    Dong, Yu
    Liu, Shengdan
    Jiang, Haichun
    Sun, Daxiang
    Zhang, Xinming
    METALS AND MATERIALS INTERNATIONAL, 2018, 24 (05) : 1149 - 1161
  • [23] Effects of Pre-ageing on Microstructure and Mechanical Properties of T9I6 Treated 2519A Aluminium Alloy
    Lingying Ye
    Yu Dong
    Shengdan Liu
    Haichun Jiang
    Daxiang Sun
    Xinming Zhang
    Metals and Materials International, 2018, 24 : 1149 - 1161
  • [24] EFFECT OF HIGH TEMPERATURE PRE-AGEING AND LOW-TEMPERATURE RE-AGEING ON MECHANICAL PROPERTIES AND INTERGRANULAR CORROSION SUSCEPTIBILITY OF Al-Mg-Si-Cu ALLOYS
    Li Hai
    Mao Qingzhong
    Wang Zhixiu
    Miao Fenfen
    Fang Bijun
    Song Renguo
    Zheng Ziqiao
    ACTA METALLURGICA SINICA, 2014, 50 (11) : 1357 - 1366
  • [25] Effect of high temperature pre-ageing and low-temperature re-ageing on mechanical properties and intergranular corrosion susceptibility of Al-Mg-Si-Cu alloys
    Li, Hai
    Mao, Qingzhong
    Wang, Zhixiu
    Miao, Fenfen
    Fang, Bijun
    Song, Renguo
    Zheng, Ziqiao
    Jinshu Xuebao/Acta Metallurgica Sinica, 2014, 50 (11): : 1357 - 1366
  • [26] Synergy effect of Si addition and pre-straining on microstructure and properties of Al-Cu-Mg alloys with a medium Cu/Mg ratio
    Li, Jiyu
    Chen, Songyi
    Li, Fushan
    Chen, Kanghua
    Huang, Lanping
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 767
  • [27] Effect of pre-straining and natural aging on the hardening response during artificial aging of en aw 6082 and lead free en aw 6023 aluminium alloys
    Fujda M.
    Matvija M.
    Horňak P.
    Materials Science Forum, 2019, 952 : 82 - 91
  • [28] Regulation of Microstructure, Residual Stress, and Mechanical Properties by Pre-straining and Subsequent Heat Treatment in Selective Laser Melted 304L Stainless Steel
    Zhang, Fanfan
    Zhang, Kaiyu
    Zhong, Fengping
    Huang, Liuyi
    Zhang, Wanliang
    Zhou, Chengshuang
    Huang, Liangliang
    Lin, Zhongxiang
    Li, Liangliang
    Zhang, Meng
    Zhang, Lin
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025, 34 (05) : 3717 - 3730
  • [29] Pre-deformation effect on stress-relaxation ageing behavior and mechanical properties of AA2219 alloy
    Yang, Youliang
    Zhan, Lihua
    Liu, Chunhui
    International Journal of Lightweight Materials and Manufacture, 2020, 3 (01): : 73 - 76
  • [30] Effect of pre-deformation on microstructure and mechanical properties of 2219 aluminum alloy sheet by thermomechanical treatment
    An Li-hui
    Cai Yang
    Liu Wei
    Yuan Shi-jian
    Zhu Shi-qiang
    Meng Fan-cheng
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 : S370 - S375