OPTICAL MICROSCOPY AS A SIMPLE METHOD FOR ANALYSIS OF BOILER TUBE FAILURE

被引:0
|
作者
Jovanovic, Milan T. [1 ]
Miskovic, Zoran [1 ]
Maksimovic, Vesna [1 ]
Cvijovic-Alagic, Ivana [1 ]
机构
[1] Univ Belgrade, Inst Nucl Sci Vinca, Dept Mat Sci, POB 522, Belgrade 11001, Serbia
关键词
Boiler tube; Austenite; Bainite; Widmanstatten ferrite; Overheating; Failure; TRANSFORMATION;
D O I
10.30544/461
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A severely damaged low carbon steel boiler tube was the object of this investigation. Detailed microstructural characterization was performed by optical microscopy, whereas scanning electron microscopy (SEM) was applied only in a few cases. Results show that a variety of microstructures was formed in the material of the damaged boiler tube during its exploitation. The failure of the tube is the result of very inhomogeneous overheating. The side of the boiler tube toward fire (F) was exposed to high overheating temperature, which in some locations was well above the A(3) transformation temperature. The side toward boiler (BL) was subjected to lower temperatures, i.e. in the region mostly between A(1) and A(3) temperatures. Variations in temperatures and cooling rates, which resulted in microstructural inhomogeneity, are the main cause for the formation and multiplication of stresses leading to the rupture of the tube.
引用
收藏
页码:301 / 313
页数:13
相关论文
共 50 条
  • [11] Boiler tube failure root cause analysis advisory system
    Gonzalez, H
    Chang, PS
    PROCEEDINGS OF THE TWENTY-NINTH SOUTHEASTERN SYMPOSIUM ON SYSTEM THEORY, 1997, : 201 - 205
  • [12] Boiler Stack Economizer Tube Failure
    Haase, Ryan J.
    Hanke, Larry D.
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2013, 13 (05) : 513 - 520
  • [13] Discussion of 'An Overheat Boiler Tube Failure'
    Tanzer, Aaron
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2006, 6 (02) : 31 - 32
  • [14] Failure Analysis Of Steel Superheater Tube Fractured In A Boiler Of A Power Plant
    Huda, Zainul
    FRACTURE AND STRENGTH OF SOLIDS VII, PTS 1 AND 2, 2011, 462-463 : 467 - 471
  • [15] An investigation of failure analysis of a superheater boiler tube working for 40 months
    Ahmadian, Peyman
    CANADIAN METALLURGICAL QUARTERLY, 2024, 63 (04) : 1347 - 1355
  • [16] Failure Analysis of Welded Joint in Superheater Tube in a Waste Incineration Boiler
    Yongjun Li
    Zhigang Li
    Jiahong Lan
    Hualin Chen
    Zanzan Zhang
    Yezheng Li
    Zongjian Feng
    Shuhai Cen
    Xiaobin Zhang
    Journal of Failure Analysis and Prevention, 2023, 23 : 1452 - 1468
  • [17] Failure Analysis of Welded Joint in Superheater Tube in a Waste Incineration Boiler
    Li, Yongjun
    Li, Zhigang
    Lan, Jiahong
    Chen, Hualin
    Zhang, Zanzan
    Li, Yezheng
    Feng, Zongjian
    Cen, Shuhai
    Zhang, Xiaobin
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2023, 23 (04) : 1452 - 1468
  • [18] Failure analysis of primary waste heat boiler tube in ammonia plant
    Ardy, Husaini
    Putra, Yudhistira Perdana
    Anggoro, Adimas Dwi
    Wibowo, Arie
    HELIYON, 2021, 7 (02)
  • [19] ROOT CAUSE ANALYSIS OF BOILER FINAL SUPERHEATER BENDING TUBE FAILURE
    Tzeng, C. F.
    Kao, C. S.
    Chen, T. T.
    JOINT EPRI - 123HIMAT INTERNATIONAL CONFERENCE ON ADVANCES IN HIGH-TEMPERATURE MATERIALS, 2019, 2019, : 715 - 725
  • [20] Oxygen pitting failure of a bagasse boiler tube
    Heyes, AM
    ENGINEERING FAILURE ANALYSIS, 2001, 8 (02) : 123 - 131