Dry sliding wear characteristics of Al-7Si-0.3Mg alloy with minor additions o f magnesium at high temperature

被引:1
|
作者
Prabhudev, M. S. [1 ]
Kori, S. A. [2 ]
机构
[1] Govt Polytech, Dept Mech Engn, Kalgi, India
[2] Cent Univ Andhra Pradesh CUAP, Anantapur, Andhra Pradesh, India
关键词
High-temperature wear; A356; alloy; microstructure; worn surface; Al-Si alloys; wear rate; frictional force; Al-20%g; MECHANICAL-PROPERTIES; GRAIN-REFINEMENT; ALUMINUM; BEHAVIOR; MICROSTRUCTURE; COPPER; MG;
D O I
10.1080/17515831.2021.1945861
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this paper, effect of minor additions of magnesium content in the form of master alloys on the high-temperature dry sliding wear behaviour for A356 alloy has been reported. Alloy composition, normal pressures and sliding distances on A356 alloy at constant temperature of 300 C was studied. The cast alloys and worn surfaces were characterized by SEM/EDX microanalysis. The results indicate that the wear rate of A356 alloy increases with an increase in normal pressures and sliding distances in all the cases and decreases when 0.7% Mg is added to A356 alloy. The decrease in wear rate after the addition of Mg is mainly due to changes in microstructure which lead to improvement in mechanical properties. Further, worn surface study indicates that the formation of iron-rich oxide layer between the mating surfaces during sliding improves sliding wear performance. [GRAPHICS] .
引用
收藏
页码:2 / 9
页数:8
相关论文
共 50 条
  • [1] Dry sliding wear characteristics of Al-7Si-0.3Mg alloy with minor additions of magnesium at high temperature
    Prabhudev, M.S.
    Kori, S.A.
    Tribology - Materials, Surfaces and Interfaces, 2022, 16 (01): : 2 - 9
  • [2] Sliding wear characteristics of Al-7Si-0.3Mg alloy with minor additions of copper at elevated temperature
    Kori, S. A.
    Prabhudev, M. S.
    WEAR, 2011, 271 (5-6) : 680 - 688
  • [3] Inhibition of delayed ageing by trace additions in Al-7Si-0.3Mg Cast alloy
    Murali, S.
    Kashyap, K.T.
    Raman, K.S.
    Murthy, K.S.S.
    Scripta metallurgica et materialia, 1993, 29 (11): : 1421 - 1426
  • [4] Study of the influence of mischmetal additions to Al-7Si-0.3Mg (LM 25/356) alloy
    Regional Research Lab , Trivandrum, India
    Metall Mat Trans A Phys Metall Mat Sci, 5 (1283-1292):
  • [5] A study of the influence of mischmetal additions to Al-7Si-0.3Mg (LM 25/356) alloy
    Ravi, M
    Pillai, UTS
    Pai, BC
    Damodaran, AD
    Dwarakadasa, ES
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (05): : 1283 - 1292
  • [6] The effect of Sn additions on the semi-solid microstructure of an Al-7Si-0.3Mg alloy
    Kliauga, AM
    Ferrante, M
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 337 (1-2): : 67 - 72
  • [7] Eutectic Morphology of Al-7Si-0.3Mg Alloys with Scandium Additions
    Phromphong Pandee
    C. M. Gourlay
    S. A. Belyakov
    Ryota Ozaki
    Hideyuki Yasuda
    Chaowalit Limmaneevichitr
    Metallurgical and Materials Transactions A, 2014, 45 : 4549 - 4560
  • [8] Eutectic Morphology of Al-7Si-0.3Mg Alloys with Scandium Additions
    Pandee, Phromphong
    Gourlay, C. M.
    Belyakov, S. A.
    Ozaki, Ryota
    Yasuda, Hideyuki
    Limmaneevichitr, Chaowalit
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (10): : 4549 - 4560
  • [9] Dry sliding wear performance of A356 alloy with minor additions of Magnesium
    Prabhudev, M. S.
    Auradi, V.
    Venkateshwarlu, K.
    Suresha, S. M.
    Kori, S. A.
    DYNAMICS OF MACHINES AND MECHANISMS, INDUSTRIAL RESEARCH, 2014, 592-594 : 175 - +
  • [10] Solutionizing Temperature Effect on the Dry Sliding Wear Performance of Al-7Si-0.3Mg-3Ni Hypoeutectic Alloy
    Raveendranath, Vasudev
    Senan, V. R. Aravind
    Venkateswarlu, K.
    Shankar, Karthik V.
    SILICON, 2023, 15 (09) : 4159 - 4170