Effect of superalloy substrate and bond coating on TBC lifetime

被引:44
|
作者
Pint, B. A. [1 ]
Haynes, J. A. [1 ]
Zhang, Y. [2 ]
机构
[1] Oak Ridge Natl Lab, Div Mat Sci & Technol, Oak Ridge, TN 37831 USA
[2] Tennessee Technol Univ, Cookeville, TN 38505 USA
来源
SURFACE & COATINGS TECHNOLOGY | 2010年 / 205卷 / 05期
关键词
TBC lifetime; Pt diffusion coating; Pt aluminide coating; Scale adhesion; Oxidation; THERMAL BARRIER COATINGS; SINGLE-CRYSTAL SUPERALLOYS; GAMMA' NIPTAL COATINGS; NI-BASED SUPERALLOYS; OXIDATION BEHAVIOR; ALUMINIDE COATINGS; WATER-VAPOR; PLATINUM; SYSTEMS; PERFORMANCE;
D O I
10.1016/j.surfcoat.2010.08.154
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Several different single-crystal superalloys were coated with different bond coatings to study the effect of composition on the cyclic oxidation lifetime of an yttria-stabilized zirconia (YSZ) top coating deposited by electron beam physical vapor deposition from a commercial source. Three different superalloys were coated with a 7 mu m Pt layer that was diffused into the surface prior to YSZ deposition. One of the superalloys, N5, was coated with a low activity, Pt-modified aluminide coating and Pt-diffusion coatings with 3 and 7 mu m of Pt. Three coatings of each type were furnace cycled to failure in 1 h cycles at 1150 degrees C to assess average coating lifetime. The 7 mu m Pt diffusion coating on N5 had an average YSZ coating lifetime >50% higher than a Pt-modified aluminide coating on N5. Without a YSZ coating, the Pt-modified aluminide coating on N5 showed the typical surface deformation during cycling, however, the deformation was greatly reduced when constrained by the YSZ coating. The 3 mu m Pt diffusion coating had a similar average lifetime as the Pt-modified aluminide coating but a much wider scatter. The Pt diffusion bond coating on superalloy X4 containing Ti exhibited the shortest YSZ coating lifetime, this alloy-coating combination also showed the worst alumina scale adhesion without a YSZ coating. The third generation superalloy N6 exhibited the longest coating lifetime with a 7 mu m Pt diffusion coating. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:1236 / 1240
页数:5
相关论文
共 50 条
  • [41] Advanced MCrAlY alloys with doubled TBC lifetime
    He, Jianhong
    SURFACE & COATINGS TECHNOLOGY, 2022, 448
  • [42] Study of the coating stability of a TBC system
    Guerre, C
    Molins, R
    Remy, L
    MATERIALS AT HIGH TEMPERATURES, 2000, 17 (02) : 197 - 203
  • [43] The Effect of Environment on Thermal Barrier Coating Lifetime
    Pint, Bruce A.
    Unocic, Kinga A.
    Haynes, J. Allen
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 2016, 138 (08):
  • [44] Effect of ion implantation on growth of thermally grown oxide in MCrAlY coating for TBC
    Byon, Eungsun
    Zhang, Shihong
    Lee, Sung-Hun
    Lee, Goo-Hyun
    Kwon, Sik-Chol
    SURFACE & COATINGS TECHNOLOGY, 2010, 205 : S435 - S438
  • [45] Effect of the number of layers on the bond strength for multi-layer brittle coating-substrate system
    Wang YongGuang
    Ni ZiFeng
    Chen GuoZhong
    Chen AnQi
    Su YongShuai
    Zhao YongWu
    SCIENCE CHINA-TECHNOLOGICAL SCIENCES, 2012, 55 (10) : 2936 - 2940
  • [46] Effect of the thickness of cold sprayed aluminium alloy coating on the adhesive bond strength with an aluminium alloy substrate
    Xiong, Yuming
    Zhuang, Wyman
    Zhang, Mingxing
    SURFACE & COATINGS TECHNOLOGY, 2015, 270 : 259 - 265
  • [47] Effect of the number of layers on the bond strength for multi-layer brittle coating-substrate system
    WANG YongGuang 1
    2 School of Mechanical Engineering
    Science China(Technological Sciences), 2012, (10) : 2936 - 2940
  • [48] Effect of the number of layers on the bond strength for multi-layer brittle coating-substrate system
    WANG YongGuang NI ZiFeng CHEN GuoZhong CHEN AnQi SU YongShuai ZHAO YongWu Kelin Environmental Protection EquipmentIncSuzhou China School of Mechanical EngineeringJiangnan UniversityWuxi China
    Science China(Technological Sciences), 2012, 55 (10) : 2936 - 2940
  • [49] Effect of the number of layers on the bond strength for multi-layer brittle coating-substrate system
    YongGuang Wang
    ZiFeng Ni
    GuoZhong Chen
    AnQi Chen
    YongShuai Su
    YongWu Zhao
    Science China Technological Sciences, 2012, 55 : 2936 - 2940
  • [50] `High-temperature cyclic oxidation of Pt-rich γ-γ′ bond-coatings. Part II: Effect of Pt and Al on TBC system lifetime
    Audigie, Pauline
    Rouaix-Vande Put, Aurelie
    Malie, Andre
    Thouron, Carole
    Monceau, Daniel
    CORROSION SCIENCE, 2019, 150 : 1 - 8