Repair of Bulk-Fill and Nanohybrid Resin Composites: Effect of Surface Conditioning, Adhesive Promoters, and Long-Term Aging

被引:9
|
作者
Ugurlu, Muhittin [1 ]
Husain, Nadin Al-Haj [2 ,3 ]
Oezcan, Mutlu [3 ]
机构
[1] Suleyman Demirel Univ, Fac Dent, Dept Restorat Dent, TR-32200 Isparta, Turkey
[2] Univ Bern, Sch Dent Med, Dept Reconstruct Dent & Gerodontol, CH-3010 Bern, Switzerland
[3] Univ Zurich, Ctr Dent Med, Div Dent Biomat, Clin Reconstruct Dent, CH-8032 Zurich, Switzerland
关键词
air-abrasion; aged resin composite; dental materials; diamond bur; durability; minimally invasive dentistry; restorative dentistry; silane; universal adhesive; BOND STRENGTH; INTERMEDIATE AGENTS; RESTORATIONS; SILANE; DURABILITY; LONGEVITY; PROTOCOLS;
D O I
10.3390/ma15134688
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The aim of the study was to investigate the effect of different repair procedures on the repair bond strength of bulk-fill and nanohybrid resin composites after different aging periods. The resin composite blocks (8 x 8 x 4 mm(3)) were prepared from a bulk-fill (reliaFIL Bulk) and a nanohybrid (reliaFIL LC) resin composite and grouped according to aging duration (6 months, 1 year, and 2 years). Following aging, the blocks were assigned to different surface treatments; air-abrasion with aluminum oxide powder, roughening with a diamond bur, and no treatment. After cleansing with phosphoric acid, a silane layer (Porcelain Primer) was applied on the surface of half of the specimens in each group. The specimens were subdivided into two groups (n = 5): Scotchbond Universal (3M Oral Care) and All-Bond Universal (Bisco). The blocks were repaired with the nanohybrid composite (8 x 8 x 8 mm (3)). The repaired specimens were stored in distilled water (37 degrees C/24 h) and segmented into beams. Half of the beams were immediately subjected to microtensile mu TBS testing (1 mm/min), while the other half was stored in distilled water (37 degrees C) for 6 months before testing. Failure modes were analyzed using stereomicroscope and SEM. Statistical analyses were performed with ANOVA and least significant difference tests (LSD) tests (p = 0.05). The extension of aging periods (6 months, 1 year, and 2 years) reduced the repair bond strength in some groups for both resin composites (p < 0.05). The air-abrasion and bur roughening improved the repair bond strength (p < 0.05). The silane application did not influence the repair bond strength and durability (p > 0.05). There was no difference among the universal adhesives in the same surface treatment groups (p > 0.05). The mechanical roughening treatments are necessary for the repair of resin composite. The universal adhesives might be used for the repair of resin composites regardless of silane content without prior silane application.
引用
收藏
页数:13
相关论文
共 50 条
  • [11] Regional ultimate tensile strength and water sorption/solubility of bulk-fill and conventional resin composites: The effect of long-term water storage
    Rummani, Ghassan
    Ide, Kurumi
    Hosaka, Keiichi
    Tichy, Antonin
    Abdou, Ahmed
    Otsuki, Masayuki
    Nakajima, Masatoshi
    DENTAL MATERIALS JOURNAL, 2021, 40 (06) : 1394 - 1402
  • [12] Effect of tooth brushing on gloss retention and surface roughness of five bulk-fill resin composites
    O'Neill, Catherine
    Kreplak, Laurent
    Rueggeberg, Frederick A.
    Labrie, Daniel
    Shimokawa, Carlos Alberto Kenji
    Price, Richard Bengt
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2018, 30 (01) : 59 - 69
  • [13] Repair potential of a bulk-fill resin composite: Effect of different surface-treatment protocols
    Akgul, Sinem
    Alp, Cemile Kedici
    Bala, Oya
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2021, 129 (06)
  • [14] Surface roughness and oxygen inhibited layer control in bulk-fill and conventional nanohybrid resin composites with and without polishing: in vitro study
    Gaviria-Martinez, Andrea
    Castro-Ramirez, Leonor
    Ladera-Castaneda, Marysela
    Cervantes-Ganoza, Luis
    Cachay-Criado, Hernan
    Alvino-Vales, Maria
    Garcia-Luna, Goretty
    Lopez-Gurreonero, Carlos
    Cornejo-Pinto, Alberto
    Cayo-Rojas, Cesar F.
    BMC ORAL HEALTH, 2022, 22 (01)
  • [15] Surface roughness and oxygen inhibited layer control in bulk-fill and conventional nanohybrid resin composites with and without polishing: in vitro study
    Andrea Gaviria-Martinez
    Leonor Castro-Ramirez
    Marysela Ladera-Castañeda
    Luis Cervantes-Ganoza
    Hernán Cachay-Criado
    María Alvino-Vales
    Goretty Garcia-Luna
    Carlos López-Gurreonero
    Alberto Cornejo-Pinto
    César F. Cayo-Rojas
    BMC Oral Health, 22
  • [16] Effect of Shortened Light-Curing Modes on Bulk-Fill Resin Composites
    Sampaio, C. S.
    Pizarro, P. G.
    Atria, P. J.
    Hirata, R.
    Giannini, M.
    Mahn, E.
    OPERATIVE DENTISTRY, 2020, 45 (05) : 496 - 505
  • [17] Effect of Fibres on Physico-Mechanical Properties of Bulk-Fill Resin Composites
    Alshabib, Abdulrahman
    Silikas, Nick
    Algamaiah, Hamad
    Alayad, Abdullah S.
    Alawaji, Rahaf
    Almogbel, Shaikha
    Aldosari, Ahad
    Alhotan, Abdulaziz
    POLYMERS, 2023, 15 (16)
  • [18] The Effect of Gravity on Marginal Integrity of Different Flowable Bulk-Fill Resin Composites
    Baltacioglu, Ismail Hakki
    Demirel, Gulbike
    Kolsuz, Mehmet Eray
    Orhan, Kaan
    MEDICINA-LITHUANIA, 2024, 60 (03):
  • [19] Effect of Light Curing Distance on Microhardness Profiles of Bulk-Fill Resin Composites
    Hasanain, Fatin A.
    Nassar, Hani M.
    Ajaj, Reem A.
    POLYMERS, 2022, 14 (03)
  • [20] Effect of Finishing Systems on Surface Roughness and Gloss of Full-Body Bulk-Fill Resin Composites
    Paolone, Gaetano
    Moratti, Eugenio
    Goracci, Cecilia
    Gherlone, Enrico
    Vichi, Alessandro
    MATERIALS, 2020, 13 (24) : 1 - 9