摘要
Cu-6 wt.%Ag, Cu-12 wt.%Ag and Cu-24 wt.%Ag alloys were prepared by vacuum melting, solution treating at 740 degrees C for 4 h and aging at 450 degrees C for different times. The effect of aging treatment was investigated by observing the microstructure and determining the hardness. During aging treatment, discontinuous precipitation reaction can occur along high-angle grain boundaries and continuous precipitation reaction within Cu dendritic arms. Abundant high-angle grain boundaries result in a precipitation reaction that is predominantly discontinuous in Cu-6 wt. %Ag while net-like eutectic colonies surrounding Cu dendritic arms result in a precipitation reaction that is predominantly continuous in Cu-24 wt. %Ag. In Cu-12 wt. %Ag, continuous precipitates within Cu dendrites coexist with discontinuous precipitates next to high-angle grain boundaries. Aging only for 1 h can significantly increase the hardness although the precipitation reaction is insufficient. The increasing rate of the hardness becomes slow as aging time longer than 1 h. The hardness keeps approximately constant for Cu-12 wt.%Ag and Cu-24 wt.%Ag and slightly decreases for Cu-6 wt.%Ag with increasing aging time from 16 to 37 h. The precipitation reaction during aging treatment has more significant hardening benefit to the alloys with lower Ag contents. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:150 / 155
页数:6
相关论文
共 50 条
  • [31] Structure and mechanical properties of Cu-Ag nanocomposite films
    Misjak, F.
    Bama, P. B.
    Toth, A. L.
    Ujvari, T.
    Bertoti, I.
    Radnoczi, G.
    THIN SOLID FILMS, 2008, 516 (12) : 3931 - 3934
  • [32] Role of the Aging Treatment in the Microstructure Evolution and Mechanical Properties of Cu/Sn-Bi-Ag-In/Cu Joint
    Li, Zhen
    Wu, Guanzhi
    Ding, Kai
    Gao, Yulai
    TMS 2022 151ST ANNUAL MEETING & EXHIBITION SUPPLEMENTAL PROCEEDINGS, 2022, : 1079 - 1087
  • [33] Effect of combination on properties of Cu-Ag nanocomposites synthesized by heat treatment
    Shafiei, S.M.M.
    Salahi, E.
    Tayebi Fard, S.A.
    International Journal of Engineering, Transactions B: Applications, 2010, 23 (3-4): : 209 - 214
  • [34] Effect of alloying additives on microstructure and mechanical properties of Sn-Ag-Cu solder alloys
    Kim, KS
    Huh, SH
    Suganuma, K
    PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II, 2001, : 1051 - 1054
  • [35] Effect of Mg Content on Microstructure and Mechanical Properties of Al-Cu-Mg-Ag Alloys
    Duan Anjing
    Liu Zhiyi
    Xu Jing
    Bai Song
    Fang Tianwen
    RARE METAL MATERIALS AND ENGINEERING, 2010, 39 : 52 - 55
  • [36] Influence of Fe addition on microstructure and properties of Cu-Ag composite
    Zuo, Xiaowei
    Zhu, Jianzheng
    An, Bailing
    Han, Ke
    Li, Rui
    Wang, Engang
    METALS AND MATERIALS INTERNATIONAL, 2017, 23 (05) : 974 - 983
  • [37] Influence of Fe addition on microstructure and properties of Cu-Ag composite
    Xiaowei Zuo
    Jianzheng Zhu
    Bailing An
    Ke Han
    Rui Li
    Engang Wang
    Metals and Materials International, 2017, 23 : 974 - 983
  • [38] Structural properties and evolution in the solidification process of Cu-Ag alloys
    Zhao, Yan
    Bian, Xiufang
    Qin, Xubo
    Qin, Jingyu
    Hou, Xiaoxia
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2007, 353 (11-12) : 1177 - 1187
  • [39] SURFACE TENSION OF Cu-Ag ALLOYS
    Siwiec, G.
    Oleksiak, B.
    Smalcerz, A.
    Wieczorek, J.
    ARCHIVES OF METALLURGY AND MATERIALS, 2013, 58 (01) : 193 - 195
  • [40] Precipitation behaviour in Cu-Ag alloys
    Spaic, S
    Pristavec, M
    ZEITSCHRIFT FUR METALLKUNDE, 1997, 88 (12): : 925 - 928