Formation of Cr-modified silicide coatings on a Ti-Nb-Si based ultrahigh-temperature alloy by pack cementation process

被引:47
|
作者
Qiao, Yanqiang [1 ]
Guo, Xiping [1 ]
机构
[1] NW Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti-Nb-Si based ultrahigh temperature alloy; Coating structure; Phase constituents; Cr-modified silicide coating; Pack cementation process; OXIDATION-RESISTANT COATINGS; PHASE-EQUILIBRIA; MOLTEN-SALT; BEHAVIOR; NIOBIUM; MICROSTRUCTURE; COMPOSITES; AL; DEPOSITION; ADDITIONS;
D O I
10.1016/j.apsusc.2010.05.091
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Cr-modified silicide coatings were prepared on a Ti-Nb-Si based ultrahigh temperature alloy by Si-Cr co-deposition at 1250 degrees C, 1350 degrees C and 1400 degrees C for 5-20 h respectively. It was found that both coating structure and phase constituents changed significantly with increase in the co-deposition temperature and holding time. The outer layers in all coatings prepared at 1250 degrees C for 5-20 h consisted of (Ti,X)(5)Si(3) (X represents Nb, Cr and Hf elements). (Ti,X)(5)Si(4) was found as the only phase constituent in the intermediate layers in both coatings prepared at 1250 degrees C for 5 and 10 h, but the intermediate layers in the coatings prepared at 1250 degrees C for 15 and 20 h were mainly composed of (Ti,X)(5)Si(3) phase that was derived from the decomposition of (Ti,X)(5)Si(4) phase. In the coating prepared at 1350 degrees C for 5 h, single (Ti X)(5)Si(3) phase was found in its outmost layer, the same as that in the outer layers in the coatings prepared at 1250 degrees C; but in the coatings prepared at 1350 degrees C for 10-20 h, (Nb(1.95)Cr(1.05))Cr(2)Si(3) ternary phase was found in the outmost layers besides (Ti,X)(5)Si(3) phase. In the coatings prepared at 1400 degrees C for 5-20 h, (Nb(1.95)Cr(1.05))Cr(2)Si(3) ternary phase was the single phase constituent in their outmost layers. The phase transformation (Ti,X)(5)Si(4)->(Ti,X)(5)Si(3) + Si occurred in the intermediate layers of the coatings prepared at 1350 and 1400 degrees C with prolonging co-deposition time, similar to the situation in the coatings prepared at 1250 degrees C for 15 and 20 h, but this transformation has been speeded up by increase in the co-deposition temperature. The transitional layers were mainly composed of (Ti,X)(5)Si(3) phase in all coatings. The influence of co-deposition temperature on the diffusion ability of Cr atoms was greater than that of Si atoms in the Si-Cr co-deposition processes investigated. The growth of coatings obeyed inverse logarithmic laws at all three co-deposition temperatures. The Si-Cr co-deposition coating prepared at 1350 degrees C for 10 h showed a good oxidation resistance due to the formation of SiO(2) and Nb, Cr-doped TiO(2) scale after oxidation at 1250 degrees C for 10 h. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:7462 / 7471
页数:10
相关论文
共 50 条
  • [1] Y and Al modified silicide coatings on an Nb-Ti-Si based ultrahigh temperature alloy prepared by pack cementation process
    Zhang, Ping
    Guo, Xiping
    SURFACE & COATINGS TECHNOLOGY, 2011, 206 (2-3): : 446 - 454
  • [2] Microstructure of Si-Cr co-deposition coatings on a Ti-Nb-Si based high temperature alloy by pack cementation process
    Qiao, Yan-Qiang
    Guo, Xi-Ping
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2010, 31 (03): : 125 - 131
  • [3] Structure of Al-modified silicide coatings on an Nb-based ultrahigh temperature alloy prepared by pack cementation techniques
    Tian, Xiaodong
    Guo, Xiping
    SURFACE & COATINGS TECHNOLOGY, 2009, 203 (09): : 1161 - 1166
  • [4] Structure and Oxidation Behavior of Zr–Y Modified Silicide Coatings Prepared on an Nb–Ti–Si–Cr Based Ultrahigh Temperature Alloy
    Xuan Li
    Xiping Guo
    Yanqiang Qiao
    Oxidation of Metals, 2015, 83 : 253 - 271
  • [5] FORMATION OF Ge-Y MODIFIED SILICIDE COATINGS ON Nb-Ti-Si BASE ULTRAHIGH TEMPERATURE ALLOY
    Yang Lingxiao
    Guo Xiping
    Qiao Yanqiang
    Pan Ruobing
    ACTA METALLURGICA SINICA, 2013, 49 (11) : 1433 - 1438
  • [6] Oxidation behaviors of Si-Cr Co-deposition coatings on a Ti-Nb-Si based ultrahigh temperature alloy at 1250°C
    Qiao, Yan-Qiang
    Guo, Xi-Ping
    Ren, Jia-Song
    Cailiao Gongcheng/Journal of Materials Engineering, 2010, (02): : 64 - 68
  • [7] Deposition of Cr-modified silicide coatings on Nb-Si system intermetallics
    Chen, Chen
    Zhou, Chungen
    Gong, Shengkai
    Li, Shusuo
    Zhang, Yue
    Xu, Huibin
    INTERMETALLICS, 2007, 15 (5-6) : 805 - 809
  • [8] Aluminide and silicide diffusion coatings by pack cementation for Nb-Ti-Al alloy
    Chaia, N.
    Cury, P. L.
    Rodrigues, G.
    Coelho, G. C.
    Nunes, C. A.
    SURFACE & COATINGS TECHNOLOGY, 2020, 389 (389):
  • [9] Microstructure and high-temperature oxidation-resistant performance of several silicide coatings on Nb-Ti-Si based alloy prepared by pack cementation process
    Li, Jing
    Guo, Xi-Ping
    Key Engineering Materials, 2013, 533 : 145 - 165
  • [10] Structure and Oxidation Behavior of Zr-Y Modified Silicide Coatings Prepared on an Nb-Ti-Si-Cr Based Ultrahigh Temperature Alloy
    Li, Xuan
    Guo, Xiping
    Qiao, Yanqiang
    OXIDATION OF METALS, 2015, 83 (3-4): : 253 - 271