Effect of thermocycling and khat extract staining on the optical and mechanical properties of ceramic materials

被引:0
|
作者
Al Moaleem, Mohammed M. [1 ,5 ]
Alathwani, Abdulaziz A. [2 ]
Alamir, Abdulhamid A.
Alshehri, Mesfer, I [3 ]
Alsaeed, Makiah S. [4 ]
Otudi, Abdullah S. A. [2 ]
Munthiri, Hussain A. [2 ]
Atiah, Saleem A.
Yamani, Aisha M.
Madkhali, Zainab M. [2 ]
Arishi, Majid A. [2 ]
机构
[1] Jazan Univ, Dept Prosthet Dent Sci, Coll Dent, Jazan 45142, Saudi Arabia
[2] Jazan Univ, Coll Dent, Jazan, Saudi Arabia
[3] Minist Hlth, Abha, Asseir, Saudi Arabia
[4] Jazan Armed Force Hosp, Dent Dept, Abo Arish, Jazan, Saudi Arabia
[5] Ibn Al Nafis Univ, Coll Dent, Sanaa, Yemen
关键词
color measurements; feldspathic ceramic; khat; opalescence parameter; thermocycling; translucency parameter; zirconia; IN-VITRO; COLOR; TRANSLUCENCY; STABILITY;
D O I
暂无
中图分类号
R-3 [医学研究方法]; R3 [基础医学];
学科分类号
1001 ;
摘要
Background: Color stability of CAD/CAM prosthetic materials is important for long-term clinical and survival success during daily chewing habit. Aims: To assess the effects and outcome of thermocycling and khat extract (KE) staining on the optical (i.e., TP and OP) and physical properties of multilayer zirconia and feldspathic CAD/CAM ceramic. Methods: Forty specimens with dimensions of 16 mm x 12 mm x 1.8 mm were produced from multilayer zirconia and feldspathic CAD/CAM ceramic materials. Specimen's surfaces were prepared in glazed and polished forms. Before thermocycling, the color parameters of specimens were measured using a spectrophotometer, again and after the thermal aging process, the color measurement was recorded and analyzing the collected data using descriptive statistics, correlation, one-way ANOVA, and Tukey's tests. Results: After thermocycling and KE staining, the color parameters L, a, and b decreased, and Delta L*, Delta a* Delta b* had significant differences between groups (p values >= 0.050). Polished surfaces had higher TPs compared with glazed surfaces. OP values ranged from 22.1 to 16.2 and were higher in glazed than in polished surfaces. Glazed and polished zirconia (777.42 +/- 72.67N and 533 +/- 50.71 N) had significantly higher compressive fracture forces compared with glazed and polished Vita Triluxe (396.25 +/- 42.24N and 338.66 +/- 40.17N). Conclusion: KE staining and thermocycling caused slight color changes in TP and OP values, which were high in polished surfaces. TP and OP values were reduced after KE immersion and thermocycling. Compressive forces were under clinically accepted values for zirconia and less than half values for Vita Triluxe specimens. The three types of failures were presented.
引用
收藏
页码:3146 / 3156
页数:11
相关论文
共 50 条
  • [21] Evaluation of Mechanical Properties of Different Thermoplastic Orthodontic Retainer Materials after Thermoforming and Thermocycling
    Albilali, Alaa T.
    Baras, Bashayer H.
    Aldosari, Mohammad A.
    POLYMERS, 2023, 15 (07)
  • [22] The Effect of Thermocycling and Mechanical Loading on the Fracture Resistance of Graphene and All-Ceramic Anterior Crowns
    Reddy, Karri Akhil Sai
    Prasad, B. Rajendra
    Darshini, Reddy Priya
    Challa, Sai Ram
    Charishma, Mondreti Naga
    Sowjanya, Sangani
    Devi, Kakarlapudi Akhila
    Turlapati, Sai Swetha
    Teja, Pathuri Raveen
    CUREUS JOURNAL OF MEDICAL SCIENCE, 2024, 16 (05)
  • [23] Evaluation of Color Changes and Surface Topography of Different Feldspathic Ceramic Materials After Khat, Catha edulis Extract Immersion
    Al Moaleem, Mohammed M.
    Homeida, Husham E.
    Dafalla, Omer M.
    Alamir, Omar H. A.
    Dahas, Zarah A. H.
    Alqasemi, Wesam I. Q.
    Al-Sanabani, Fuad A.
    BIOSCIENCE BIOTECHNOLOGY RESEARCH COMMUNICATIONS, 2020, 13 (01): : 160 - 168
  • [24] EFFECT OF MODIFIERS ON PROPERTIES OF CERAMIC MATERIALS
    Shirinzade, I. N.
    Mammadova, I. H.
    Lutfalizad, F. Z.
    CHEMICAL PROBLEMS, 2016, (02): : 199 - 202
  • [25] Exploration on Thermal Shock Mechanical Properties of Ceramic Materials
    Wang, Yanxia
    Sun, Tiantian
    Shang, Qinghui
    Bao, Yongli
    Ma, Xiaomin
    PROCEEDINGS OF THE 2015 INTERNATIONAL CONFERENCE ON MATERIALS, ENVIRONMENTAL AND BIOLOGICAL ENGINEERING, 2015, 10 : 52 - 55
  • [26] Preparation of superhard ceramic materials and evaluation of their mechanical properties
    Itoh, H
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2004, 112 (1303) : 121 - 129
  • [27] INVESTIGATION OF THE MECHANICAL-PROPERTIES OF CERAMIC BREEDER MATERIALS
    DIENST, W
    ZIMMERMANN, H
    JOURNAL OF NUCLEAR MATERIALS, 1988, 155 : 476 - 479
  • [28] Technology and mechanical properties of ceramic preforms for composite materials
    Naplocha, K
    Janus, A
    Kaczmar, JW
    Samsonowicz, Z
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2000, 106 (1-3) : 119 - 122
  • [29] Study of the mechanical properties of ceramic materials by the nanoindentation technique
    Woirgard, J
    Tromas, C
    Girard, JC
    Audurier, V
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1998, 18 (15) : 2297 - 2305
  • [30] Effect of Silane Treatment on Mechanical Properties of Polymer-infiltrated Ceramic Dental Materials
    Shin, Ji-Yeon
    Lee, Deuk Yong
    Song, Yo-Seung
    Kim, Bae-Yeon
    POLYMER-KOREA, 2018, 42 (06) : 967 - 973