共 50 条
- [21] Hydrogen-induced wear of Ti-6Al-4V alloy NEW MATERIALS AND PROCESSES, PTS 1-3, 2012, 476-478 : 566 - +
- [24] Microstructure and mechanical properties of a friction stir processed Ti-6Al-4V alloy MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 573 : 67 - 74
- [26] Microstructure, properties and biocompatibility of the nitrided Ti-6Al-4V alloy for medical application ADVANCED MATERIALS AND TECHNOLOGIES, 2006, 513 : 15 - 24
- [27] Effect of hydrogenation on microstructure and mechanical properties of Ti-6Al-4V titanium alloy ADVANCED ENGINEERING MATERIALS III, PTS 1-3, 2013, 750-752 : 596 - 602
- [28] Microstructure and Corrosion Properties of Ti-6Al-4V alloy by Ultrasonic Shot Peening INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2015, 10 (11): : 9167 - 9178