Determination of thermal activation energy of spin-on MSQ used as interlayer dielectric

被引:2
|
作者
Aw, KC [1 ]
Ibrahim, K [1 ]
机构
[1] Univ Sci Malaysia, Sch Appl Phys, George Town 11800, Malaysia
关键词
D O I
10.1109/SMELEC.2002.1217770
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Device dimension in VLSI circuit constantly shrink with one main objective, i.e. increase in speed. However, there are other parasitic components in the VLSI circuit other than device dimension that can increase the speed of VLSI circuits. The reduction of dielectric constant of interlayer dielectric (ILD) material can improve the speed due to reduction in parasitic capacitance. Therefore, low dielectric constant (k) materials are being introduced. Low-k dielectric material is categorised as material having dielectric constant of less than 3.0. In this research Methylsilsesquioxane (MSQ), which is a type of spin-on glass (SOG), is being used as it offers low fabrication cost. There was reported activation energy for SiO2 but there is no activation energy information for MSQ. Using the technique of leakage current measurement at different bake temperatures, the activation energy of MSQ degradation due to Aluminium diffusion is approximately determined to be 0.35eV.
引用
收藏
页码:36 / 38
页数:3
相关论文
共 50 条
  • [21] ACTIVATION-ENERGY DETERMINATIONS FROM DIELECTRIC THERMAL-ANALYSIS OF REACTING POLYMERIC SYSTEMS
    NASS, KA
    SEFERIS, JC
    JOURNAL OF THERMAL ANALYSIS, 1991, 37 (10): : 2407 - 2421
  • [22] Determination of the atomic cohesive energy and Debye temperature from thermal stiffening of the dielectric constant of semiconductors
    Liu, Jin
    Yang, Xuexian
    Ouyang, Gang
    Liao, Wenhu
    Zhao, Heping
    CHEMICAL PHYSICS LETTERS, 2022, 793
  • [23] DETERMINATION OF ACTIVATION-ENERGY FOR CRYSTAL-GROWTH BY DIFFERENTIAL THERMAL-ANALYSIS
    MATUSITA, K
    SAKKA, S
    MATSUI, Y
    JOURNAL OF MATERIALS SCIENCE, 1975, 10 (06) : 961 - 966
  • [24] Determination of activation energy during the thermal degradation of Polyamide 66/glass fiber composites
    Azimi, Hamidreza
    Abedifard, Pardis
    JOURNAL OF THERMOPLASTIC COMPOSITE MATERIALS, 2020, 33 (07) : 956 - 966
  • [25] Determination of thermal stability and activation energy of polyvinyl alcohol-cassava starch blends
    Sin, Lee Tin
    Rahman, W. A. W. A.
    Rahmat, A. R.
    Mokhtar, M.
    CARBOHYDRATE POLYMERS, 2011, 83 (01) : 303 - 305
  • [26] METHODS FOR THE DETERMINATION OF THE ACTIVATION-ENERGY OF GLASS CRYSTALLIZATION FROM THERMAL-ANALYSIS
    BANSAL, NP
    BRUCE, AJ
    DOREMUS, RH
    MOYNIHAN, CT
    PHYSICS AND CHEMISTRY OF GLASSES, 1984, 25 (03): : 86 - 86
  • [28] METHODS FOR THE DETERMINATION OF THE ACTIVATION-ENERGY OF GLASS CRYSTALLIZATION FROM THERMAL-ANALYSIS
    SPEYER, RF
    RISBUD, SH
    PHYSICS AND CHEMISTRY OF GLASSES, 1983, 24 (01): : 26 - 30
  • [29] DETERMINATION OF THE ACTIVATION-ENERGY OF THERMAL DONORS OF THE 1ST TYPE IN GERMANIUM
    LITVINOV, VV
    PALCHIK, GV
    URENEV, VI
    SOVIET PHYSICS SEMICONDUCTORS-USSR, 1987, 21 (11): : 1281 - 1282
  • [30] Determination of the thermal activation energy and optical band gap of cobalt phthalocyanine thin films
    Ambily, S
    Menon, CS
    MATERIALS LETTERS, 1998, 34 (3-6) : 124 - 127