Microstructure evolution of commercial-purity titanium during cryorolling

被引:23
|
作者
D'yakonov, G. S. [1 ]
Zherebtsov, S. V. [2 ]
Klimova, M. V. [2 ]
Salishchev, G. A. [2 ]
机构
[1] Ufa State Aviat Tech Univ, Inst Phys Adv Mat, Ufa 450000, Russia
[2] Belgorod State Natl Res Univ, Lab Bulk Nanostruct Mat, Belgorod 308015, Russia
来源
PHYSICS OF METALS AND METALLOGRAPHY | 2015年 / 116卷 / 02期
关键词
titanium; cryorolling; twinning; dislocation gliding; microstructure refinement; EBSD; ANGLE GRAIN-BOUNDARIES; DEFORMATION; MECHANISMS; TEXTURE; ALLOY; SIZE; SLIP; TI;
D O I
10.1134/S0031918X14090038
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Electron backscatter diffraction and transmission electron microscopy have been used to analyze the microstructural evolution of titanium during rolling at a cryogenic temperature (T = -196A degrees C). It has been found that intensive twinning at the cryogenic deformation temperature accelerates the kinetics of microstructure refinement. The quantitative analysis of microstructure evolution in titanium upon cryorolling has shown that structure evolution is mainly related to mechanical twinning in the initial stages. A substructure is developed and deformation-induced high-angle boundaries are formed in the range of mean and high degrees of deformation. It was established that rolling to the total degree of deformation E > = 93 % (e = 2.6) at T = -196A degrees C leads to the formation of a titanium microstructure with a grain/subgrains size of approximately 80 nm. The contribution of mechanical twinning and dislocation gliding in structural transformations in titanium with increasing degree of deformation during cryorolling is discussed.
引用
收藏
页码:182 / 188
页数:7
相关论文
共 50 条
  • [21] Effect of the Rate of Multiaxial Compression at Room Temperature on the Evolution of Microstructure of Commercial-Purity Aluminum
    Yang, Y.
    Yang, S. J.
    Wang, Z.
    Gao, X. F.
    METAL SCIENCE AND HEAT TREATMENT, 2019, 61 (1-2) : 96 - 100
  • [22] Low-cycle fatigue behaviors of commercial-purity titanium
    Zhang, Z.F.
    Gu, H.C.
    Tan, X.L.
    Materials Science and Engineering A, 1998, A252 (01): : 85 - 92
  • [23] Recrystallization behavior of boron-modified commercial-purity titanium during hot deformation
    R. A. Gaisin
    V. M. Imayev
    R. M. Imayev
    The Physics of Metals and Metallography, 2015, 116 : 309 - 319
  • [24] Recrystallization behavior of boron-modified commercial-purity titanium during hot deformation
    Gaisin, R. A.
    Imayev, V. M.
    Imayev, R. M.
    PHYSICS OF METALS AND METALLOGRAPHY, 2015, 116 (03): : 309 - 319
  • [25] Low-cycle fatigue behaviors of commercial-purity titanium
    Zhang, ZF
    Gu, HC
    Tan, XL
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 252 (01): : 85 - 92
  • [26] CYCLIC DEFORMATION-BEHAVIOR AND MICROSTRUCTURE OF A COMMERCIAL-PURITY ZIRCONIUM
    XIAO, L
    GU, HC
    INTERNATIONAL JOURNAL OF FATIGUE, 1994, 16 (06) : 417 - 422
  • [27] DEFORMATION DURING MULTIPASS ROLLING OF COMMERCIAL-PURITY ALUMINUM
    SHEPPARD, T
    ZAIDI, MA
    METALS TECHNOLOGY, 1982, 9 (FEB): : 52 - 59
  • [28] On the sinterability of commercial-purity niobium
    Sandim, H.R.Z.
    Padilha, A.F.
    Key Engineering Materials, 2001, 189-191 : 296 - 301
  • [29] The grain-refinement mechanism during heavy cold-rolling of commercial-purity titanium
    Mironov, S.
    Zherebtsov, S.
    Semiatin, S. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 895
  • [30] Slip band-grain boundary interactions in commercial-purity titanium
    Guo, Y.
    Britton, T. B.
    Wilkinson, A. J.
    ACTA MATERIALIA, 2014, 76 : 1 - 12