Effect of the aspect ratio of whisker on work hardening rate of as forged 2024Al/Al18B4O33w composite

被引:5
|
作者
Yuan, Lin [1 ]
Shi, Wenchao [1 ]
Zheng, Zhenzhu [1 ]
Shan, Debin [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Heilongjiang, Peoples R China
关键词
Metal-matrix composites; Forging; Work hardening rate; Microstructures; FRACTURE-BEHAVIOR; DEFORMATION-BEHAVIOR; MATRIX COMPOSITES; GRAIN-SIZE; STRENGTH; ALLOYS;
D O I
10.1016/j.matchar.2015.04.006
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The 2024Al/Al(18)B(4)O(33)w composite fabricated by the squeeze casting technique is forged with different deformation levels to improve tensile properties. The work hardening rates of 2024Al/Al(18)B(4)O(33)w composite with different forging deformation levels are studied. The results show that the forging process plays a very important role in work hardening rate due to the reduction in the aspect ratios of whiskers and the increase in the dislocation density and the angle between whisker axis and forging direction with increasing deformation level. The variations of work hardening rates in the microscopic yield stage, yield stage and macro plastic stage are correlated with the variation of the aspect ratio of whisker. The initial work hardening rate is higher then rapidly decreases due to the more favorable for annihilation than multiplication of the initial stored dislocations. The work hardening rate of the forged 2024Al/Al(18)B(4)O(33)w composite at the deformation level of 70% with the highest initial stored dislocation density is the highest in the microscopic yield stage and macro plastic stage, but is the lowest in the yield stage due to the interaction of dislocations. The work hardening exponent increases with decreasing the aspect ratio of whiskers. The cracked and progressive cracking whiskers have an impact on work hardening capacity. (C) 2015 Elsevier Inc. All rights reserved.
引用
收藏
页码:73 / 80
页数:8
相关论文
共 50 条
  • [21] Effect of deformation temperature and degree on tensile properties of the extruded 2024Al/Al18B4O33w composite with extrusion - forging multistage hot deformationAuswirkung der Verformungstemperatur und des Verformungsgrades auf die Zugfestigkeitseigenschaften des stranggepressten 2024Al/Al18B4O33w-Verbundwerkstoffs mit mehrstufiger Warmverformung durch Strangpressen und Schmieden
    Shi, W. C.
    Chen, A.
    Cui, B. S.
    Gong, D. M.
    Xue, C. M.
    Xu, F.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2023, 54 (02) : 238 - 243
  • [22] On the thermal stability of coating in an Al18B4O33w/α-Al2O3/6061Al composite
    Ding, DY
    Wang, JN
    Ning, CQ
    Dai, KR
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 358 (1-2): : 159 - 163
  • [23] Preparation, microstructure, and electromagnetic properties of Al18B4O33w/CoxFeyBz composite powders
    Jiang, J. T.
    Zhen, L.
    Xu, C. Y.
    Shao, W. Z.
    Zhou, Z. X.
    SURFACE & COATINGS TECHNOLOGY, 2012, 212 : 14 - 19
  • [24] Effect of Bi2O3 coating on interfacial wettability and tensile properties of Al18B4O33w/Al composite
    Z. J. Li
    L. D. Wang
    H. Y. Yue
    W. D. Fei
    Journal of Materials Science, 2007, 42 : 9355 - 9358
  • [25] Effect of Bi2O3 coating on interfacial wettability and tensile properties of Al18B4O33w/Al composite
    Li, Z. J.
    Wang, L. D.
    Yue, H. Y.
    Fei, W. D.
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (22) : 9355 - 9358
  • [26] Effect of lamination structures on impact properties of Al18B4O33W/Al and aluminum laminate composites
    Hiroshima Univ, Hiroshima, Japan
    Keikinzoku J Jpn Inst Light Met, 5 (232-236):
  • [27] Fine structure of coated whiskers in Al18B4O33w/γ-Al2O3/6061Al composite
    Ding, DY
    Wang, DZ
    Yao, CK
    Rao, JC
    Li, DX
    JOURNAL OF MATERIALS SCIENCE, 2001, 36 (14) : 3497 - 3502
  • [28] Fine structure of coated whiskers in Al18B4O33w/γ-Al2O3/6061Al composite
    D. Y. Ding
    D. Z. Wang
    C. K. Yao
    J. C. Rao
    D. X. Li
    Journal of Materials Science, 2001, 36 : 3497 - 3502
  • [29] Improvement of the tensile strength of Al18B4O33w/Al composite at elevated temperatures by change of interfacial state
    Yue, H. Y.
    Wang, L. D.
    Fei, W. D.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 486 (1-2): : 409 - 412
  • [30] Effects of the sintering temperature of whisker with SnO2•Bi2O3 coatings on the damping behavior in Al18B4O33w/Al composite
    Liu, G.
    Tang, S. W.
    Hu, J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 530 : 9 - 14