Microstructure and mechanical properties of novel TiAl alloys tailored via phase and precipitate morphology

被引:30
|
作者
Wimler, David [1 ]
Lindemann, Janny [2 ]
Kremmer, Thomas [3 ]
Clemens, Helmut [1 ]
Mayer, Svea [1 ]
机构
[1] Univ Leoben, Dept Mat Sci, Leoben, Austria
[2] GfE Fremat GmbH, Brand Erbisdorf, Germany
[3] Univ Leoben, Chair Nonferrous Met, Leoben, Austria
关键词
Spark plasma sintering; Titanium aluminides; Mechanical properties; Microstructure; Heat treatment; Precipitation; TITANIUM ALUMINIDE ALLOY; DEFORMATION MECHANISMS; TENSILE PROPERTIES; THERMAL-STABILITY; CARBON ADDITION; CREEP STRENGTH; HIGH NB; GAMMA; TRANSFORMATIONS; EVOLUTION;
D O I
10.1016/j.intermet.2021.107316
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Research and development of alloys based on the intermetallic gamma-TiAl phase is experiencing a renewed interest since powder metallurgical approaches provide new near-net-shape processing options. In this work, the manufacturing via spark plasma sintering was facilitated, a straightforward manufacturing technique to consolidate gas atomized pre-alloyed TiAl powder for microstructural and mechanical evaluation. Two alloys, the so-called BMBF3 alloy (Ti-47.4Al-5.6Nb-0.4W, in at.%) and the BMBF2 alloy (Ti-48.6Al-4.1Nb-0.7W-0.4Si-0.5C-0.1B, in at.%) were microstructurally designed via a heat treatment into a mechanically balanced nearly lamellar gamma microstructure, i.e. gamma appears in globular and lamellar morphology, as well as a creep resistant fully lamellar one. The latter exhibits high creep strength up to 850 degrees C, especially due to the formation of p-Ti3AlC carbides. A heat treatment study upon this fully lamellar microstructure of the C-containing alloy links carbide formation and growth kinetics to the mechanical response of the microstructure. Thus, a stabilization heat treatment at 800 degrees C leads to the formation of finest carbides which are homogeneously distributed and increase the strength of the microstructure due to lower dislocation mobility. The two investigated alloys can be addressed as either a ductile TiAl alloy employable up to 750 degrees C (BMBF3), while the BMBF2 alloy is considered useable up to 850 degrees C.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Microstructure and properties of γ-TiAl based alloys
    Clemens, Helmut
    Schretter, Peter
    Glatz, Wolfgang
    Praktische Metallographie/Practical Metallography, 1996, 33 (01): : 17 - 35
  • [32] Dynamic behavior and microstructural evolution of TiAl alloys tailored via phase and grain size
    Liu, Rui
    Jiao, Ye
    Guo, Yansong
    Chen, Liu
    Li, Zhencheng
    Sha, Aixue
    Gao, Fan
    Chen, Pengwan
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 22 : 292 - 306
  • [33] Microstructure, Mechanical, and Tribological Properties of Nb-Doped TiAl Alloys Fabricated via Laser Metal Deposition
    Huang, Kai
    Xu, Feng
    Liu, Xinyan
    Liu, Shiqiu
    Wang, Qingge
    Baker, Ian
    Song, Min
    Wu, Hong
    MATERIALS, 2024, 17 (17)
  • [34] Effect of carbon nanotube content on the microstructure and mechanical properties of CNTs/TiAl alloys
    Huang, Lei
    Liu, Bingyi
    Wang, Zhenhua
    Yuan, Juntang
    CERAMICS INTERNATIONAL, 2023, 49 (05) : 8196 - 8203
  • [35] Microstructure and mechanical properties of beta TiAl alloys elaborated by spark plasma sintering
    Liu, Xinwang
    Zhang, Zhaolong
    Sun, Rui
    Liu, Fuchu
    Fan, Zitian
    Niu, Hongzhi
    Intermetallics, 2014, 55 : 177 - 183
  • [36] Microstructure and Mechanical Properties of As-Cast γ-TiAl Alloys with Different Cooling Rates
    K. Yang
    Z. J. Yang
    P. Deng
    Z. Y. Chen
    Z. W. Huang
    H. L. Sun
    Journal of Materials Engineering and Performance, 2019, 28 : 2271 - 2280
  • [37] Microstructure and Mechanical Properties of As-Cast -TiAl Alloys with Different Cooling Rates
    Yang, K.
    Yang, Z. J.
    Deng, P.
    Chen, Z. Y.
    Huang, Z. W.
    Sun, H. L.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (04) : 2271 - 2280
  • [38] Mechanical properties of TiAl and TiAl-base alloys
    Kishida, K
    Yokoshima, S
    Johnson, DR
    Inui, H
    Yamaguchi, M
    STABILITY OF MATERIALS, 1996, 355 : 547 - 579
  • [39] Microstructure and Mechanical Properties of TiAl Alloys with Gd Densified by Spark Plasma Sintering
    Guo, Qianqian
    Sun, Hongliang
    Liu, Rui
    Liu, Xili
    Jiang, Xiaosong
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (04) : 1627 - 1635
  • [40] Microstructure and Mechanical Properties of TiAl Alloys with Gd Densified by Spark Plasma Sintering
    Qianqian Guo
    Hongliang Sun
    Rui Liu
    Xili Liu
    Xiaosong Jiang
    Journal of Materials Engineering and Performance, 2023, 32 : 1627 - 1635