Tensile Properties and Fracture Behavior of a Powder-Thixoformed 2024Al/SiCp Composite at Elevated Temperatures

被引:7
|
作者
Li, Pubo [1 ]
Chen, Tijun [1 ]
机构
[1] Lanzhou Univ Technol, State Key Lab Adv Proc & Recycling Nonferrous Met, Lanzhou 730050, Gansu, Peoples R China
来源
METALS | 2017年 / 7卷 / 10期
关键词
powder thixoforming; composite; high temperature; tensile properties; fracture; ALUMINUM-MATRIX COMPOSITE; MICROSTRUCTURAL EVOLUTION; MECHANICAL-PROPERTIES; STRENGTHENING MECHANISMS; VOLUME FRACTION; FLOW-STRESS; GRAIN-SIZE; ALLOY; DEFORMATION; ENERGY;
D O I
10.3390/met7100408
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present work, the tensile properties and fracture behavior of a 2024Al composite reinforced with 10 vol % SiCp and fabricated via powder thixoforming (PT) were studied at temperatures ranging from 25 degrees C to 300 degrees C with a strain rate of 0.05 s(-1), as well as the PT 2024 alloy. The results indicated that the tensile strengths of both the PT materials were all decreased with increasing the temperature, but the decrease rate of the composite was smaller than that of the 2024 alloy, and the composite exhibited higher tensile strength than that of the 2024 alloy at all of the employed testing temperatures due to the strengthening role of SiCp. Increasing temperature was beneficial for enhancing the ductility of materials, and the maximum elongation was reached at 250 degrees C. The elongation decrease over 250 degrees C was attributed to the cavity formation due to the debonding of the SiCp/Al interface and the fracturing of the matrix between SiCp. The fracture of the composite at room temperature initiated from the fracture of SiCp and the debonding of the SiCp/Al interface, but that at high temperatures was dominated by void nucleation and growth in the matrix besides the interface debonding.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Effects of particles size on the mechanical properties of SiCp/2024Al composites
    Yu, Xiaodong
    Wang, Yangwei
    Wang, Fuchi
    Zhang, Chi
    Ji, Tao
    Tezhong Zhuzao Ji Youse Hejin/Special Casting and Nonferrous Alloys, 2007, 27 (09): : 672 - 673
  • [32] Dynamic compressive behavior of a 45 vol.% SiCp/2024Al composite at various high strain rates
    Zhu, Y.
    Pang, B.
    Gai, B.
    Wang, L.
    Zhang, W.
    DYMAT 2009: 9TH INTERNATIONAL CONFERENCE ON THE MECHANICAL AND PHYSICAL BEHAVIOUR OF MATERIALS UNDER DYNAMIC LOADING, VOL 1, 2009, : 155 - 161
  • [33] The microstructure and mechanical properties of Al2024-SiCp composite fabricated by powder thixoforming
    Li, Pubo
    Chen, Tijun
    Qin, He
    JOURNAL OF MATERIALS RESEARCH, 2017, 32 (11) : 2079 - 2091
  • [34] Ultrasonic spot welding of dissimilar 2024Al alloy and SiCp/2009Al composite
    Patel, V. K.
    Bhole, S. D.
    Chen, D. L.
    Ni, D. R.
    Xiao, B. L.
    Ma, Z. Y.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2019, 233 (03) : 531 - 538
  • [35] The microstructure and mechanical properties of Al2024-SiCp composite fabricated by powder thixoforming
    Pubo Li
    Tijun Chen
    He Qin
    Journal of Materials Research, 2017, 32 : 2079 - 2091
  • [36] Tensile deformation and fracture behavior of spray-deposition 7075/15SiCp aluminum matrix composite sheet at elevated temperatures
    Zhang, Hui
    He, Yusong
    Li, Luoxing
    MATERIALS CHARACTERIZATION, 2008, 59 (08) : 1078 - 1082
  • [37] Study of flow stress for Al/SiCp composite at elevated temperatures
    Joshi, SS
    Ramakrishnan, N
    Chaturvedi, RC
    Ramakrishnan, P
    PROCESSING, PROPERTIES, AND APPLICATIONS OF CAST METAL MATRIX COMPOSITES, 1996, : 119 - 126
  • [39] Effect of matrix strengthening on sliding wear properties of SiCp/2024Al composites
    Ma, ZY
    Liang, YN
    Lu, YX
    Bi, J
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 1998, 8 (04) : 556 - 561
  • [40] Tensile-properties of SiCp/Al alloy composite
    Ding, Zhanlai
    Fan, Yunchang
    Qi, Haibo
    Ren, Deliang
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 9 (SUPPL. 1): : 265 - 269