Damage in ceramic masses during drying

被引:0
|
作者
Banaszak, Jacek [1 ]
机构
[1] Poznan Tech Univ, Inst Technol & Chem Engn, PL-60965 Poznan, Poland
来源
INZYNIERIA CHEMICZNA I PROCESOWA | 2007年 / 28卷 / 02期
关键词
D O I
暂无
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
A study of damage in clay-like materials during drying is presented. The theoretical distribution of drying-induced stresses in the cross-section of a cylindrical sample are computed based on the thermomechanical drying model. These stresses are compared to measured material strength with the help of the Huber-von Mises failure criterion. In such a way, one can indicate the regions of dried material most prone to the failure. Three different types of clay-like masses commonly used in ceramic industry are considered: typical regional illite clay, kaolin clay and C130 advanced ceramic mass.
引用
收藏
页码:177 / 188
页数:12
相关论文
共 50 条
  • [41] PSYCHOMETRY OF DRYING CERAMIC MATERIALS
    REED, RJ
    AMERICAN CERAMIC SOCIETY BULLETIN, 1967, 46 (04): : 444 - &
  • [42] Drying of aqueous ceramic suspensions
    Imperial Coll, London, United Kingdom
    Key Eng Mat, Pt 1 (354-357):
  • [43] DAMAGE OF CERAMIC MATRIX COMPOSITES (CMCs) DURING MACHINING OPERATIONS
    Goller, R.
    Roesiger, A.
    ADVANCED AND REFRACTORY CERAMICS FOR ENERGY CONSERVATION AND EFFICIENCY, 2016, 256 : 3 - 10
  • [44] CERAMIC MANUAL/68 - DRYING
    不详
    CERAMIC AGE, 1968, 84 (07): : 44 - &
  • [45] PSYCHROMETRY OF DRYING CERAMIC MATERIALS
    DAVIES, TE
    CERAMIC AGE, 1968, 84 (02): : 32 - &
  • [46] Effects of slurry properties on the crack formation in ceramic green sheets during drying
    Mori, Takamasa
    Yamada, Tomofumi
    Tanaka, Tatsuya
    Katagiri, Akiko
    Tsubaki, JunIchiro
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2006, 114 (1334) : 823 - 828
  • [47] Functional ceramic for solar drying
    Rakhimov R.K.
    Saidov M.S.
    Ermakov V.P.
    Applied Solar Energy, 2008, 44 (4) : 281 - 283
  • [48] Dynamic damage behavior during cooling process of ceramic coatings
    Nishinoiri, S
    Nozawa, K
    Enoki, M
    DESIGNING, PROCESSING AND PROPERTIES OF ADVANCED ENGINEERING MATERIALS, PTS 1 AND 2, 2004, 449-4 : 717 - 720
  • [49] Criterion for crack initiation during drying: Alumina porous ceramic strength improvement
    Pourcel, F.
    Jomaa, W.
    Puiggali, J-R.
    Rouleau, L.
    POWDER TECHNOLOGY, 2007, 172 (02) : 120 - 127
  • [50] Arrhenius activation energy of damage to catalase during spray-drying
    Schaefer, Joachim
    Lee, Geoffrey
    INTERNATIONAL JOURNAL OF PHARMACEUTICS, 2015, 489 (1-2) : 124 - 130