Influence of the supersaturated silicon solid solution concentration on the effectiveness of severe plastic deformation processing in Al-7 wt.% Si casting alloy

被引:37
|
作者
Cepeda-Jimenez, C. M. [1 ]
Garcia-Infanta, J. M. [1 ]
Zhilyaev, A. P. [1 ,2 ]
Ruano, O. A. [1 ]
Carreno, F. [1 ]
机构
[1] CSIC, CENIM, Dept Met Phys, Madrid 28040, Spain
[2] Russian Acad Sci, Inst Met Superplast Problems, Ufa 450001, Russia
关键词
Al-Si alloys; Severe plastic deformation (SPD); Deformation-induced precipitation; Microstructure; Mechanical properties; HIGH-PRESSURE TORSION; GRAIN-REFINEMENT; MICROSTRUCTURAL EVOLUTION; TENSILE PROPERTIES; ALUMINUM; NICKEL; GROWTH; PRECIPITATION; HOMOGENEITY; MECHANISMS;
D O I
10.1016/j.msea.2011.07.016
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A comparative study of room temperature severe plastic deformation (SPD) of a hypoeutectic Al-7 wt.% Si casting alloy by high pressure torsion (HPT) and equal channel angular pressing (ECAP) has been performed. Microstructural parameters and microhardness were evaluated in the present work. Three different initial Si solid solution contents have been considered: as cast (C sample, 1.6 wt.% Si), annealed and quenched (Q sample, 1.2 wt.% Si) and annealed and furnace cooled (S sample, 0.7 wt.% Si). The samples processed by ECAP have smaller average Si particle sizes (0.9-1.7 mu m), than those for samples processed by HPT (2.4-4.4 mu m). The initial supersaturated Si solid solution is the major factor affecting the microstructure and the mechanical properties of the material. Fine deformation-induced Si precipitates from the supersaturated solid solution were responsible of the large grain refinement obtained by both SPD processing methods, which was considerably higher than that reported for pure aluminium. Q. samples, processed by both SPD methods, containing an intermediate concentration of Si in solid solution, show the highest hardness due to the finest and most homogeneous microstructure. The finest and homogeneous grain size was similar to 0.2 mu m for the HPTed and similar to 0.4 mu m for the ECAPed Q samples. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:7938 / 7947
页数:10
相关论文
共 37 条
  • [21] INFLUENCE OF SI ON THE THERMAL EXPANSION BEHAVIOR AND PHOTO-ELECTROCHEMICAL PROTECTION OF Al-13 WT.% SI BINARY CASTING ALLOY
    Abdelkebir, Djamel
    Rekhila, Gharib
    Ibrir, Miloud
    Mehdi, Brahim
    Trari, Mohamed
    Raho, Azzeddine Abderrahmane
    INTERNATIONAL JOURNAL OF METALCASTING, 2024,
  • [22] Mechanical and electrical properties of an ultrafine grained Al-8.5 wt. % RE (RE=5.4 wt.% Ce, 3.1wt.% La) alloy processed by severe plastic deformation
    Murashkin, M. Yu.
    Sabirov, I.
    Medvedev, A. E.
    Enikeev, N. A.
    Lefebvre, W.
    Valiev, R. Z.
    Sauvage, X.
    MATERIALS & DESIGN, 2016, 90 : 433 - 442
  • [23] The effect of geometrically necessary dislocations on grain refinement during severe plastic deformation and subsequent annealing of Al-7% Si
    Morris, M. A. Munoz
    Gutierrez-Urrutia, I.
    Morris, D. G.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 493 (1-2): : 141 - 147
  • [24] Assessment of homogeneity of the shear-strain pattern in Al-7 wt%Si casting alloy processed by high-pressure torsion
    Cepeda-Jimenez, C. M.
    Orozco-Caballero, A.
    Garcia-Infanta, J. M.
    Zhilyaev, A. P.
    Ruano, O. A.
    Carreno, F.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 597 : 102 - 110
  • [25] Influence of TMF-induced fluid flow on the microstructure of Al-Si7-Mn1 wt.% alloy
    Orth, A.
    Ratke, L.
    3RD INTERNATIONAL CONFERENCE ON ADVANCES IN SOLIDIFICATION PROCESSES, 2012, 27
  • [26] Influence of severe plastic deformation on intermetallic particles in Mg-12 wt.%Zn alloy investigated using transmission electron microscopy
    Nemec, M.
    Gartnerova, V.
    Jager, A.
    MATERIALS CHARACTERIZATION, 2016, 119 : 129 - 136
  • [27] Effect of Silicon State on Microstructure and Properties of Al-1%Si Alloy During Severe Plastic Deformation
    Tang J.
    Yan J.
    Shen Y.
    Shen, Yao (yaoshen@sjtu.edu.cn), 1600, Shanghai Jiaotong University (55): : 249 - 257
  • [28] COMPOSITIONAL VARIATIONS IN A DEFORMED Ni-7. 1 wt. % Al SOLID SOLUTION ALLOY DURING RAPID HEATING.
    Gridnev, V.N.
    Efimov, A.I.
    Osipenko, I.A.
    Sozinov, A.L.
    Physics of Metals (English Translation of Metallofizika), 1984, 5 (01): : 171 - 178
  • [29] Influence of Severe Plastic Deformation on Precipitation Hardening in an Al-Mg-Si Alloy: Microstructure and Mechanical Properties
    Tsai, Meng-Shan
    Sun, Pei-Ling
    Kao, Po-Wen
    Chang, Chih-Pu
    MATERIALS TRANSACTIONS, 2009, 50 (04) : 771 - 775
  • [30] Influence of the microstructure on the physicomechanical properties of the aluminum alloy Al–Mg–Si nanostructured under severe plastic deformation
    A. M. Mavlyutov
    I. A. Kasatkin
    M. Yu. Murashkin
    R. Z. Valiev
    T. S. Orlova
    Physics of the Solid State, 2015, 57 : 2051 - 2058