Correlation of Mechanical Properties with Diameter and Cooling Rate of 1080 Wire-Rod

被引:5
|
作者
Kohli, A. [1 ]
Poirier, D. R. [1 ]
机构
[1] Univ Arizona, Dept Mat Sci & Engn, Tucson, AZ 85721 USA
关键词
pearlite transformation; steel; wire-rod; PEARLITIC STEEL WIRES; HIGH-CARBON STEEL; STRENGTH;
D O I
10.1007/s11665-017-3079-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
More than 540 heats of 1080 wire-rod were statistically analyzed by regression analyses to see whether tensile strength and percent reduction in area (%RA) relate to wire-rod diameter and composition. As diameter increases from 5.6 to 12.7 mm, the trend in %RA shows a decrease with negligible effect on the trend of the tensile strength. It was found that the estimated cooling rate at 700 A degrees C during controlled cooling is responsible for the "diameter effect." The effect of composition on %RA is minor when contrasted to the "diameter effect." In particular, the effect of the concentrations of the residual elements on %RA within the compositional range studied is negligible.
引用
收藏
页码:5871 / 5876