IMC growth and shear strength of Sn-Ag-Cu/Co-P ball grid array solder joints under thermal cycling

被引:28
|
作者
Yang, Donghua [1 ,2 ]
Cai, Jian [3 ,4 ]
Wang, Qian [3 ]
Li, Jingwei [3 ]
Hu, Yang [3 ]
Li, Liangliang [1 ]
机构
[1] Tsinghua Univ, Sch Mat Sci & Engn, Key Lab Adv Mat MOE, Beijing 100084, Peoples R China
[2] Chongqing Univ Technol, Sch Mat Sci & Engn, Chongqing 400054, Peoples R China
[3] Tsinghua Univ, Inst Microelect, Beijing 100084, Peoples R China
[4] Tsinghua Natl Lab Informat Sci & Technol, Beijing 100084, Peoples R China
基金
中国博士后科学基金;
关键词
LEAD-FREE SOLDER; INTERFACIAL REACTIONS; CU SOLDER; NI-P; MICROSTRUCTURE; METALLIZATION; EVOLUTION; ALLOYS; INTERMETALLICS; RELIABILITY;
D O I
10.1007/s10854-014-2489-7
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Co-P films with P contents of 4.0 and 8.0 at.% were electroplated on printed circuit boards and used as surface finish of ball grid array (BGA) packages. Sn-3.0 wt% Ag-0.5 wt% Cu (SAC305) solder balls were reflowed on the Co-P finish to form SAC/Co-P solder joints. The morphology and growth of intermetallic compounds (IMCs) in SAC/Co-P joints under thermal cycling were systematically analyzed, and the effects of IMCs on shear strength and fractured surface of the joints were studied. SAC/Cu BGA solder joints were also prepared as a comparison. It was found that CoSn3 and (Cu, Co)(6)Sn-5 grew at the interface of SAC/Co-4 at.% P solder joints during thermal cycling. The shear strength of SAC/Co-4 at.% P joints exceeded that of SAC/Cu joints after 100 thermal cycles, because the granule size of (Cu, Co)(6)Sn-5 was smaller than that of Cu6Sn5 and no Kirkendall void existed at the interface of SAC/Co-4 at.% P joints. For SAC/Co-8 at.% P joints, a layer of smooth and void-free Co-Sn-P formed at the interface, and the shear strength of SAC/Co-8 at.% P joints increased by 8.4 % in comparison with that of SAC/Cu joints after 300 cycles. In addition, the fractured surface of three kinds of joints after thermal cycling was examined. The experimental data demonstrated that Co-P surface finish enhanced the shear strength of solder joints after thermal cycling and improved the reliability of BGA packages.
引用
收藏
页码:962 / 969
页数:8
相关论文
共 50 条
  • [41] Microstructure evolution and microimpact performance of Sn-Ag-Cu solder joints under thermal cycle test
    Y. L. Huang
    K. L. Lin
    D. S. Liu
    Journal of Materials Research, 2010, 25 : 1312 - 1320
  • [42] Grain growth in eutectic Pb/Sn ball grid array solder joints
    Basaran, C
    Wen, YJ
    ITHERM 2002: EIGHTH INTERSOCIETY CONFERENCE ON THERMAL AND THERMOMECHANICAL PHENOMENA IN ELECTRONIC SYSTEMS, PROCEEDINGS, 2002, : 903 - 908
  • [43] Effect of multiple reflow cycles on ball impact responses of Sn-Ag-Cu solder joints
    Lai, Yi-Shao
    Kao, C. R.
    Chang, Hsiao-Chuan
    Kao, Chin-Li
    SOLDERING & SURFACE MOUNT TECHNOLOGY, 2009, 21 (03) : 4 - 9
  • [44] Acoustic Microscopy of Interfacial Crack in Sn-Ag-Cu Alloy Solder Joints under Shear Fatigue Testing
    Kato, Hiroshi
    Kobayashi, Hirotsugu
    MATERIALS TRANSACTIONS, 2008, 49 (09) : 2068 - 2075
  • [45] TEM and EBSD characterization revealing the recrystallization process occurring in the Sn-3.0Ag-0.5Cu Ball Grid Array solder joints during thermal cycling
    Du, Yihui
    Wang, Yishu
    Ji, Xiaoliang
    Tan, Shihai
    Han, Jing
    Guo, Fu
    MATERIALS CHARACTERIZATION, 2023, 200
  • [46] Size dependence on shear fatigue and fracture behavior of ball grid array structure Cu/Sn-3.0Ag-0.5Cu/Cu solder joints under current stressing
    Wang, Bo
    Li, Wangyun
    Pan, Kailin
    Huang, Wei
    Gong, Yubing
    FRONTIERS IN MATERIALS, 2024, 11
  • [47] Effects of static thermal aging and thermal cycling on the microstructure and shear strength of Sn95.5Ag3.8Cu0.7 solder joints
    Ahat, S
    Sheng, M
    Luo, L
    JOURNAL OF MATERIALS RESEARCH, 2001, 16 (10) : 2914 - 2921
  • [48] Effects of static thermal aging and thermal cycling on the microstructure and shear strength of Sn95.5Ag3.8Cu0.7 solder joints
    Shawkret Ahat
    Mei Sheng
    Le Luo
    Journal of Materials Research, 2001, 16 : 2914 - 2921
  • [49] Effects of thermal cycling on shear strength and microstructures of soldered joints of ceramic ball grid array package
    College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 210016, China
    不详
    Hanjie Xuebao, 2006, 6 (1-4):
  • [50] Impact of different aging conditions on the IMC layer growth and shear strength of Ni-modified MWCNTs reinforced Sn-Ag-Cu composite solder
    Zhai, Xinmeng
    Chen, Yue
    Li, Yuefeng
    SOLDERING & SURFACE MOUNT TECHNOLOGY, 2022, 34 (03) : 174 - 182