Damp-heat induced degradation in photovoltaic modules manufactured with passivated emitter and rear contact solar cells

被引:17
|
作者
Kyranaki, Nikoleta [1 ]
Smith, Alex [1 ]
Yendall, Keith [2 ]
Hutt, David A. [3 ]
Whalley, David C. [3 ]
Gottschalg, Ralph [4 ,5 ]
Betts, Thomas R. [1 ]
机构
[1] Loughborough Univ, Ctr Renewable Energy Syst Technol CREST, Loughborough LE11 3TU, Leics, England
[2] Loughborough Univ, Dept Mat, Loughborough, Leics, England
[3] Loughborough Univ, Wolfson Sch Mech Elect & Mfg Engn, Loughborough, Leics, England
[4] Fraunhofer Ctr Silicon Photovolta CSP, Halle, Germany
[5] Anhalt Univ Appl Sci, Dept Elect Mech & Econ Engn, Kothen, Germany
来源
PROGRESS IN PHOTOVOLTAICS | 2022年 / 30卷 / 09期
基金
欧盟地平线“2020”;
关键词
corrosion; damp-heat; durability; PERC; PV modules; SILICON; IMPACT;
D O I
10.1002/pip.3556
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Corrosion is one of the main PV module failure mechanisms, as it can cause severe electrical performance degradation in PV modules exposed to hot and humid environments. Moisture penetrating a photovoltaic (PV) module may react with the metallic components causing corrosion. In addition, acetic acid which is produced by hydrolysis of ethylene vinyl acetate (EVA), the most common encapsulant, may further degrade metallic components. Corrosion is one of the main PV module failure mechanisms, as it can cause severe electrical performance degradation in PV modules exposed to hot and humid environments. The specific chemical reactions involved in the corrosion mechanisms for the different components are well understood. However, which of these causes the most serious degradation in the field, and therefore, most severe power loss is unknown. Moreover, the severity of corrosion in the absence of acetic acid is not yet well researched. This work distinguished between the front and rear side corrosion mechanisms and identified the different electrical signatures observed due to them. The experiment included damp-heat (DH) conditioning of single-cell mini-modules, containing passivated emitter and rear contact (PERC) solar cells, laminated with a polyethylene terephthalate (PET) based backsheet. Furthermore, half-encapsulated PERC PV cells were tested, with either the front or the rear side exposed. Electrical and material characterisation were conducted for the investigation of the sample degradation, and the performance decrease, related to the degradation of the rear surface passivation, was examined.
引用
收藏
页码:1061 / 1071
页数:11
相关论文
共 50 条
  • [21] Unveiling the origin of metal contact failures in TOPCon solar cells through accelerated damp-heat testing
    Wu, Xinyuan
    Sen, Chandany
    Wang, Xutao
    Cheng, Yuhao
    Lv, Ruirui
    Song, Hao
    Yu, Yuanjie
    Liao, Baochen
    Ma, Sheng
    Khan, Muhammad Umair
    Ciesla, Alison
    Hoex, Bram
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2024, 278
  • [22] Crystal Symmetry-Inspired Algorithm for Optimal Design of Contemporary Mono Passivated Emitter and Rear Cell Solar Photovoltaic Modules
    Vais, Ram Ishwar
    Sahay, Kuldeep
    Chiranjeevi, Tirumalasetty
    Devarapalli, Ramesh
    Knypinski, Lukasz
    ALGORITHMS, 2024, 17 (07)
  • [23] Damp-Heat Induced Performance Degradation for InGaP/GaAs/Ge Triple-Junction Solar Cell
    Hong, Hwen-Fen
    Huang, Tsung-Shiew
    Uen, Wu-Yih
    Chen, Yen-Yeh
    JOURNAL OF NANOMATERIALS, 2014, 2014
  • [24] Acetic acid detection in photovoltaic modules during ultraviolet irradiation and damp-heat combined tests
    Asano, Shota
    Hamaoka, Ryo
    Jonai, Sachiko
    Hara, Yukiko
    Masuda, Atsushi
    Umeda, Norihiro
    Iwami, Kentaro
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2022, 61 (06)
  • [25] PRELIMINARY damp-heat stability studies of encapsulated CIGS solar cells
    Sundaramoorthy, R.
    Pern, F. J.
    Gessert, T.
    RELIABILITY OF PHOTOVOLTAIC CELLS, MODULES, COMPONENTS, AND SYSTEMS III, 2010, 7773
  • [26] Characterization of front contact degradation in monocrystalline and multicrystalline silicon photovoltaic modules following damp heat exposure
    Iqbal, Nafis
    Colvin, Dylan J.
    Schneller, Eric J.
    Sakthivel, Tamil S.
    Ristau, Roger
    Huey, Bryan D.
    Yu, Ben X. J.
    Jaubert, Jean-Nicolas
    Curran, Alan J.
    Wang, Menghong
    Seal, Sudipta
    French, Roger H.
    Davis, Kristopher O.
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2022, 235
  • [27] Enhancing Reliability and Regeneration of Single Passivated Emitter Rear Contact Solar Cell Modules through Alternating Current Power Application to Mitigate Light and Elevated Temperature-Induced Degradation
    Jony, Jaljalalul Abedin
    Yousuf, Hasnain
    Zahid, Muhammad Aleem
    Khokhar, Muhammad Quddamah
    Madara, Polgampola Chamani
    Rahman, Rafi Ur
    Kim, Youngkuk
    Aida, Maha Nur
    Sanyal, Simpy
    Park, Sangheon
    Dhungel, Suresh Kumar
    Yi, Junsin
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2024,
  • [28] Effect of Al Contact Pitch on Rear Passivated Solar Cells
    Cesar, I.
    Mewe, A. A.
    Manshanden, P.
    Romijn, I. G.
    Janssen, L.
    Weeber, A. W.
    PROCEEDINGS OF THE SILICONPV 2011 CONFERENCE (1ST INTERNATIONAL CONFERENCE ON CRYSTALLINE SILICON PHOTOVOLTAICS), 2011, 8 : 672 - 680
  • [29] Method and Equipment for Reducing the Efficiency Degradation of Monocrystalline Passivated Emitter and Rear Cells
    Fan, Weitao
    Shen, Honglie
    Zhang, Xin
    Pan, Hong
    ENERGIES, 2024, 17 (07)
  • [30] Pathway towards 24% efficiency for fully screen-printed passivated emitter and rear contact solar cells
    Zhang, Yuchao
    Wang, Li
    Chen, Daniel
    Kim, Moonyong
    Hallam, Brett
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2021, 54 (21)