Influence of Work Hardening on the Surface of Backup Rolls for a 4-High Rolling Mill Fractured during Rolling Campaign

被引:5
|
作者
Servin-Castaneda, Rumualdo [1 ]
Arreola-Villa, Sixtos Antonio [1 ]
Perez-Alvarado, Alejandro [1 ]
Calderon-Ramos, Ismael [1 ]
Torres-Gonzalez, Ruben [2 ]
Martinez-Hurtado, Alonso [2 ]
机构
[1] Univ Autonoma Coahuila, Fac Ingn Mecan & Elect, Unidad Norte, Monclova Coahuila 25750, Mexico
[2] Univ Autonoma Coahuila, Fac Ingn Mecan & Elect, Unidad Torreon, Torreon Coahuila 27410, Mexico
关键词
backup roll; spalling; fracture; work hardening; mechanical contact; CONTACT FATIGUE; CROWN CONTROL; CONTOUR; DESIGN; MODEL; FLATNESS; BEHAVIOR; PROFILE; WIDE; LIFE;
D O I
10.3390/ma15103524
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Backup rolls are the main tool in a four-high rolling mill; the rolling forces applied in load cells promote the fatigue of the material due to mechanical contact between backup rolls and work rolls. This work investigated the causes of recurrent failures in backup rolls, with cracking always initiated on the surface of the roll body and finishing in the main radius between neck and roll body. Aiming to find the causes of failure, visual inspection and morphology of the fracture were performed, complemented with mechanical tests of hardness on the stress concentration area, in addition to validating the results by applying the finite element method, using ANSYS Mechanical Static Structural Software. It was concluded that the fatigue crack initiated on the surface of BUR due to work hardening continued growing up over the fatigued material, creating beach marks, and finally, a fracture occurred in the main radius of BUR due to stress concentration. The work hardening is the main cause of spalling on BURs and other mechanical components exposed to mechanical contact.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] Use of idler work rolls in two-high rolling with longitudinal stock slitting in mill line
    Zhuchkov, SM
    STEEL IN TRANSLATION, 1997, 27 (07) : 28 - 33
  • [42] Influence of surface texturing and hard chromium coating on the wear of steels used in cold rolling mill rolls
    De Mello, J. D. B.
    Goncalves, J. L., Jr.
    Costa, H. L.
    WEAR, 2013, 302 (1-2) : 1295 - 1309
  • [43] Comparison of tandem cold-rolling mills with 4-high and 6-high mill-stand technology
    Finstermann, Gerhard
    Seilinger, Alois
    Nopp, Gregor
    Djumlija, Gerlinde
    STAHL UND EISEN, 2006, 126 (10): : 57 - 64
  • [44] HIGH-TEMPERATURE THERMOMECHANICAL SURFACE TREATMENT OF LONG COLD-ROLLING MILL ROLLS.
    Shavrin, O.I.
    Savinov, V.A.
    Kreknin, L.T.
    1978, 22 (5-6): : 407 - 409
  • [45] Research and application of computer control system for aluminium single-stand 4-high cold rolling mill
    Zhang, Fei
    Wang, Xiang
    Zong, Shengyue
    Xiang, Xiaofei
    JOURNAL OF ENGINEERING-JOE, 2016, 2016 (11): : 415 - 422
  • [46] IMPACT OF RADIAL RUNOUT BACKUP ROLLS ON FORMATION OF LONGITUDINAL GAGE INTERFERENCE COLD-ROLLED ELECTRICAL STEEL DURING ROLLING ON THE CONTINUOUS MILL
    Babushko, Yury
    Pimenov, Vladimir
    Mazur, Igor
    METAL 2011: 20TH ANNIVERSARY INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2011, : 317 - 323
  • [47] Influence of dispersoids on microstructure evolution and work hardening of aluminium alloys during tension and cold rolling
    Zhao, Qinglong
    Holmedal, Bjorn
    Li, Yanjun
    PHILOSOPHICAL MAGAZINE, 2013, 93 (22) : 2995 - 3011
  • [48] Experimental and Mathematical Model Study of Attenuation Process of the Surface Roughness of Textured Work Rolls during Cold Rolling
    You Y.
    Li H.
    Xia C.
    Kong N.
    Zhang J.
    Jia S.
    Li, Hongbo (lihongbo@ustb.edu.cn), 2018, Chinese Mechanical Engineering Society (54): : 173 - 183
  • [49] CONTROL OF THE SURFACE QUALITY DURING HOT-ROLLING ON A HIGH-SPEED ROD MILL
    TASSIN, S
    PESCHE, F
    WIRE JOURNAL INTERNATIONAL, 1983, 16 (09): : 156 - &
  • [50] INFLUENCE OF ROLLING CONDITIONS AND CHEMICAL-COMPOSITIONS OF ROLLED MATERIAL ON STRIP SURFACE FLAW CAUSED BY SURFACE DETERIORATION OF HOT WORK ROLLS
    OIKE, Y
    SATO, J
    MINAMI, K
    YOSHITAKE, K
    YAMANAKA, S
    ISIJ INTERNATIONAL, 1992, 32 (11) : 1211 - 1215