Fabrication of Fe-6.5wt% Si bulk by spark plasma sintering

被引:0
|
作者
Hu, CZ [1 ]
Zhang, DM [1 ]
Zhang, LM [1 ]
机构
[1] Wuhan Univ Technol, State Key Lab Adv Technol Mat Synth & Proc, Wuhan 430070, Peoples R China
来源
JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION | 2005年 / 20卷 / 01期
关键词
Fe-6.5wt% Si; spark plasma sintering; mechanical alloying; non-equilibrium;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fe-6.5 wt% Si composite compact was fabricated by spark plasma sintering SPS Mechanical alloying (AM) was used to prepare Fe-Si composite powders. The composite powders were sintered by SPS at elev-sated temperature from 500 degrees C to 700 degrees C. The experimental results indicate that the non-equilibrium state of composite Fe-Si is preserved in the compact. The density of the bulk rises with the increasing temperature and there is no diffusion of silicon and iron in the interface.
引用
收藏
页码:72 / 74
页数:3
相关论文
共 50 条
  • [21] Core loss reduction for Fe-6.5wt%Si soft magnetic composites doped with Co element
    Wang, Jian
    Liu, Xin
    Lei, Chao
    Mao, Xinhua
    Liu, Danhua
    Fan, Xi'an
    Luo, Zigui
    Luo, Fan
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2020, 502
  • [22] High efficiency warm-cold rolling technology of Fe-6.5wt%Si alloy sheets
    Xie, Jianxin
    Pan, Hongjiang
    Fu, Huadong
    Zhang, Zhihao
    11TH INTERNATIONAL CONFERENCE ON TECHNOLOGY OF PLASTICITY, ICTP 2014, 2014, 81 : 149 - 154
  • [23] Fabrication of non-equilibrium Fe-Si compact by spark plasma sintering
    Zhang, DM
    Zhang, LM
    Hu, CZ
    COMPOSITE MATERIALS III, 2003, 249 : 307 - 310
  • [24] Fe-6.5wt%Si硅钢薄带的制备工艺及发展前景
    龙琼
    胡素丽
    路坊海
    曾英
    周登凤
    磁性材料及器件, 2016, 47 (02) : 61 - 66
  • [25] Warm/cold rolling processes for producing Fe-6.5wt% Si electrical steel with columnar grains
    Fu, Hua-dong
    Zhang, Zhi-hao
    Pan, Hong-jiang
    Mo, Yuan-ke
    Xie, Jian-xin
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2013, 20 (06) : 535 - 540
  • [26] Alloy elements added in Fe-6.5wt% Si silicon steel and their effect on ductility and magnetic properties
    Cheng, Zhaoyang
    Liu, Jing
    Chen, Wensi
    Sun, Guodong
    Lin, Xifeng
    Zhu, Yuan
    Zhu, Shang
    Zhu, Jiachen
    Xiang, Zhidong
    ADVANCED ENGINEERING MATERIALS III, PTS 1-3, 2013, 750-752 : 426 - +
  • [27] Warm/cold rolling processes for producing Fe-6.5wt% Si electrical steel with columnar grains
    Hua-dong Fu
    Zhi-hao Zhang
    Hong-jiang Pan
    Yuan-ke Mo
    Jian-xin Xie
    International Journal of Minerals, Metallurgy, and Materials, 2013, 20 : 535 - 540
  • [28] Soft Magnetic Properties of Fe-6.5wt%Si/SrFe12O19 Composites
    Feng Hu
    Jiangli Ni
    Shuangjiu Feng
    Xucai Kan
    Yujie Yang
    Qingrong Lv
    Xiansong Liu
    Journal of Superconductivity and Novel Magnetism, 2020, 33 : 2779 - 2785
  • [29] Soft Magnetic Properties of Fe-6.5wt%Si/SrFe12O19 Composites
    Hu, Feng
    Ni, Jiangli
    Feng, Shuangjiu
    Kan, Xucai
    Yang, Yujie
    Lv, Qingrong
    Liu, Xiansong
    JOURNAL OF SUPERCONDUCTIVITY AND NOVEL MAGNETISM, 2020, 33 (09) : 2779 - 2785
  • [30] Study of the brittle behaviour of annealed Fe-6.5wt%Si ribbons produced by planar flow casting
    Viala, B
    Degauque, J
    Fagot, M
    Baricco, M
    Ferrara, E
    Fiorillo, F
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 212 (01): : 62 - 68