Removal of sodium (Na2O) from alumina extracted coal fly ash by a mild hydrothermal process

被引:15
|
作者
Li, Huiquan [1 ]
Hui, Junbo [1 ,2 ]
Wang, Chenye [1 ]
Bao, Weijun [1 ]
Sun, Zhenhua [1 ]
机构
[1] Chinese Acad Sci, Key Lab Green Proc & Engn, Inst Proc Engn, Natl Engn Lab Hydromet Cleaner Prod Technol, Beijing 100190, Peoples R China
[2] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
关键词
Coal fly ash; NaCaHSiO4; Sodium removal; Hydrothermal process; C-S-H; ALKALI;
D O I
10.1016/j.hydromet.2015.02.001
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Sodium was removed from alumina-extracted coal fly ash (CFA) by using diluted NaOH solution. The effects of reaction temperature, reaction time, and NaOH concentration on sodium removal were studied. Result shows that the sodium (Na2O) content of the alumina-extracted CFA was decreased from 20 wt.% to 0.6 wt.% under optimal conditions: temperature of 185 degrees C, NaOH concentration of 50 g/L, residence time of 2 h, and liquid-to-solid ratio of 40 for water washing. The possible mechanism of sodium removal was also investigated using Fourier transform infrared spectroscopy, X-ray diffraction analysis, and nuclear magnetic resonance spectroscopy. The results indicated that NaCaHSiO4 in the residue was decomposed by NaOH to form NaSiO3 and Ca(OH)(2), and then converted into tobermorite [Ca5Si6O16(OH)(2)center dot nH(2)O] and NaOH. The sodium obtained through the reaction in the residue was mainly combined with the silanol group and then washed with water. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:1 / 5
页数:5
相关论文
共 50 条
  • [21] VOLATILIZATION OF NA2O FROM MOLTEN SODIUM DISILICATE
    HOLA, M
    MATOUSEK, J
    HLAVAC, J
    SILIKATY, 1974, 18 (03): : 209 - 215
  • [22] Analysis of c-lattice parameters to evaluate Na2O loss from and Na2O content in β"-alumina ceramics
    Bay, Marie-Claude
    Heinz, Meike V. F.
    Danilewsky, Andreas N.
    Battaglia, Corsin
    Vogt, Ulrich F.
    CERAMICS INTERNATIONAL, 2021, 47 (10) : 13402 - 13408
  • [23] Synthesis of zeolite from coal fly ash by microwave hydrothermal treatment with pulverization process
    Fukasawa, Tomonori
    Karisma, Achmad Dwitama
    Shibata, Daiki
    Huang, An-Ni
    Fukui, Kunihiro
    ADVANCED POWDER TECHNOLOGY, 2017, 28 (03) : 798 - 804
  • [24] Microwave-assisted zeolite synthesis from coal fly ash in hydrothermal process
    Inada, M
    Tsujimoto, H
    Eguchi, Y
    Enomoto, N
    Hojo, J
    FUEL, 2005, 84 (12-13) : 1482 - 1486
  • [25] Effect of fly ash to slag ratio and Na2O content on leaching behaviour of fly Ash/Slag based alkali activated materials
    Srinivasamurthy, Lakshmikanth
    Chevali, Venkata S.
    Zhang, Zuhua
    Wang, Hao
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 383
  • [26] An XRD study of the effect of the SiO2/Na2O ratio on the alkali activation of fly ash
    Criado, M.
    Fernandez-Jimenez, A.
    de la Torre, A. G.
    Aranda, M. A. G.
    Palomo, A.
    CEMENT AND CONCRETE RESEARCH, 2007, 37 (05) : 671 - 679
  • [27] Room temperature alkali activation of fly ash: The effect of Na2O/SiO2 ratio
    Bignozzi, Maria Chiara
    Manzi, Stefania
    Natali, Maria Elia
    Rickard, William D. A.
    van Riessen, Arie
    CONSTRUCTION AND BUILDING MATERIALS, 2014, 69 : 262 - 270
  • [28] DURABILITY OF FLY ASH GEOPOLYMER MORTARS IN NITRIC ACID - EFFECT OF ALKALI (Na2O) CONTENT
    Thokchom, Suresh
    Ghosh, Partha
    Ghosh, Somnath
    JOURNAL OF CIVIL ENGINEERING AND MANAGEMENT, 2011, 17 (03) : 393 - 399
  • [29] Effects of calcium oxide and ferric oxide on the process of alumina extraction of coal fly ash activated by sodium carbonate
    Liu, Dandan
    Fang, Li
    Guo, Yanxia
    Yan, Kezhou
    Yao, Cong
    Cheng, Fangqin
    HYDROMETALLURGY, 2018, 179 : 149 - 156
  • [30] Binding of SO3 to fly ash components: CaO, MgO, Na2O and K2O
    Galloway, Benjamin D.
    Sasmaz, Erdem
    Padak, Bihter
    FUEL, 2015, 145 : 79 - 83