Interlaminar fracture toughness of carbon fibre composites with electrospun nanofibrous interleaves of polystyrene and cellulose nanocrystals

被引:3
|
作者
Kanari, Konstantina [1 ]
Wisnom, Michael R. [1 ]
Harniman, Robert [2 ]
Eichhorn, Stephen J. [1 ]
机构
[1] Univ Bristol, Sch Civil Aerosp & Mech Engn, Bristol Composite Inst, Bristol BS8 1TS, Avon, England
[2] Univ Bristol, Sch Chem, Bristol BS8 1TS, Avon, England
基金
英国工程与自然科学研究理事会;
关键词
MECHANICAL-PROPERTIES; MODE-I; SURFACE-MORPHOLOGY; REINFORCEMENT; DEFORMATION; DELAMINATION; DENSITY; MICROMECHANISMS; ORIENTATION; PARAMETERS;
D O I
10.1007/s10853-022-07953-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Polystyrene nanofibres reinforced with cellulose nanocrystals have been produced by electrospinning. Two different orientations of the nanofibres were produced, namely aligned and random, and these nanofibrous interleaves were investigated both as-spun and after thermal treatment. Aligned nanofibres exhibited a 2500% increase in their Young's modulus compared to the randomly orientated materials, while the ultimate tensile strength increased by up to 300%. It is also demonstrated that crazing occurs in the nanofibres, which is thought to enhance the fracture properties of the materials. Interleaves of both orientations were then included in a carbon fibre-reinforced polymer laminate. The fracture toughness of the laminate was determined under both mode I and mode II testing. No increases in mode I toughness were observed. It was, however, found that the aligned interleaves increased the mode II toughness of the composite laminate (from 1.9 +/- 0.3 to 2.7 +/- 0.2 kJ m(-2)). This increase is demonstrated to be due to a combination of nanofibre bridging and the formation of microcracks in the resin under applied tensile and shear load.
引用
收藏
页码:21080 / 21103
页数:24
相关论文
共 50 条
  • [21] Preparation of highly electrically conductive carbon-fiber composites with high interlaminar fracture toughness by using silver-plated interleaves
    Guo, Miaocai
    Yi, Xiaosu
    Rudd, Chris
    Liu, Xiaoling
    COMPOSITES SCIENCE AND TECHNOLOGY, 2019, 176 : 29 - 36
  • [22] Carbon nanotube shear-pressed sheet interleaves for Mode I interlaminar fracture toughness enhancement
    Stahl, James J.
    Bogdanovich, Alexander E.
    Bradford, Philip D.
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2016, 80 : 127 - 137
  • [23] A review on mode-I interlaminar fracture toughness of fibre reinforced composites
    Nasuha, N.
    Azmi, A. I.
    Tan, C. L.
    INTERNATIONAL CONFERENCE ON APPLICATIONS AND DESIGN IN MECHANICAL ENGINEERING (ICADME 2017), 2017, 908
  • [24] Dependence on fibre type of interlaminar fracture toughness enhancement in interleaved polymer composites
    Vallack, Nicola
    Potluri, Prasad
    Sampson, William W.
    COMPOSITES SCIENCE AND TECHNOLOGY, 2023, 241
  • [25] Enhancing interlaminar fracture toughness of woven carbon fibre/epoxy composites with engineering thermoplastic and carbon-based nanomaterials
    Tangthana-umrung, Kanokporn
    Mahmood, Humza
    Zhang, Xiaomeng
    Gresil, Matthieu
    COMPOSITE STRUCTURES, 2022, 282
  • [26] Effect of Paper or Silver Nanowires-Loaded Paper Interleaves on the Electrical Conductivity and Interlaminar Fracture Toughness of Composites
    Guo, Miaocai
    Yi, Xiaosu
    AEROSPACE, 2018, 5 (03)
  • [27] Mode II interlaminar fracture toughness of woven E-glass/epoxy composites in the presence of mat interleaves
    Hosseini, Mohammad Reza
    Taheri-Behrooz, Fathollah
    Salamat-Talab, Mazaher
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2020, 98 (98)
  • [28] FRACTOGRAPHY OF THE INTERLAMINAR FRACTURE OF CARBON-FIBRE EPOXY COMPOSITES
    BASCOM, WD
    BOLL, DJ
    FULLER, B
    PHILLIPS, PJ
    JOURNAL OF MATERIALS SCIENCE, 1985, 20 (09) : 3184 - 3190
  • [29] INTERLAMINAR FRACTURE MORPHOLOGY OF CARBON FIBRE/PEEK COMPOSITES.
    Crick, R.A.
    Leach, D.C.
    Meakin, P.J.
    Moore, D.R.
    1600, (22):
  • [30] STRENGTH AND FRACTURE TOUGHNESS OF CARBON FIBRE POLYESTER COMPOSITES
    HARRIS, B
    BEAUMONT, WR
    MONCUNIL.E
    JOURNAL OF MATERIALS SCIENCE, 1971, 6 (03) : 238 - &