Impact of mechanical activation on sintering kinetics and mechanical properties of ultrafine-grained 95W-Ni-Fe tungsten heavy alloys

被引:34
|
作者
Chuvil'deev, V. N. [1 ]
Nokhrin, A., V [1 ]
Boldin, M. S. [1 ]
Baranov, G., V [2 ]
Sakharov, N., V [1 ]
Belov, V. Yu [2 ]
Lantsev, E. A. [1 ]
Popov, A. A. [1 ]
Melekhin, N., V [1 ]
Lopatin, Yu G. [1 ]
Blagoveshchenskiy, Yu, V [3 ]
Isaeva, N., V [3 ]
机构
[1] Lobachevsky State Univ Nizhny Novgorod, Nizhnii Novgorod, Russia
[2] Russian Fed Nucl Ctr, All Russian Res Inst Expt Phys, Sarov, Nizhny Novgorod, Russia
[3] Russian Acad Sci, AA Baykov Inst Met & Mat Sci, Moscow, Russia
关键词
Tungsten alloys; Mechanical activation; Spark plasma sintering; Diffusion; Grain boundaries; Strength; DENSIFICATION BEHAVIOR; TENSILE PROPERTIES; MICROSTRUCTURE; PHASE; BOUNDARIES; COMPOSITE; POWDERS; CONSOLIDATION; SEGREGATION; NANOPOWDERS;
D O I
10.1016/j.jallcom.2018.09.176
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This paper is a study of sintering mechanisms, structure, and mechanical properties of ultrafine-grained 95W-Ni-Fe tungsten heavy alloys. Powder particle sizes were controlled by mechanical activation (MA) of original coarse-grained components and by addition of ultrafine particles. W-Ni-Fe alloys were obtained by sintering in hydrogen and Spark Plasma Sintering (SPS) in a vacuum. The dependence of ultrafine-grained (UFG) alloy density on sintering temperatures has been found to be non-monotonic with a maximum corresponding to the optimal sintering temperature. It has been demonstrated that the sintering activation energy of UFG alloys is significantly lower than that of coarse-grained alloys. It has been shown that the optimal SPS temperature for mechanically activated nanopowders goes down by 350-400 degrees C in comparison with the optimal sintering temperature in hydrogen for coarse-grained 95W-Ni-Fe powder composition. The reason for a lower optimal sintering temperature lies in a decreased activation energy of grain-boundary diffusion and formation of a non-equilibrium solid solution of nickel and iron in the surface layer of tungsten ci-W particles during high-energy MA. High-energy MA and SPS were used to obtain samples of UFG tungsten alloys with high mechanical properties: macro-elastic limit - up to 2250 MPa, yield stress - up to 2500 MPa. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:666 / 688
页数:23
相关论文
共 50 条
  • [21] Microstructure and mechanical properties of ultrafine-grained Fe-14Cr and ODS Fe-14Cr model alloys
    Auger, M. A.
    Leguey, T.
    Munoz, A.
    Monge, M. A.
    de Castro, V.
    Fernandez, P.
    Garces, G.
    Pareja, R.
    JOURNAL OF NUCLEAR MATERIALS, 2011, 417 (1-3) : 213 - 216
  • [22] Effects of reinforcing tungsten fibers and skeleton pre-sintering temperature on microstructure, mechanical and electrical properties of ultrafine-grained tungsten-copper composites
    Ji, Kaile
    Zhang, Yiheng
    Chen, Bingqing
    Zhang, Qiqi
    Xi, Aiying
    Zhao, Zhao
    Liu, Changgen
    Sun, Jiacheng
    Fang, De
    Wang, Qinghao
    Zhan, Mingrui
    Zhuo, Longchao
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2022, 108
  • [23] Microstructure and mechanical properties of fine-grained W-7Ni-3Fe heavy alloy by spark plasma sintering
    Xiang, D. P.
    Ding, L.
    Li, Y. Y.
    Li, J. B.
    Li, X. Q.
    Li, C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 551 : 95 - 99
  • [24] Effects of Ni/Co ratio and mechanical alloying on characteristics and sintering behavior of W-Ni-Co tungsten heavy alloys
    Chen, Chun-Liang
    Ma, Shih-Hsun
    Journal of Alloys and Compounds, 2017, 711 : 488 - 494
  • [25] Electrical Conductivity of Ultrafine-Grained Cu and Al Alloys: Attaining the Best Compromise with Mechanical Properties
    Gonzalez-Hernandez, Joaquin E.
    Cubero-Sesin, Jorge M.
    MATERIALS TRANSACTIONS, 2023, 64 (08) : 1754 - 1768
  • [26] The Effect of Chemical and Phase Composition on Mechanical Properties and Thermal Stability of Ultrafine-Grained Titanium Alloys
    Naydenkin, E. V.
    Mishin, I. P.
    Ratochka, I. V.
    Lykova, O. N.
    PROCEEDINGS OF THE INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS WITH HIERARCHICAL STRUCTURE FOR NEW TECHNOLOGIES AND RELIABLE STRUCTURES 2019, 2019, 2167
  • [27] Shrinkage kinetics during sintering W-Ni-Fe heavy alloy with ultrafine grain
    Wang, Jun
    Zhang, Liying
    Guo, Zhimeng
    Lin, Tao
    Wu, Chengyi
    Wu, Qinghua
    Beijing Keji Daxue Xuebao/Journal of University of Science and Technology Beijing, 2002, 24 (02):
  • [28] Effects of sintering conditions on mechanical properties of mechanically alloyed tungsten heavy alloys
    Ryu, Ho J.
    Hong, Soon H.
    Key Engineering Materials, 2000, 183 (II : 1291 - 1296
  • [29] Effects of sintering conditions on mechanical properties of mechanically alloyed tungsten heavy alloys
    Ho J. Ryu
    Soon H. Hong
    Metals and Materials International, 2001, 7 : 221 - 226
  • [30] Effects of sintering conditions on mechanical properties of mechanically alloyed tungsten heavy alloys
    Ryu, Ho J.
    Hong, Soon H.
    2001, Korean Institute of Metals and Materials (07):