Review of the initiation and arrest temperatures for delayed hydride cracking in zirconium alloys

被引:0
|
作者
Kim, YS [1 ]
Choi, SJ [1 ]
Cheong, YM [1 ]
机构
[1] Korea Atom Energy Res Inst, Zirconium Team, Taejon 305353, South Korea
关键词
delayed hydfide cracking; DHC initiation and arrest temperatures; ratcheting thermal cycle; terminal solid solubility; hydrogen; zirconium alloys;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Based on Kim's delayed hydride cracking (DHC) model, this study reanalyzes the critical temperatures for DHC initiation and arrest in zirconium alloys that had previously been investigated with Puls DHC model. in an unratcheting thermal cycle where DHC crack tip hydrides were dissolved fully at the peak temperature, the DHC initiation was suppressed, which required a supercooling or DeltaT from the terminal solid solubility for dissolution (TSSD) temperatures. At a hydrogen concentration as low as 7 ppm H, the DHC initiation temperatures coincided with the TSSD, which is in conflict with Puls' DHC model. In a ratcheting thermal cycle, where the hydrides precipitated at the DHC crack tip were not fully dissolved, the DHC initiation was enhanced, so as to require a lesser DeltaT, compared to that of the unratcheting thermal cycle. Therefore, the DHC initiation temperatures are concluded to depend upon at what temperatures the hydrides can nucleate in the zirconium matrix with the supersaturated hydrogen concentration. The DHC arrest temperatures were governed by the critical supersaturated hydrogen concentration or DeltaC regardless of the thermal cycle treatment, providing further supportive evidence that Kim's DHC model is feasible.
引用
收藏
页码:39 / 47
页数:9
相关论文
共 50 条
  • [41] A review on hydride precipitation in zirconium alloys
    Bair, Jacob
    Zaeem, Mohsen Asle
    Tonks, Michael
    JOURNAL OF NUCLEAR MATERIALS, 2015, 466 : 12 - 20
  • [42] HYDRIDE PRECIPITATES IN ZIRCONIUM ALLOYS (A REVIEW)
    ELLS, CE
    JOURNAL OF NUCLEAR MATERIALS, 1968, 28 (02) : 129 - &
  • [43] DEPENDENCE OF THE THRESHOLD STRESS INTENSITY FACTOR ON HYDROGEN CONCENTRATION DURING DELAYED HYDRIDE CRACKING IN ZIRCONIUM ALLOYS
    SHI, SQ
    PULS, MP
    JOURNAL OF NUCLEAR MATERIALS, 1995, 218 (01) : 30 - 36
  • [44] CATEGORIZATION OF DELAYED HYDRIDE CRACKING IN ZIRCONIUM ALLOYS IN TERMS OF CUMULATIVE AND NON-CUMULATIVE FRACTURE MODES
    SMITH, E
    INTERNATIONAL JOURNAL OF FRACTURE, 1995, 71 (01) : R19 - R24
  • [45] Temperature Dependences of the Delayed Hydride Cracking Rate of Fuel Claddings Made of Zirconium Alloys of Various Compositions
    Markelov, V. A.
    Gusev, A. Yu.
    Kotov, P. V.
    Novikov, V. V.
    Saburov, N. S.
    RUSSIAN METALLURGY, 2014, 2014 (04): : 341 - 346
  • [46] CONTROL OF MICROSTRUCTURE TO INCREASE THE TOLERANCE OF ZIRCONIUM ALLOYS TO HYDRIDE CRACKING
    COLEMAN, CE
    SAGAT, S
    AMOUZOUVI, KF
    CIM BULLETIN, 1987, 80 (902): : 89 - 89
  • [47] A combined SIF and temperature model of delayed hydride cracking in zirconium materials
    Shmakov, A. A.
    Singh, R. N.
    Yan, D.
    Eadie, R. L.
    Matvienko, Yu. G.
    COMPUTATIONAL MATERIALS SCIENCE, 2007, 39 (01) : 237 - 241
  • [48] FEM STUDY OF DELAYED HYDRIDE CRACKING IN ZIRCONIUM ALLOY FUEL CLADDING
    Uno, Masayoshi
    Ito, Masato
    Muta, Hiroaki
    Kurosaki, Ken
    Yamanaka, Shinsuke
    Ogata, Keizo
    ADVANCES IN ENERGY MATERIALS, 2009, 205 : 59 - +
  • [49] Near threshold delayed hydride crack growth in zirconium alloys
    Smith, E
    JOURNAL OF MATERIALS SCIENCE, 1995, 30 (23) : 5910 - 5914
  • [50] Zirconium hydride phase mapping in Zircaloy-2 cladding after delayed hydride cracking
    Colldeweih, Aaron W.
    Makowska, Malgorzata G.
    Tabai, Omaia
    Sanchez, Dario Ferreira
    Bertsch, Johannes
    MATERIALIA, 2023, 27