Silk Fibroin Degradation Related to Rheological and Mechanical Properties

被引:67
|
作者
Partlow, Benjamin P. [1 ]
Tabatabai, A. Pasha [2 ]
Leisk, Gary G. [3 ]
Cebe, Peggy [4 ]
Blair, Daniel L. [2 ]
Kaplan, David L. [1 ]
机构
[1] Tufts Univ, Dept Biomed Engn, 4 Colby St, Medford, MA 02155 USA
[2] Georgetown Univ, Dept Phys, Inst Soft Matter Synth & Metrol, 506 Reiss Sci Bldg,37th & O St NW, Washington, DC 20057 USA
[3] Tufts Univ, Dept Mech Engn, 200 Coll Ave, Medford, MA 02155 USA
[4] Tufts Univ, Dept Phys & Astron, 574 Boston Ave, Medford, MA 02155 USA
基金
美国国家科学基金会;
关键词
biomaterials; biopolymers; degradation; molecular weight; silk fibroin; SPIDER SILK; STRENGTH; POLYMER; TOUGHNESS; SERICIN; PROTEIN; FILMS; NANOCONFINEMENT; TEMPERATURE; MORPHOLOGY;
D O I
10.1002/mabi.201500370
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
Regenerated silk fibroin has been proposed as a material substrate for biomedical, optical, and electronic applications. Preparation of the silk fibroin solution requires extraction (degumming) to remove contaminants, but results in the degradation of the fibroin protein. Here, a mechanism of fibroin degradation is proposed and the molecular weight and polydispersity is characterized as a function of extraction time. Rheological analysis reveals significant changes in the viscosity of samples while mechanical characterization of cast and drawn films shows increased moduli, extensibility, and strength upon drawing. Fifteen minutes extraction time results in degraded fibroin that generates the strongest films. Structural analysis by wide angle X-ray scattering (WAXS) and Fourier transform infrared spectroscopy (FTIR) indicates molecular alignment in the drawn films and shows that the drawing process converts amorphous films into the crystalline, beta-sheet, secondary structure. Most interesting, by using selected extraction times, films with near-native crystallinity, alignment, and molecular weight can be achieved; yet maximal mechanical properties for the films from regenerated silk fibroin solutions are found with solutions subjected to some degree of degradation. These results suggest that the regenerated solutions and the film casting and drawing processes introduce more complexity than native spinning processes.
引用
收藏
页码:666 / 675
页数:10
相关论文
共 50 条
  • [31] Rheological properties of dilute solutions of natural silk fibroin in N-methylmorpholine oxide
    Novoselov, NP
    Sashina, ES
    RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY, 2003, 77 (05): : 761 - 763
  • [32] Rheological properties of dilute solutions of natural silk fibroin in N-methylmorpholine oxide
    Novoselov, N.P.
    Sashina, E.S.
    Zhurnal Fizicheskoj Khimii, 2003, 77 (05): : 852 - 856
  • [33] IMMUNOCHEMICAL PROPERTIES OF SILK FIBROIN
    DENUCE, JM
    ARCHIVES INTERNATIONALES DE PHYSIOLOGIE ET DE BIOCHIMIE, 1966, 74 (03): : 514 - &
  • [34] Structural characterization and mechanical properties of electrospun silk fibroin nanofiber mats
    N. Amiraliyan
    M. Nouri
    M. Haghighat Kish
    Polymer Science Series A, 2010, 52 : 407 - 412
  • [35] Preparation of silk fibroin/bacterial cellulose composite films and their mechanical properties
    Jung, Rira
    Jin, Hyoung-Joon
    ASBM7: ADVANCED BIOMATERIALS VII, 2007, 342-343 : 741 - +
  • [36] Mechanical and biological properties of silk fibroin/carbon nanotube nanocomposite films
    Caixia Pan
    Qifan Xie
    Zeyun Hu
    Mingying Yang
    Liangjun Zhu
    Fibers and Polymers, 2015, 16 : 1781 - 1787
  • [37] Structural changes and their effect on mechanical properties of silk fibroin/chitosan blends
    Park, SJ
    Lee, KY
    Ha, WS
    Park, SY
    JOURNAL OF APPLIED POLYMER SCIENCE, 1999, 74 (11) : 2571 - 2575
  • [38] Shape memory and mechanical properties of silk fibroin/poly(ε-caprolactone) composites
    Sun, Yehua
    Luo, Yuzhuo
    Dong, Yubing
    Fu, Yaqin
    MATERIALS LETTERS, 2017, 193 : 26 - 29
  • [39] The effects of electrical discharge on the mechanical properties of Bombyx mori silk fibroin
    Yumusak, Cigdem
    Alekberov, Vilayet
    FIBERS AND POLYMERS, 2008, 9 (01) : 15 - 20
  • [40] IMPROVING THE MECHANICAL PROPERTIES OF SILK FIBER/FIBROIN COMPOSITES BY INTERFACIAL MODIFICATION
    Yuan Qingqing
    Yao Jinrong
    Shao Zhengzhong
    ACTA POLYMERICA SINICA, 2011, (11) : 1329 - 1335