Microstructure Evolution of Peak-Aged ZK60 Magnesium Alloy under High Strain Rate Deformation

被引:1
|
作者
Yang, Yang [1 ,2 ]
Yang, Shuangjun [1 ]
Wang, Zhen [1 ]
机构
[1] Cent South Univ, Sch Mat Sci & Engn, 932 Lushan South Rd, Changsha 410083, Hunan, Peoples R China
[2] Minist Educ, Key Lab Nonferrous Met, Changsha 410083, Peoples R China
基金
中国国家自然科学基金;
关键词
high strain rate; microstructure; precipitates; transmission electron microscope; ZK60 magnesium alloy; SHEAR LOCALIZATION; BEHAVIOR; TRANSFORMATION; PRECIPITATION; BANDS;
D O I
10.1520/JTE20200272
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The microstructure evolution of peak-aged ZK60 magnesium alloy under high strain rate deformation was studied by the radial collapse of a thick-walled cylinder technique and transmission electron microscope. The results showed that the rod-like beta(')(1) phase was the main precipitated phase in the peak-aged ZK60 magnesium alloy, and precipitate-free regions were present along the grain boundaries. A large number of twins and dislocations were produced in the sample within 4.0 mu s after high strain rate loading, and a number of thin and long rod-like ss 1' phases were observed within the dislocated tangle of the deformed sample. The length and diameter of the rod-like phases in the samples were gradually reduced, and some of the rodlike phases were converted into spherical phases with increasing strain rate, which indicated that the original precipitated phases were partly dissolved after high strain rate loading. The microhardness of the samples increased from HV80.12 to HV101.20 as the strain rate increased.
引用
收藏
页码:4671 / 4680
页数:10
相关论文
共 50 条
  • [31] Correlation of plastic deformation and dynamic recrystallization in magnesium alloy Zk60
    Galiyev, A
    Kaibyshev, R
    Gottstein, G
    ACTA MATERIALIA, 2001, 49 (07) : 1199 - 1207
  • [32] Thermal simulation on hot deformation behavior of ZK60 magnesium alloy
    School of Materials Science and Engineering, Central South University, Changsha 410083, China
    Cailiao Gongcheng, 2009, 11 (45-50):
  • [33] Fatigue of ZK60 magnesium alloy under uniaxial loading
    Xiong, Ying
    Jiang, Yanyao
    INTERNATIONAL JOURNAL OF FATIGUE, 2014, 64 : 74 - 83
  • [34] Microstructure and Corrosion of Cast Magnesium Alloy ZK60 in NaCl Solution
    Li, Zhen
    Peng, Zeyin
    Qi, Kai
    Li, Hui
    Qiu, Yubing
    Guo, Xingpeng
    MATERIALS, 2020, 13 (17)
  • [35] Influence of impurities on microstructure and mechanical properties of ZK60 magnesium alloy
    潘复生
    毛建军
    陈先华
    彭建
    王敬丰
    TransactionsofNonferrousMetalsSocietyofChina, 2010, 20 (07) : 1299 - 1304
  • [36] Plastic deformation behavior of ZK60 magnesium alloy with addition of neodymium
    余琨
    王晓艳
    芮守泰
    王日初
    JournalofCentralSouthUniversityofTechnology, 2008, (04) : 434 - 437
  • [37] Ratcheting deformation and fatigue of surface treated ZK60 magnesium alloy
    Xiong, Ying
    Yu, Yi
    INTERNATIONAL JOURNAL OF FATIGUE, 2022, 156
  • [38] Effects of Gd on microstructure and mechanical property of ZK60 magnesium alloy
    Huang, Zheng-hua
    Qi, Wen-jun
    Xu, Jing
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2013, 23 (09) : 2568 - 2576
  • [39] Evolution of microstructure, texture and mechanical properties of ZK60 magnesium alloy in a single rolling pass
    Wang, Wenke
    Cui, Guorong
    Zhang, Wencong
    Chen, Wenzhen
    Wang, Erde
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 724 : 486 - 492
  • [40] Plastic deformation behavior of ZK60 magnesium alloy with addition of neodymium
    Yu Kun
    Wang Xiao-yan
    Rui Shou-tai
    Wang Ri-chu
    JOURNAL OF CENTRAL SOUTH UNIVERSITY OF TECHNOLOGY, 2008, 15 (04): : 434 - 437