Corrosion behavior of ternary Fe-15Cu-5Al alloy in pure oxygen at 1000 °C

被引:0
|
作者
Yang Gan-lan [1 ]
Xiang Jun-huai [1 ,2 ]
Zhang Wen-hua [1 ]
Zhao Qiong [1 ]
Bai Ling-yun [1 ]
机构
[1] Jiangxi Sci & Technol Normal Univ, Sch Mat Sci & Engn, Nanchang 330013, Peoples R China
[2] E China Inst Technol, Key Lab Nucl Resources & Environm, Minist Educ, Nanchang, Peoples R China
关键词
Fe-15Cu-5Al alloy; ternary alloy; corrosion behavior; nodules;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The corrosion behavior of ternary Fe-15Cu-5Al (mole fraction, %) alloy was studied at 1000 degrees C in 0.1 MPa pure oxygen. The Fe-rich alloy shows two parabolic oxidation stages, with a small increase of the parabolic rate constant from 1.9 x 10(-9) to 4.1 x 10(-9) g(2)/(cm(4).s). The scale grown on the alloy is very complicated, with formation of overgrown nodules interspersed among bulky stratified scales. The nodules and the bulky stratified scales are always composed of an outer layer of CuFe2O4 and of an inner layer containing Fe2O3 and Fe3O4. Beneath the external scale of the nodules, there is an internal oxidation zone where iron oxide is mixed with copper metal. Furthermore, the base of the internal oxidation zone is characterized by a discontinuous aluminum-enriched layer of either Al2O3 or FeAl2O4. For the stratified scales, no internal oxidation zone is present beneath the innermost Al2O3 or FeAl2O4 layer. Aluminum depletion is present in advance of the internal oxidation front, while iron depletion is not observed. The corrosion feature of the ternary Fe-15Cu-5Al alloy is partly associated with that of the corresponding binary Fe-Cu and Fe-Al alloys. The peculiar scale microstructure observed is considered mainly as a consequence of the limited solubility of the iron and copper components in one another and of the monovariant system of the ternary Fe-15Cu-5Al alloy.
引用
收藏
页码:S175 / S179
页数:5
相关论文
共 50 条
  • [41] OXIDATION OF A FE-MN-AL-C ALLOY AT 1000-DEGREES-C
    LOPES, MFS
    ASSUNCAO, FCR
    JOURNAL OF METALS, 1985, 37 (11): : A63 - A63
  • [42] SCALING BEHAVIOR OF AN FE-4.54 WT-PERCENT CU ALLOY IN THE RANGE 700-C TO 1000-C UNDER 1 ATM OXYGEN
    NANNI, P
    GESMUNDO, F
    CORROSION, 1980, 36 (03) : 119 - 125
  • [43] Effect of Ge Contents on Oxidation Resistance of Ni-15Cr-5Al Alloy at 1000°C
    Gu, Huiling
    Guo, Jiaojiao
    Wang, Kang
    Shen, Fang
    Gu, Yunxin
    Zhang, Xiuhai
    Wei, Zongwu
    Advances in Materials Science and Engineering, 2024, 2024
  • [44] Dealloying Behavior of Al-Cu-Sn ternary alloy in an Alkaline Solution
    Feng, Yefei
    Zhang, Shichao
    Xing, Yalan
    Liu, Wenbo
    NEW MATERIALS, APPLICATIONS AND PROCESSES, PTS 1-3, 2012, 399-401 : 774 - 779
  • [45] Effect of Ti on the Corrosion Behavior of Fe22Cr5Al3Mo Alloy in 500°C Superheated Steam
    Sun Rongrong
    Yao Meiyi
    Lin Xiaodong
    Zhang Wenhuai
    Qiu Yunlong
    Hu Lijuan
    Xie Yaoping
    Yang Jian
    Dong Jianxin
    Cheng Guoguang
    ACTA METALLURGICA SINICA, 2022, 58 (05) : 610 - 622
  • [46] Comparative Study on the Corrosion Resistance of Al-Cr-Fe Alloy Containing Quasicrystals and Pure Al
    Li, R. T.
    Murugan, Vinod K.
    Dong, Z. L.
    Khor, K. A.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2016, 32 (10) : 1054 - 1058
  • [47] Effect of chromium on the oxidation of a Fe-10Al alloy at 1000°C
    Zhang, ZG
    Niu, Y
    PRICM 5: THE FIFTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-5, 2005, 475-479 : 685 - 688
  • [48] Oxidation of a ternary Cu-Ni-Fe alloy under low oxygen pressures at 800-900°C
    Li, YS
    Niu, Y
    Gesmundo, F
    JOURNAL OF ALLOYS AND COMPOUNDS, 2001, 317 : 578 - 582
  • [49] Corrosion resistance of the Fe-Al-C permanent magnet alloy
    Giza, K
    Bala, H
    Wyslocki, JJ
    Szymura, S
    INTERMETALLICS, 1998, 6 (05) : 357 - 362
  • [50] Heat Treatment in an Alloy Al64Cu27Fe15
    Nascimento, Luciano
    ORBITAL-THE ELECTRONIC JOURNAL OF CHEMISTRY, 2020, 12 (04): : 253 - 257