Effects of substituting Ni with Cu on the microstructures and electrochemical characteristics of the as-cast and quenchedLa0.7Mg0.3Ni2.55-xCo0.45Cux(x=0-0.4)electrode alloys

被引:23
|
作者
Zhang, Yang-huan
Li, Bao-wei
Ren, Hui-ping
Cai, Ying
Dong, Xiao-ping
Wang, Xin-lin
机构
[1] Cent Iron & Steel Res Inst, Dept Funct Mat Res Ctr, Beijing 100081, Peoples R China
[2] Inner Mongolia Univ Sci & Technol, Sch Mat, Baotou 01410, Peoples R China
[3] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
La-Mg-Ni-based hydrogen storage alloy; substitution of Cu for Ni; microstructure; electrochemical characteristic;
D O I
10.1016/j.ijhydene.2007.03.008
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The La-Mg-Ni-based PuNi3-type La0.7Mg0.3Ni2.55-xCo0.45Cux (x=0, 0.1, 0.2, 0.3, 0.4) hydrogen storage alloys were prepared by casting and rapid quenching. Ni in the alloy was partly substituted by Cu in order to improve the cycle stabilities of the alloys. The effects of the substitution of Cu for Ni on the microstructures and electrochemical performances of the as-cast and quenched alloys were investigated in detail. The results obtained by XRD, SEM and TEM show that the as-cast and quenched alloys have a multiphase structure which is composed of two main phases (La, Mg)Ni-3 and LaNi5 as well as a residual phase LaNi2. The substitution of Cu for Ni leads to an obvious increase of the LaNi2 phase in the as-cast alloys, and it also helps the formation of a desired amorphous phase in the as-quenched alloy. The results of the electrochemical measurement indicate that the substitution of Cu for Ni obviously decreases the discharge capacities of the as-cast and quenched alloys, but it significantly improves their cycle stabilities. The substitution of Cu for Ni slightly improves the discharge potential characteristics and the activation capabilities of the as-cast alloys, but it leads to reversal results for the as-quenched alloys. (C) 2007 International Association for Hydrogen Energy. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:3420 / 3426
页数:7
相关论文
共 50 条
  • [21] Microstructure and electrochemical performances of La0.7Mg0.3Ni2.55-xCo0.45Mx (M = Cu, Cr, Al; x=0-0.4) hydrogen storage alloys prepared by casting and rapid quenching
    Zhang, Yang-Huan
    Li, Bao-Wei
    Cai, Ying
    Dong, Xiao-Ping
    Ren, Jiang-Yuan
    Wang, Xin-Lin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 458 (1-2): : 67 - 72
  • [22] Investigation on structures and electrochemical characteristics of the as-cast and quenched La0.5Ce0.2Mg0.3Co0.4Ni2.6-xMnx (x=0-0.4) electrode alloys
    Zhang, Yang-huan
    Li, Bao-wei
    Ren, Hui-ping
    Wu, Zhong-wang
    Dong, Xiao-ping
    Wang, Xin-lin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 461 (1-2) : 591 - 597
  • [23] The effect of Mn substitution for Ni on the structural and electrochemical properties of La0.7Mg0.3Ni2.55-xCo0.45Mnx hydrogen storage electrode alloys
    Liu, YF
    Pan, HG
    Gao, MX
    Zhu, YF
    Lei, YQ
    Wang, QD
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2004, 29 (03) : 297 - 305
  • [24] Effects of the substitution of Mn for Ni on structures and electrochemical performances of the as-cast and quenched La0.5Ce0.2Mg0.3Co0.4Ni2.6-xMnx (x=0-0.4) electrode alloys
    Li, Bao-wei
    Zhang, Yang-huan
    Wu, Zhong-wang
    Shi, Yan-chun
    Pang, Zai-guang
    Wang, Xin-lin
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2008, 33 (01) : 141 - 148
  • [25] Effect of Mn content on the structure and electrochemical characteristics of La0.7Mg0.3Ni2.975-xCo0.525Mnx (x=0-0.4) hydrogen storage alloys
    Zhang, XB
    Sun, DZ
    Yin, WY
    Chai, YJ
    Zhao, MS
    ELECTROCHIMICA ACTA, 2005, 50 (14) : 2911 - 2918
  • [26] Cycle Stabilities of La0.7Mg0.3Ni2.55-xCo0.45Mx (M=Fe, Cu, Al;x=0, 0.1) Electrode Alloys Prepared by Casting and Rapid Quenching
    张羊换
    赵栋梁
    董小平
    郭世海
    祁焱
    王新林
    Journal of Rare Earths, 2007, (S1) : 419 - 425
  • [27] La0.7Mg0.3Ni2.55-xCo0.45Alx(x=0~0.4)贮氢合金的循环稳定性
    张羊换
    任慧平
    李保卫
    董小平
    赵小龙
    王新林
    中国有色金属学报, 2006, (08) : 1320 - 1325
  • [28] Cycle Stabilities of La0.7Mg0.3Ni2.55-xCo0.45Mx (M = fe, cu, al; x=0, 0.1) electrode alloys prepared by casting and rapid quenching
    Zhang Yanghuan
    Zhao Dongliang
    Dong Xiaoping
    Guo Shihai
    Qi Yan
    Xinlin, Wang
    JOURNAL OF RARE EARTHS, 2007, 25 : 419 - 425
  • [29] Effects of rapid quenching on structure and electrochemical characteristics of La0.5Ce0.2Mg0.3Co0.4Ni2.6-xMnx (x=0-0.4) electrode alloys
    Zhang Yang-huan
    Zhao Dong-liang
    Dong Xiao-ping
    Qi Yan
    Guo Shi-hai
    Wang Xin-lin
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2009, 19 (02) : 364 - 371
  • [30] Effects of rapid quenching on structure and electrochemical characteristics of La0.5Ce0.2Mg0.3Co0.4Ni2.6-xMnx(x=0-0.4) electrode alloys
    张羊换
    赵栋梁
    董小平
    祁焱
    郭世海
    王新林
    TransactionsofNonferrousMetalsSocietyofChina, 2009, 19 (02) : 364 - 371