Effect of polypropylene fiber length on mechanical and thermal properties of autoclaved aerated concrete

被引:25
|
作者
Pehlivanli, Zuhtu Onur [1 ]
Uzun, Ibrahim [2 ]
机构
[1] Kirikkale Univ, Fac Engn & Architecture, Dept Met & Mat Engn, TR-71450 Kirikkale, Turkey
[2] Kirikkale Univ, Fac Engn & Architecture, Dept Mech Engn, TR-71450 Kirikkale, Turkey
关键词
Autoclaved aerated concrete; Polypropylene fiber; Thermal conductivity; Compressive strength; Flexural strength; STRENGTH; CONDUCTIVITY; BASALT;
D O I
10.1016/j.conbuildmat.2022.126506
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this experimental study, the effect of polypropylene fiber (PF) length on the thermal conductivity, pressure and flexural strength values of autoclaved aerated concrete (AAC) was investigated. The investigation used samples from G2/04, G3/05, and G4/06 classes AAC manufacturing in three different density and compressive strength groups. PF of three different lengths, 3, 6, and 12 mm, were chosen as reinforcement material, and AAC samples were made by adding 1.0% in the same volumetric ratios into the matrix material, taking into consideration their specific gravity. After the samples were kept in curing at 60 degrees C for 4 h, they were cured in an autoclave at 180 degrees C at 11 bar pressure for 7 h. After the autoclave process was completed, the flexural and compressive strength, thermal conductivity values of the samples were tested and the internal structure images were examined with a scanning electron microscope (SEM). It was observed that the flexural and compressive strengths of the samples increased with PF reinforcement in all density groups, while the thermal resistances decreased and the fiber length (for 3, 6 and 12 mm) had a positive effect on the compressive and flexural strengths of all examined AAC classes. It was obtained by 70.4% increase in the compressive and flexural strengths of G2/04 class of AAC samples with 12 mm length PF addition. As the PF length increases, the thermal conductivity values of all samples also increase and the highest thermal conductivity increase was observed in the G5/06 class samples with a value of 20.2%. In general, it was observed that the compressive strength, bending strength and thermal conductivity values of all samples increased depending on the increase in PF length. It has been observed that thermal conductivity values are worsen at more higher rates while the strength values of AAC at all fiber lengths is improves with PF additive.
引用
收藏
页数:7
相关论文
共 50 条
  • [31] Effect of bulk density and moisture content on the properties of autoclaved aerated concrete
    Uncik, Stanislav
    Struharova, Alena
    Hlavinkova, Maria
    Sabova, Andrea
    Balkovic, Svetozar
    CEMENT WAPNO BETON, 2013, 18 (04): : 189 - 196
  • [32] Sorption isotherm and length change behavior of autoclaved aerated concrete
    Lam Nguyen Trong
    Asamoto, Shingo
    Matsui, Kunio
    CEMENT & CONCRETE COMPOSITES, 2018, 94 : 136 - 144
  • [33] Autoclaved aerated concrete: experimental evaluation of its thermal properties at high temperatures
    Campanale, Manuela
    Moro, Lorenzo
    HIGH TEMPERATURES-HIGH PRESSURES, 2015, 44 (05) : 369 - 382
  • [34] Thermal behaviour of autoclaved aerated concrete exposed to fire
    Karim, Ghazi Wakili
    Hugi, E.
    Karvonen, L.
    Schnewlin, P.
    Winnefeld, F.
    CEMENT & CONCRETE COMPOSITES, 2015, 62 : 52 - 58
  • [35] Effect of recycled concrete fine powder after calcination on the properties of autoclaved aerated concrete
    Deng, Yang
    Wu, Li
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2024, 20
  • [36] Effect of Moisture Movement on Tested Thermal Conductivity of Moist Aerated Autoclaved Concrete
    M. Campanale
    M. Deganello
    L. Moro
    Transport in Porous Media, 2013, 98 : 125 - 146
  • [37] Effect of Moisture Movement on Tested Thermal Conductivity of Moist Aerated Autoclaved Concrete
    Campanale, M.
    Deganello, M.
    Moro, L.
    TRANSPORT IN POROUS MEDIA, 2013, 98 (01) : 125 - 146
  • [38] Mechanical properties and interface improvement of bamboo cellulose nanofibers reinforced autoclaved aerated concrete
    Zhang, Jie
    Huang, Fei
    Wu, Yuchao
    Fu, Tengfei
    Huang, Biao
    Liu, Wendi
    Qiu, Renhui
    CEMENT & CONCRETE COMPOSITES, 2022, 134
  • [39] Influence of alunite in quartz raw material on the chemical and mechanical properties of autoclaved aerated concrete
    Isu, N
    Mitsuda, T
    APPLIED MINERALOGY, VOLS 1 AND 2: RESEARCH, ECONOMY, TECHNOLOGY, ECOLOGY AND CULTURE, 2000, : 811 - 814
  • [40] Influence of zeolite additive on properties of autoclaved aerated concrete
    Albayrak, Mustafa
    Yorukoglu, Abdulkerim
    Karahan, Serdar
    Atlihan, Sema
    Aruntas, H. Yilmaz
    Girgin, Ismail
    BUILDING AND ENVIRONMENT, 2007, 42 (09) : 3161 - 3165