Experimental Investigation on Hygroscopic Aging of Glass Fiber Reinforced Vinylester Resin Composites

被引:7
|
作者
He, Weiping [1 ]
Li, Xu [1 ]
Li, Piao [1 ]
Fang, Shirui [2 ]
Ding, Anxin [2 ,3 ]
机构
[1] Wuhan Second Ship Design & Res Inst, Wuhan 430061, Peoples R China
[2] Wuhan Univ Technol, Sch Mat Sci & Engn, Wuhan 430070, Peoples R China
[3] Wuhan Univ Technol, State Key Lab Adv Technol Mat Synth & Proc, Wuhan 430070, Peoples R China
基金
中国国家自然科学基金;
关键词
glass fiber reinforced polymer (GFRP); vinylester resin; hygroscopic aging; moisture absorption; MOISTURE DIFFUSION PARAMETERS; PVC FOAM CORE; SANDWICH COMPOSITES; ABSORPTION; DURABILITY; BEHAVIOR; FACES;
D O I
10.3390/polym14183828
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The hygroscopic behavior of vinylester resin and high strength glass fiber reinforced vinylester resin composites were examined here, including weight change and the resulting degradation of mechanical properties. The prepared resin and composites specimens were immersed in deionized water and artificial seawater with an applied temperature of 70 degrees C, and then the specimens were weighed at specified time intervals in combination with the observation of surface morphologies using a scanning electron microscope. Identification of variations of functional groups was also carried out using Fourier-transform infrared spectroscopy. Meanwhile, the mechanical properties for resin and the composite specimens were tested periodically. The observations on surficial morphologies and the test on weight change display that the vinylester resin hydrolyzes seriously after immersion in deionized water, and that the embedment of glass fiber effectively inhibits the moisture absorption and hydrolysis for resin matrix in composites. The results from the mechanical properties test reveal that the tensile strength of pure resin decreases by 35.3% after 7 days' immersion and keeps small fluctuation in the sequent immersion duration. However, the compressive strength of pure resin consistently dwells at 100 +/- 2 MPa during immersion. After immersion for 90 days, the tensile strength decreases by 28.5% and 38.4%, the compressive strength reduces by 7.2% and 16.6%, and the in-plane shear strength reduces by 16.6% and 15.2% for the composites immersed into deionized water and artificial seawater, respectively. The main highlights of this paper are that it provides a more comprehensive mechanical properties test in combination with the microscopic characterization on a matrix and its composites to reveal the aging behavior of composites under a hygroscopic environment.
引用
收藏
页数:18
相关论文
共 50 条
  • [21] Impact fatigue of glass fibre-vinylester resin composites
    Roy, R
    Sarkar, BK
    Bose, NR
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2001, 32 (06) : 871 - 876
  • [22] Flexural properties of some experimental dental glass fiber reinforced composites with different resin matrices
    Preimerean, C.
    Petrescu, A.
    Buruiana, T.
    Stanulet, L.
    Moldovan, M.
    Nicola, C.
    Trif, M.
    Furtos, G.
    Colceriu, A.
    Tamas, C.
    Prodan, D.
    JOURNAL OF OPTOELECTRONICS AND ADVANCED MATERIALS, 2007, 9 (11): : 3361 - 3363
  • [23] BALLISTIC APPLICATIONS OF GLASS AND KEVLAR FIBER VINYLESTER COMPOSITES
    PANDA, SP
    NAVALE, NG
    SARAF, MN
    GUPTA, RK
    GOEL, RA
    DEFENCE SCIENCE JOURNAL, 1994, 44 (04) : 341 - 343
  • [24] Experimental investigation and numerical modeling of creep response of glass fiber reinforced polymer composites
    Berardi, Valentino Paolo
    Perrella, Michele
    Armentani, Enrico
    Cricri, Gabriele
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2021, 44 (04) : 1085 - 1095
  • [25] Experimental Investigation on the Durability of Glass Fiber-Reinforced Polymer Composites Containing Nanocomposite
    Li, Weiwen
    Ji, Chunyang
    Zhu, Honggang
    Xing, Feng
    Wu, Jiaxin
    Niu, Xueli
    JOURNAL OF NANOMATERIALS, 2013, 2013
  • [26] Experimental study on natural aging of glass fiber reinforced plastic composites under marine environment
    Zhang, Yingjun
    Zhu, Xi
    Mei, Zhiyuan
    Li, Huadong
    Huazhong Keji Daxue Xuebao (Ziran Kexue Ban)/Journal of Huazhong University of Science and Technology (Natural Science Edition), 2011, 39 (03): : 14 - 17
  • [27] Investigation of Fiber-Reinforced Modified Epoxy Resin Composites
    Quddos, A.
    Khan, M. B.
    Khan, R. N.
    Ghauri, M. K. K.
    ADVANCED MATERIALS XII, 2012, 510-511 : 577 - +
  • [28] Effects of Hygrothermal Aging on the Thermal-Mechanical Properties of Vinylester Resin and its Pultruded Carbon Fiber Composites
    Yu, Yunhua
    Li, Peng
    Sui, Gang
    Yang, Xiaoping
    Liu, Hongliang
    POLYMER COMPOSITES, 2009, 30 (10) : 1458 - 1464
  • [29] Investigation of aging resistance for dental resin composites with and without glass flakes
    Dan Feng
    Shujun Dong
    Zuosen Shi
    Zhanchen Cui
    Song Zhu
    Clinical Oral Investigations, 2023, 27 : 6903 - 6914
  • [30] Investigation of aging resistance for dental resin composites with and without glass flakes
    Feng, Dan
    Dong, Shujun
    Shi, Zuosen
    Cui, Zhanchen
    Zhu, Song
    CLINICAL ORAL INVESTIGATIONS, 2023, 27 (11) : 6903 - 6914