Effect of heat treatment on deformation and mechanical properties of 8 mol% yttria-stabilized zirconia by Berkovich nanoindentation

被引:26
|
作者
Mao, W. G. [1 ,2 ]
Luo, J. M. [1 ,2 ,3 ]
Dai, C. Y. [1 ,2 ]
Shen, Y. G. [3 ]
机构
[1] Xiangtan Univ, Sch Mat Sci & Engn, Xiangtan 411105, Hunan, Peoples R China
[2] Xiangtan Univ, Hunan Prov Key Lab Thin Film Mat & Devices, Xiangtan 411105, Hunan, Peoples R China
[3] City Univ Hong Kong, Dept Mech & Biomed Engn, Kowloon, Hong Kong, Peoples R China
基金
中国国家自然科学基金;
关键词
Thermal barrier coatings; Heat treatment; Nanoindentation; Mechanical properties; Hertzian contact theory; THERMAL-BARRIER COATINGS; FOREIGN OBJECT DAMAGE; RESIDUAL-STRESS; ELASTIC-MODULUS; INDENTATION; BEHAVIOR; HARDNESS; CORROSION; EROSION; SYSTEMS;
D O I
10.1016/j.apsusc.2015.02.108
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effect of thermal treatment on the elasto-plastic transition and mechanical properties of air plasmasprayed 8 mol% Y2O3-stabilized ZrO2 (8YSZ) thermal barrier coatings was studied by nanoindentation test at ultra-low loads with a Berkovich indenter. The area contact function of the indenter was calibrated repeatedly under nano-scales, and the indenter tip radius was estimated under different indentation depths, respectively. Owing to the heterogeneous and porous microstructure, the scatter of all collected experimental data was analyzed by Weibull statistic method. It is interesting to observe that the hardness exhibits an apparent reverse indentation size effect under very small depths. The Young's modulus of 8YSZ varies with ranging from 213 to 246 GPa due to the sintering effect. True hardness of 8YSZ increases from as-received 72.9 GPa to a top value 79.7 GPa under 100 thermal cycles, and then slightly decreases from this value to 75.5 GPa under 175 thermal cycles. The pure elastic and elasto-plastic indentation curves were obtained by adjusting the indentation load magnitude. The elasto-plastic transition and resolved shear stress fields were discussed carefully from the use of energetic models and Hertzian contact theory. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:92 / 98
页数:7
相关论文
共 50 条
  • [21] Elasto-plastic characteristics and mechanical properties of as-sprayed 8 mol% yttria-stabilized zirconia coating under nano-scales measured by nanoindentation
    Luo, J. M.
    Dai, C. Y.
    Shen, Y. G.
    Mao, W. G.
    APPLIED SURFACE SCIENCE, 2014, 309 : 271 - 277
  • [22] Improvement of mechanical strength of 8 mol % yttria-stabilized zirconia ceramics by spark-plasma sintering
    Takeuchi, T
    Kondoh, I
    Tamari, N
    Balakrishnan, N
    Nomura, K
    Kageyama, H
    Takeda, Y
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2002, 149 (04) : A455 - A461
  • [23] Nanoindentation examination of yttria-stabilized zirconia (YSZ) crystal
    Fujikane, Masaki
    Setoyama, Daigo
    Nagao, Shijo
    Nowak, Roman
    Yamanaka, Shinsuke
    JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 431 (1-2) : 250 - 255
  • [24] Sinterability of commercial 8 mol% yttria-stabilized zirconia powders and the effect of sintered density on the ionic conductivity
    I. R. Gibson
    G. P. Dransfield
    J. T. S. Irvine
    Journal of Materials Science, 1998, 33 : 4297 - 4305
  • [25] Effect of superspeed sintering on translucency, opalescence, microstructure, and phase fraction of multilayered 4 mol% yttria-stabilized tetragonal zirconia polycrystal and 6 mol% yttria-stabilized partially stabilized zirconia ceramics
    Shin, Hye-Jeong
    Kwon, Yong-Hoon
    Seol, Hyo-Joung
    JOURNAL OF PROSTHETIC DENTISTRY, 2023, 130 (02): : 254.e1 - 254.e10
  • [26] Sinterability of commercial 8 mol% yttria-stabilized zirconia powders and the effect of sintered density on the ionic conductivity
    Gibson, IR
    Dransfield, GP
    Irvine, JTS
    JOURNAL OF MATERIALS SCIENCE, 1998, 33 (17) : 4297 - 4305
  • [28] Densification of porous 8 mol% yttria-stabilized zirconia component: modelling and experimental studies
    Lu, J.
    Song, X. C.
    Zhang, T. S.
    Hng, H. H.
    Ma, J.
    JOURNAL OF MATERIALS SCIENCE, 2010, 45 (03) : 575 - 581
  • [29] Texture development in 3 mol% yttria-stabilized tetragonal zirconia
    Suarez, Gustavo
    Sakka, Yoshio
    Suzuki, Tohru
    Uchikoshi, Tetsuo
    Aglietti, Esteban F.
    MATERIALS RESEARCH BULLETIN, 2009, 44 (08) : 1802 - 1805
  • [30] Influence of trace impurities on the mechanical characteristics of a superplastic 2 mol% yttria-stabilized zirconia
    Univ of California, San Diego, United States
    Acta Mater, 15 (5557-5568):