Formation of Cr-modified silicide coatings on a Ti-Nb-Si based ultrahigh-temperature alloy by pack cementation process

被引:47
|
作者
Qiao, Yanqiang [1 ]
Guo, Xiping [1 ]
机构
[1] NW Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti-Nb-Si based ultrahigh temperature alloy; Coating structure; Phase constituents; Cr-modified silicide coating; Pack cementation process; OXIDATION-RESISTANT COATINGS; PHASE-EQUILIBRIA; MOLTEN-SALT; BEHAVIOR; NIOBIUM; MICROSTRUCTURE; COMPOSITES; AL; DEPOSITION; ADDITIONS;
D O I
10.1016/j.apsusc.2010.05.091
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Cr-modified silicide coatings were prepared on a Ti-Nb-Si based ultrahigh temperature alloy by Si-Cr co-deposition at 1250 degrees C, 1350 degrees C and 1400 degrees C for 5-20 h respectively. It was found that both coating structure and phase constituents changed significantly with increase in the co-deposition temperature and holding time. The outer layers in all coatings prepared at 1250 degrees C for 5-20 h consisted of (Ti,X)(5)Si(3) (X represents Nb, Cr and Hf elements). (Ti,X)(5)Si(4) was found as the only phase constituent in the intermediate layers in both coatings prepared at 1250 degrees C for 5 and 10 h, but the intermediate layers in the coatings prepared at 1250 degrees C for 15 and 20 h were mainly composed of (Ti,X)(5)Si(3) phase that was derived from the decomposition of (Ti,X)(5)Si(4) phase. In the coating prepared at 1350 degrees C for 5 h, single (Ti X)(5)Si(3) phase was found in its outmost layer, the same as that in the outer layers in the coatings prepared at 1250 degrees C; but in the coatings prepared at 1350 degrees C for 10-20 h, (Nb(1.95)Cr(1.05))Cr(2)Si(3) ternary phase was found in the outmost layers besides (Ti,X)(5)Si(3) phase. In the coatings prepared at 1400 degrees C for 5-20 h, (Nb(1.95)Cr(1.05))Cr(2)Si(3) ternary phase was the single phase constituent in their outmost layers. The phase transformation (Ti,X)(5)Si(4)->(Ti,X)(5)Si(3) + Si occurred in the intermediate layers of the coatings prepared at 1350 and 1400 degrees C with prolonging co-deposition time, similar to the situation in the coatings prepared at 1250 degrees C for 15 and 20 h, but this transformation has been speeded up by increase in the co-deposition temperature. The transitional layers were mainly composed of (Ti,X)(5)Si(3) phase in all coatings. The influence of co-deposition temperature on the diffusion ability of Cr atoms was greater than that of Si atoms in the Si-Cr co-deposition processes investigated. The growth of coatings obeyed inverse logarithmic laws at all three co-deposition temperatures. The Si-Cr co-deposition coating prepared at 1350 degrees C for 10 h showed a good oxidation resistance due to the formation of SiO(2) and Nb, Cr-doped TiO(2) scale after oxidation at 1250 degrees C for 10 h. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:7462 / 7471
页数:10
相关论文
共 50 条
  • [41] Effect of CeO2 on microstructure and oxidation resistance of silicide coatings prepared on Nb-silicide-based ultrahigh temperature alloy
    Zhang, Yi
    Guo, Xi-Ping
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2013, 23 (01): : 99 - 107
  • [42] Oxidation behavior and pack siliconized oxidation-resistant coatings of an Nb-based ultrahigh temperature alloy
    Guo, X. P.
    Zhao, L. X.
    Guan, P.
    Kusabiraki, K.
    PRICM 6: SIXTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-3, 2007, 561-565 : 371 - +
  • [43] Microstructure and ambient mechanical properties of Nb-Ti-Cr-Si based ultrahigh temperature alloy by consumable arc melting
    Guo, Baohui
    Guo, Xiping
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2013, 42 (07): : 1387 - 1392
  • [44] Microstructure and Ambient Mechanical Properties of Nb-Ti-Cr-Si Based Ultrahigh Temperature Alloy by Consumable Arc Melting
    Guo Baohui
    Guo Xiping
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 (07) : 1387 - 1392
  • [45] Study of yttrium and cerium on the oxidation resistance of silicide coatings prepared on Ti-6Al-4V alloy by pack-cementation process
    于文海
    田进
    田伟
    赵俊
    李涌泉
    刘言正
    JournalofRareEarths, 2015, 33 (02) : 221 - 226
  • [46] Study of yttrium and cerium on the oxidation resistance of silicide coatings prepared on Ti-6Al-4V alloy by pack-cementation process
    Yu Wenhai
    Tian Jin
    Tian Wei
    Zhao Jun
    Li Yongquan
    Liu Yanzheng
    JOURNAL OF RARE EARTHS, 2015, 33 (02) : 221 - 226
  • [47] Microstructure Development of Directionally Solidified Nb-Ti-Si Based Ultrahigh Temperature Alloy
    Guo Haisheng Guo Xiping Yao Chengfang State Key Laboratory of Solidification Processing Northwestern Polytechnical University Xian China
    稀有金属材料与工程, 2009, 38(S3) (S3) : 24 - 27
  • [48] Microstructure Development of Directionally Solidified Nb-Ti-Si Based Ultrahigh Temperature Alloy
    Guo Haisheng
    Guo Xiping
    Yao Chengfang
    RARE METAL MATERIALS AND ENGINEERING, 2009, 38 : 24 - 27
  • [49] Effect of Al content on the structure and oxidation resistance of Y and Al modified silicide coatings prepared on Nb-Ti-Si based alloy
    Zhang, Ping
    Guo, Xiping
    CORROSION SCIENCE, 2013, 71 : 10 - 19
  • [50] MICROSTRUCTURE AND OXIDATION BEHAVIOR OF ZrSi2-NbSi2 MULTILAYER COATINGS ON AN Nb-Ti-Si-Cr BASE ULTRAHIGH TEMPERATURE ALLOY
    Li Xuan
    Guo Xiping
    Qiao Yanqiang
    ACTA METALLURGICA SINICA, 2015, 51 (06) : 693 - 700