Dry sliding wear characteristics of Al-7Si-0.3Mg alloy with minor additions o f magnesium at high temperature

被引:1
|
作者
Prabhudev, M. S. [1 ]
Kori, S. A. [2 ]
机构
[1] Govt Polytech, Dept Mech Engn, Kalgi, India
[2] Cent Univ Andhra Pradesh CUAP, Anantapur, Andhra Pradesh, India
关键词
High-temperature wear; A356; alloy; microstructure; worn surface; Al-Si alloys; wear rate; frictional force; Al-20%g; MECHANICAL-PROPERTIES; GRAIN-REFINEMENT; ALUMINUM; BEHAVIOR; MICROSTRUCTURE; COPPER; MG;
D O I
10.1080/17515831.2021.1945861
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this paper, effect of minor additions of magnesium content in the form of master alloys on the high-temperature dry sliding wear behaviour for A356 alloy has been reported. Alloy composition, normal pressures and sliding distances on A356 alloy at constant temperature of 300 C was studied. The cast alloys and worn surfaces were characterized by SEM/EDX microanalysis. The results indicate that the wear rate of A356 alloy increases with an increase in normal pressures and sliding distances in all the cases and decreases when 0.7% Mg is added to A356 alloy. The decrease in wear rate after the addition of Mg is mainly due to changes in microstructure which lead to improvement in mechanical properties. Further, worn surface study indicates that the formation of iron-rich oxide layer between the mating surfaces during sliding improves sliding wear performance. [GRAPHICS] .
引用
收藏
页码:2 / 9
页数:8
相关论文
共 50 条
  • [31] Structure and properties of calcium and strontium treated Al-7Si-0.3Mg alloy: A comparison
    Kumari, S.S. Sreeja
    Pillai, R.M.
    Pai, B.C.
    Journal of Alloys and Compounds, 2008, 460 (1-2): : 472 - 477
  • [32] Effect of rare earth Sm on microstructure of Al-7Si-0.3Mg aluminum alloy
    Dong Y.-H.
    Jia Z.-H.
    Wen B.-Y.
    Liu Y.-Y.
    Liu Q.
    Wu J.-Z.
    Gao S.-E.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2020, 30 (03): : 479 - 488
  • [33] Stir cast and extruded Al-7Si-0.3Mg alloy containing iron and beryllium
    Murali, S
    Muthukkaruppan, S
    Raman, KS
    Murthy, KSS
    MATERIALS SCIENCE AND TECHNOLOGY, 1997, 13 (04) : 337 - 342
  • [34] EFFECT OF MAGNESIUM, IRON (IMPURITY) AND SOLIDIFICATION RATES ON THE FRACTURE-TOUGHNESS OF AL-7SI-0.3MG CASTING ALLOY
    MURALI, S
    RAMAN, KS
    MURTHY, KSS
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 151 (01): : 1 - 10
  • [35] Structure and properties of calcium and strontium treated Al-7Si-0.3Mg alloy: A comparison
    Kumari, S. S. Sreeja
    Pillai, R. M.
    Pai, B. C.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 460 (1-2) : 472 - 477
  • [36] Effect of Spinning Deformation Processing on the Wear and Corrosion Properties of Al-7Si-0.3Mg Alloys
    Cheng, Yin Chun
    Lin, Chih Kuang
    Tan, An Hung
    Lin, Jing Chie
    Lee, Sheng Long
    MATERIALS AND MANUFACTURING PROCESSES, 2010, 25 (07) : 689 - 695
  • [37] Effects of Loading and Sliding Speed on the Dry Sliding Wear Behavior of Mg-3Al-0.4Si Magnesium Alloy
    Niu, X. D.
    An, D. Q.
    Han, X.
    Sun, W.
    Su, T. F.
    An, J.
    Li, R. G.
    TRIBOLOGY TRANSACTIONS, 2017, 60 (02) : 238 - 248
  • [38] Thermal Fatigue Crack Propagation Process and Mechanism of Multicomponent Al-7Si-0.3Mg Alloy
    Wang, Zhengjun
    Liu, Xinyang
    Dong, Chen
    Chen, Jie
    Liu, Lianxiang
    CRYSTALS, 2023, 13 (07)
  • [39] Effect of iron and combined iron and beryllium additions on the fracture toughness and microstructures of squeeze-cast Al-7Si-0.3Mg alloy
    Murali, S
    Trivedi, A
    Shamanna, KS
    Murthy, KSS
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1996, 5 (04) : 462 - 468
  • [40] FATIGUE FEATURES AND MECHANISM OF Al-7Si-0.3Mg CAST ALLOY UNDER NONPROPORTIONAL LOADINGS
    Mo Defeng
    He Guoqiu
    Zhu Zhengyu
    Liu Xiaoshan
    Zhang Weihua
    ACTA METALLURGICA SINICA, 2009, 45 (07) : 861 - 865