Effect of homogenization treatment on microstructure and mechanical properties of DC cast 7X50 aluminum alloy

被引:48
|
作者
Cong, Fu-guan [1 ,2 ]
Zhao, Gang [1 ]
Jiang, Feng [3 ]
Tian, Ni [1 ]
Li, Rui-feng [1 ]
机构
[1] Northeastern Univ, Minist Educ, Key Lab Anisotropy & Text Mat, Shenyang 110004, Peoples R China
[2] Northeast Light Alloy Co Ltd, Harbin 150060, Peoples R China
[3] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
关键词
7X50 aluminum alloy; microstructural evolution; homogenization; residual phase; recrystallization; MACRO SEGREGATION; MAGNETIC-FIELD; EVOLUTION; PHASES; RECRYSTALLIZATION; PARTICLES; ZIRCONIUM;
D O I
10.1016/S1003-6326(15)63694-9
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The evolution of the eutectic structures in the as-cast and homogenized 7X50 aluminum alloys was studied by scanning electron microscopy (SEM), transmission electron microscopy (TEM), energy dispersive spectrometer (EDS), differential scanning calorimetry(DSC), X-ray diffraction(XRD) and tensile test. The results show that the main phases are S(Al2CuMg), T(Al2Mg3Zn3) and MgZn2, with a small amount of Al7Cu2Fe and Al3Zr in the as-cast 7X50 alloy. The volume fraction of the dendritic-network structure and residual phase decreases gradually during the homogenization. After homogenization at 470 degrees C for 24 h and then 482 degrees C for 12 h, the T(Al2Mg3Zn3) phase disappears and minimal S(Al2CuMg) phase remains, while almost no change has happened for Al7Cu2Fe. There is a strong endothermic peak at 477.8 degrees C in the DSC curve of as-cast alloy. A new endothermic peak appears at 487.5 degrees C for the sample homogenized at 470 degrees C for 1 h. However, this endothermic peak disappears after being homogenized at 482 degrees C for 24 h. The T(Al2Mg3Zn3) phase cannot be observed by XRD, which is consistent with that T phase is the associated one of S(Al2CuMg) phase and MgZn2 phase. The volume fraction of recrystallized grains is substantially less in the plate with pre-homogenization treatment. The strength and fracture toughness of the plate with pre-homogenization treatment are about 15 MPa and 3.3 MPa.m(1/2) higher than those of the material with conventional homogenization treatment.
引用
收藏
页码:1027 / 1034
页数:8
相关论文
共 50 条
  • [21] Effect of a Novel Thermomechanical Treatment on Microstructure and Mechanical Properties of 7034 Aluminum Alloy
    Xue, Kemin
    Tian, Zhehuan
    Wang, Kecheng
    Li, Yunhui
    Shi, Wenchao
    Li, Ping
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [22] Effect of online quenching on microstructure and mechanical properties of 7A62 aluminum alloy
    Yue X.-M.
    Liu W.-H.
    Song Y.-F.
    Hu Q.
    Huang H.
    Li H.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2023, 33 (11): : 3595 - 3605
  • [24] Mechanisms of formation of hydrogen porosity in 7X50 and 2X24 aluminum alloys, effects on mechanical behavior
    Marquis, FDS
    GAS INTERACTIONS IN NONFERROUS METALS PROCESSING, 1996, : 43 - 62
  • [25] Research on microstructure in as-cast 7A55 aluminum alloy and its evolution during homogenization
    Lv Xinyu
    Guo Erjun
    Li Zhihui
    Wang Guojun
    RARE METALS, 2011, 30 (06) : 664 - 668
  • [26] Research on microstructure in as-cast 7A55 aluminum alloy and its evolution during homogenization
    Xinyu Lv
    Erjun Guo
    Zhihui Li
    Guojun Wang
    Rare Metals, 2011, 30 : 664 - 668
  • [27] Influences of Ni Addition on Microstructure and Mechanical Properties of Cast Aluminum Alloy 207
    Kang, Fuwei
    Xu, Pei
    Wang, Enhao
    Zhang, Bo
    Tian, Chun
    Wang, Bing
    Li, Shangzhuo
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (18) : 9761 - 9769
  • [28] Microstructure and mechanical properties of aluminum alloy 5182 ingot cast by electromagnetic casting
    Cao, Zhi-Qiang
    Zhang, Xing-Guo
    Jin, Jun-Ze
    Jia, Fei
    Hao, Hai
    Cailiao Kexue yu Gongyi/Material Science and Technology, 2002, 10 (03): : 242 - 246
  • [29] Effect of different homogenization times on the mechanical properties of 7075 aluminum alloy
    Chen, Feng-feng
    He, Jia-wen
    Li, Yang
    Deng, Bei-yue
    Zhu, Jun -lin
    Yang, Hong -mei
    Li, Meng -nie
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 31 : 2582 - 2592
  • [30] Effect of minor strontium and homogenization process on as-cast microstructure and mechanical properties of Al-Mg-Si-Cu-Mn wrought aluminum alloy
    Li Can
    Chen Wen-lin
    Lei Yuan
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2019, 47 (02): : 90 - 98