Reduction of etching damage in lead-zirconate-titanate thin films with inductively coupled plasma

被引:8
|
作者
Lim, KT [1 ]
Kim, KT [1 ]
Kim, DP [1 ]
Kim, CI [1 ]
机构
[1] Chung Ang Univ, Sch Elect & Elect Engn, Seoul 156756, South Korea
来源
关键词
D O I
10.1116/1.1568743
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work, we etched lead-zirconate-titanate (PZT) films with various additive gases (O-2 and Ar) in Cl-2/CF4 plasmas, while mixing ratio was fixed at 8/2. After the etching, the plasma induced damages are characterized in terms of hysteresis curves, leakage current, retention properties, and switching polarization. When the electrical properties of PZT etched in O-2 or Ar added to Cl-2/CF4 were compared, the value of remanent polarization in O-2 added to Cl-2/CF4 plasma is higher than that in Ar added plasma. The maximum etch rate of the PZT thin films was 145 nm/min for 30% Ar added Cl-2/CF4 gas having mixing ratio of 8/2 and 110 nm/min for 10% O-2 added to that same gas mixture. In order to recover the ferroelectic properties of the PZT thin films after etching, we annealed the etched PZT thin films at 550degreesC in an O-2 atmosphere for 10 min. From the hysteresis curves, leakage current, retention property, and switching polarization, the reduction of the etching damage and the recovery via the annealing turned out to be more effective when O-2 was added to Cl-2/CF4 than Ar. X-ray diffraction showed that the structural damage was lower when O-2 was added to Cl-2/CF4 and the improvement in the ferroelectric properties of the annealed samples was consistent with the increased intensities of the (100) and the (200) PZT peaks. (C) 2003 American Vacuum Society.
引用
收藏
页码:1563 / 1567
页数:5
相关论文
共 50 条
  • [1] FLUORINE ION ETCHING OF LEAD-ZIRCONATE-TITANATE THIN-FILMS
    LAU, WM
    BELLO, I
    SAYER, M
    ZOU, LC
    APPLIED PHYSICS LETTERS, 1994, 64 (03) : 300 - 305
  • [2] EPITAXIAL LEAD-ZIRCONATE-TITANATE THIN-FILMS ON SAPPHIRE
    BRAUN, W
    KWAK, BS
    ERBIL, A
    BUDAI, JD
    WILKENS, BJ
    APPLIED PHYSICS LETTERS, 1993, 63 (04) : 467 - 469
  • [3] PREPARATION OF LEAD-ZIRCONATE-TITANATE THIN-FILMS BY REACTIVE EVAPORATION
    TORII, K
    SAITOH, S
    OHJI, Y
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1994, 33 (9B): : 5287 - 5290
  • [4] Ion beam etching of lead-zirconate-titanate thin films:: Correlation between etching parameters and electrical properties evolution
    Soyer, C
    Cattan, E
    Rèmiens, D
    Guilloux-Viry, M
    JOURNAL OF APPLIED PHYSICS, 2002, 92 (02) : 1048 - 1055
  • [5] Oxygen plasma effects on sol-gel-derived lead-zirconate-titanate thin films
    Jang, HK
    Lee, SK
    Lee, CE
    Noh, SJ
    Lee, WI
    APPLIED PHYSICS LETTERS, 2000, 76 (07) : 882 - 884
  • [6] Characterization of sputtered lead-zirconate-titanate thin films with various compositions
    Sakoda, Tomoyuki
    Aoki, Katsuhiro
    Fukuda, Yukio
    Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers, 1999, 38 (6 A): : 3600 - 3603
  • [7] Characterization of sputtered lead-zirconate-titanate thin films with various compositions
    Sakoda, T
    Aoki, K
    Fukuda, Y
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1999, 38 (6A): : 3600 - 3603
  • [8] Electrical damage induced by reactive ion-beam etching of lead-zirconate-titanate thin films -: art. no. 114110
    Soyer, C
    Cattan, E
    Rèmiens, D
    JOURNAL OF APPLIED PHYSICS, 2005, 97 (11)
  • [9] REACTIVE ION ETCHING OF LEAD-ZIRCONATE-TITANATE (PZT) THIN-FILM CAPACITORS
    VIJAY, DP
    DESU, SB
    PAN, W
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1993, 140 (09) : 2635 - 2639
  • [10] Microstructural characterization of sol-gel lead-zirconate-titanate thin films
    Impey, SA
    Huang, Z
    Patel, A
    Beanland, R
    Shorrocks, NM
    Watton, R
    Whatmore, RW
    JOURNAL OF APPLIED PHYSICS, 1998, 83 (04) : 2202 - 2208