Coal Bottom Ash as a Sustainable Supplementary Cementitious Material for the Concrete Exposed to Seawater

被引:12
|
作者
Mangi, Sajjad Ali [1 ,2 ]
Ibrahim, Mohd Haziman Wan [1 ]
Jamaluddin, Norwati [1 ]
Arshad, Mohd Fadzil [3 ]
Memon, Sheeraz Ahmed [4 ]
Shahidan, Shahiron [1 ]
Jaya, Ramadhansyah Putra [5 ]
机构
[1] Univ Tun Hussein Onn Malaysia, Fac Civil & Environm Engn, Jamilus Res Ctr, Batu Pahat 86400, Johor, Malaysia
[2] Mehran Univ Engn & Technol, Dept Civil Engn, SZAB Campus Khairpur Mirs, Sindh, Pakistan
[3] Univ Teknol MARA, Fac Civil Engn, Shah Alam 40450, Selangor, Malaysia
[4] Mehran Univ Engn & Technol, Inst Environm Engn & Management, Jamshoro, Pakistan
[5] Univ Malaysia Pahang, Fac Civil Engn & Earth Resources, Kuantan, Pahang, Malaysia
关键词
TERNARY BLENDS; STRENGTH;
D O I
10.1063/1.5115361
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
The performances of concrete construction exposed to seawater have been considered since long-time. It was generally perceived that the seawater effects could be decelerated by introducing supplementary cementitious materials (SCM) in concrete, which probably reduces its penetrability. Lower penetrability retains the aggressive slats out of the concrete, slows leaching of soluble materials such as lime, reduces the carbonation depth, and better corrosion protection to the reinforcement. Therefore, this study aims to evaluate the compressive strength performances of concrete with and without CBA exposed to seawater. In this study CBA was ground for 20 hours, to get particle fineness as comparable to the cement. Two types of concrete mixes were prepared; one is without ground CBA (M1) and another is with 10% of ground CBA (M2) as a SCM. Concrete cubes were prepared and immersed in normal water for 28 days, to get the desired strength. Afterward, samples were shifted in seawater. The specimens were evaluated for variation in compressive strength and change in weight under dual environments; normal water and seawater at 28, 56 and 90 days. It was experimentally determined that presence of CBA in concrete, raises the strength after 56 days. The strength of M2 concrete at 90 days, gives about 11.3% and 10.2% greater strength under normal water and seawater respectively as compared to M1 concrete. Hence, the CBA presence in concrete, reduces the penetration of aggressive salts, it is an indication of better durability performances of CBA concrete. The practical investigations concluded that the use of CBA as SCM improves the strength of concrete in normal water as well as in seawater environment.
引用
收藏
页数:8
相关论文
共 50 条
  • [21] Sugarcane bagasse ash as supplementary cementitious material in concrete- a review
    Thomas, B. S.
    Yang, J.
    Bahurudeen, A.
    Abdalla, J. A.
    Hawileh, R. A.
    Hamada, H. M.
    Nazar, S.
    Jittin, V
    Ashish, D. K.
    MATERIALS TODAY SUSTAINABILITY, 2021, 15
  • [22] INFLUENCE OF BOTTOM ASH AS A SAND REPLACEMENT MATERIAL ON DURABILITY OF SELF-COMPACTING CONCRETE EXPOSED TO SEAWATER
    Ibrahim, Wan M. H.
    Hamzah, A. F.
    Jamaluddin, N.
    Mangi, S. A.
    Ramadhansyah, P. J.
    JOURNAL OF ENGINEERING SCIENCE AND TECHNOLOGY, 2020, 15 (01): : 555 - 571
  • [23] Waste ceramic powder for sustainable concrete production as supplementary cementitious material
    Ozkilic, Yasin Onuralp
    Bahrami, Alireza
    Guzel, Yusuf
    Soganci, Ali Sinan
    Karalar, Memduh
    Althaqafi, Essam
    Celik, Ali Ihsan
    Zeybek, Ozer
    Jagadesh, P.
    FRONTIERS IN MATERIALS, 2025, 11
  • [24] Development and Performance Evaluation of Coir Pith Ash as Supplementary Cementitious Material in Concrete
    Venugopal, Balagopal
    Sambamurthy, Viswanathan
    JOURNAL OF ENGINEERING AND TECHNOLOGICAL SCIENCES, 2018, 50 (06): : 856 - 869
  • [25] Availability of sugarcane bagasse ash and potential for use as a supplementary cementitious material in concrete
    Indian Institute of Technology, Madras, India
    不详
    Indian Concr J, 6 (41-50):
  • [26] Biomass ash as supplementary cementitious material (SCM)
    Salvo, M.
    Rizzo, S.
    Caldirola, M.
    Novajra, G.
    Canonico, F.
    Bianchi, M.
    Ferraris, M.
    ADVANCES IN APPLIED CERAMICS, 2015, 114 : S3 - S10
  • [27] Evaluation of bagasse ash as supplementary cementitious material
    Ganesan, K.
    Rajagopal, K.
    Thangavel, K.
    CEMENT & CONCRETE COMPOSITES, 2007, 29 (06): : 515 - 524
  • [28] Characterization of sugarcane bagasse ash as a potential supplementary cementitious material: Comparison with coal combustion fly ash
    Zhang, Ping
    Liao, Wenyu
    Kumar, Aditya
    Zhang, Qian
    Ma, Hongyan
    JOURNAL OF CLEANER PRODUCTION, 2020, 277
  • [29] A study on the integrated implementation of supplementary cementitious material and coarse aggregate for sustainable concrete
    Islam, Mohammad Momeen Ul
    JOURNAL OF BUILDING ENGINEERING, 2023, 73
  • [30] An Investigation on Fresh and Hardened Properties of Concrete Blended with Rice Husk Ash as Cementitious Ingredient and Coal Bottom Ash as Sand Replacement Material
    Bheel, Naraindas
    Keerio, Manthar Ali
    Kumar, Aneel
    Shahzaib, Jam
    Ali, Zohaib
    Ali, Mouzzam
    Sohu, Samiullah
    SILICON, 2022, 14 (02) : 677 - 688