Corrosion behaviour of As sintered P/M Al-SiC composites

被引:0
|
作者
Rajiv, EP
Srinivasan, PB
Balakrisiinan, K
机构
[1] GUJARAT HEAVY CHEM LTD,VERAVAL,GUJARAT,INDIA
[2] CENT ELECTROCHEM RES INST,KARAIKKUDI 630006,TAMIL NADU,INDIA
来源
BULLETIN OF ELECTROCHEMISTRY | 1997年 / 13卷 / 03期
关键词
composites; aluminium; silicon carbide and corrosion;
D O I
暂无
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Metal matrix composites based on aluminium alloy matrices are widely being used for structural applications. Though these composites are made by both liquid metallurgy and powder processing routes, the corrosion resistance of these materials is still not well understood. In the present study, an attempt has been made to produce composites consisting of commercial pure aluminium (99%) and silicon carbide pal-tides by the powder metallurgy route and characterize their corrosion behaviour in the as sintered condition in 3.5% NaCl solution of varying pH levels, Results of the study indicate that the composites in the as sintered state have better corrosion resistance than the monolithic material.
引用
收藏
页码:107 / 111
页数:5
相关论文
共 50 条
  • [21] Microstructures and mechanical properties of spark plasma sintered Al-SiC composites containing high volume fraction of SiC
    Zhang, Zhao-Hui
    Wang, Fu-Chi
    Luo, Jie
    Lee, Shu-Kui
    Wang, Lu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (27-28): : 7235 - 7240
  • [22] Solidification Behaviour of Al-SiC Composite Foam
    Das, S.
    Mondal, D. P.
    Rohatgi, Pradeep
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (11) : 2861 - 2866
  • [23] Effect of sintering temperature on microstructure and selected properties of spark plasma sintered Al-SiC composites
    Leszczynska-Madej, Beata
    Garbiec, Dariusz
    Madej, Marcin
    VACUUM, 2019, 164 : 250 - 255
  • [24] THE THERMOMECHANICAL PROCESSING OF AL-SIC PARTICULATE COMPOSITES
    HUMPHREYS, FJ
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1991, 135 : 267 - 273
  • [25] INTERFACES AND FAILURE MECHANISMS IN AL-SIC COMPOSITES
    NUTT, SR
    JOURNAL OF METALS, 1985, 37 (11): : A111 - A112
  • [26] QUENCH STRENGTHENING MECHANISM OF AL-SIC COMPOSITES
    MA, ZY
    BI, J
    LU, YX
    GAO, YX
    SCRIPTA METALLURGICA ET MATERIALIA, 1993, 29 (02): : 225 - 229
  • [27] High temperature properties of Al-SiC composites
    Saigal, A
    Doherty, B
    Materials in the Automotive Industry, 2001, : 267 - 277
  • [28] Modelling wear behaviour of Al-SiC metal matrix composites: soft computing technique
    Vijayakumar, S.
    Karunamoorthy, L.
    TRIBOLOGY-MATERIALS SURFACES & INTERFACES, 2012, 6 (01) : 25 - 30
  • [29] Toughening mechanisms in Al/Al-SiC laminated metal composites
    Lesuer, DR
    Wadsworth, J
    Riddle, RA
    Syn, CK
    Lewandowski, JJ
    Hunt, WH
    LAYERED MATERIALS FOR STRUCTURAL APPLICATIONS, 1996, 434 : 205 - 211
  • [30] THE EFFECT OF FABRICATION TECHNIQUES ON THE PROPERTIES OF AL-SIC COMPOSITES
    LING, CP
    BUSH, MB
    PERERA, DS
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1995, 48 (1-4) : 325 - 331