Vacuum Brazing of Metallized YSZ and Crofer Alloy Using 72Ag-28Cu Filler Foil

被引:2
|
作者
Huang, Liang-Wei [1 ,2 ]
Shiue, Ren-Kae [1 ]
Liu, Chien-Kuo [2 ]
Cheng, Yung-Neng [2 ]
Lee, Ruey-Yi [2 ]
Tsay, Leu-Wen [3 ]
机构
[1] Natl Taiwan Univ, Dept Mat Sci & Engn, Taipei 10617, Taiwan
[2] Inst Nucl Energy Res, Nucl Fuels & Mat Div, Taoyuan 32546, Taiwan
[3] Natl Taiwan Ocean Univ, Dept Optoelect & Mat Technol, Keelung 20224, Taiwan
关键词
vacuum brazing; metallization; interfacial reaction; gas-tight; COMPRESSIVE SEALS; JOINTS; MICROSTRUCTURE; TEMPERATURE; ELECTROLYTE; INTERFACE; EVOLUTION; CERAMICS; BEHAVIOR; ALUMINA;
D O I
10.3390/ma15030939
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The study focused on dissimilar brazing of metallized YSZ (Yttria-Stabilized Zirconia) and Crofer alloy using BAg-8 (72Ag-28Cu, wt%) filler foil. The YSZ substrate was metallized by sequentially sputtering Ti (0.5/1 mu m), Cu (1/3 mu m), and Ag (1.5/5 mu m) layers, and the Crofer substrate was coated with Ag layers with a thickness of 1.5 and 5 mu m, respectively. The BAg-8 filler demonstrated excellent wettability on both metallized YSZ and Crofer substrates. The brazed joint primarily consisted of Ag-Cu eutectic. The metallized Ti layer dissolved into the braze melt, and the Ti preferentially reacted with YSZ and Fe from the Crofer substrate. The globular Fe2Ti intermetallic compound was observed on the YSZ side of the joint. The interfacial reaction of Ti was increased when the thickness of the metallized Ti layer was increased from 0.5 to 1 mu m. Both brazed joints were crack free, and no pressure drop was detected after testing at room temperature for 24 h. In the YSZ/Ti(0.5 mu)/Cu(1 mu)/Ag(1.5 mu)/BAg-8(50 mu)/Ag(1.5 mu)/Crofer joint tested at 600 degrees C, the pressure of helium decreased from 2.01 to 1.91 psig. In contrast, the helium pressure of the YSZ/Ti(1 mu)/Cu(3 mu)/Ag(5 mu)/BAg-8(50 mu)/Ag(5 mu)/Crofer joint slightly decreased from 2.02 to 1.98 psig during the cooling cycle of the test. The greater interfacial reaction between the metallized YSZ and BAg-8 filler due to the thicker metallized Ti layer on the YSZ substrate was responsible for the improved gas-tight performance of the joint.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] Brazing W and Fe-Ni-Co alloy using Ag-28Cu and Ag-27Cu-3.5Ti fillers
    Shang, Jianli
    Yan, Jiazhen
    Li, Ning
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 611 : 91 - 95
  • [42] Microstructure and Mechanical Property of Titanium Film-Modified Sapphire/High Nb-TiAl Alloy Joints Using Ag-Cu Filler by Vacuum Brazing
    Chen, S. F.
    Wang, Y. S.
    Sun, D. B.
    Xing, X. G.
    Gao, J.
    Hei, H. J.
    Wang, Y. L.
    Yu, S. W.
    Lin, J. P.
    JOM, 2024, 76 (12) : 7304 - 7314
  • [43] Vacuum brazing of Si/SiC ceramic composite and Invar alloy using Ti50Cu-W filler metals
    Huang, J. (jihuahuang47@sina.com), 1600, China Welding, 111 Hexing Road, Harbin, 150080, China (21):
  • [44] Induction brazing of γ-TiAl to alloy steel AISI 4140 using filler metal of eutectic Ag-Cu alloy coated with Ti film
    Koo, JM
    Lee, WB
    Kim, MG
    Kim, DU
    Kim, YJ
    Jung, SB
    MATERIALS TRANSACTIONS, 2005, 46 (02) : 303 - 308
  • [45] Solubility and dissolution rate of Ni base alloy to molten Ag-Cu-Pd brazing filler
    Ikeshoji, TT
    Watanabe, Y
    Suzumura, A
    Yamazaki, T
    JSME INTERNATIONAL JOURNAL SERIES A-SOLID MECHANICS AND MATERIAL ENGINEERING, 2005, 48 (04) : 346 - 351
  • [46] Brazing of diamond to invar with Ag-Cu-Ti filler alloy: Wettability, microstructure and mechanical performance
    Li, Yulong
    Wu, Qi
    Lin, Wei
    Wu, Haoyue
    Tu, Bing
    Zhang, Lin
    Pan, Pan
    Lei, Min
    DIAMOND AND RELATED MATERIALS, 2024, 145
  • [47] Brazing YAG ceramic to Kovar alloy with Ag-Cu-Ti filler alloy: Wettability, microstructure and mechanical properties
    Li, Yulong
    Wang, Cheng
    Li, Xuewen
    Zhang, Lin
    Pan, Pan
    Lei, Min
    VACUUM, 2023, 213
  • [48] Vacuum Brazing of C/C Composite and TiAl Intermetallic Alloy Using BNi-2 Brazing Filler Metal
    Li, Shengnan
    Du, Dong
    Zhang, Lei
    Hao, Qingle
    Long, Weimin
    MATERIALS, 2021, 14 (08)
  • [49] Vacuum brazing of TiB2 cermet to TiAl-based alloys using Ag-Cu-Zn filler metal
    Li, ZR
    Feng, JC
    Cao, J
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2003, 13 : 39 - 41
  • [50] Vacuum brazing of electroless Ni-P alloy-coated SiCp/Al composites using aluminum-based filler metal foil
    Wang, Peng
    Xu, Dongxia
    Niu, Jitai
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2016, 122 (12):