Effect of Mixed Salts on Atmospheric Corrosion of 304 Stainless Steel

被引:18
|
作者
Guo, Liya [1 ,2 ]
Mi, Na [1 ]
Mohammed-Ali, Haval [1 ,3 ]
Ghahari, Majid [1 ]
Du Plessis, Andrew [1 ]
Cook, Angus [1 ]
Street, Steven [1 ]
Reinhard, Christina [4 ]
Atwood, Robert C. [4 ]
Rayment, Trevor [4 ]
Davenport, Alison J. [1 ]
机构
[1] Univ Birmingham, Sch Met & Mat, Birmingham B15 2TT, W Midlands, England
[2] Imperial Coll London, Dept Mat, London SW7 2AZ, England
[3] Univ Zakho, Dept Phys, Zakho, Iraq
[4] Diamond Light Source Ltd, Didcot OX11 0DE, Oxon, England
基金
英国工程与自然科学研究理事会;
关键词
X-RAY MICROTOMOGRAPHY; PITTING CORROSION; STAINLESS-STEEL; LOCALIZED CORROSION; RELATIVE-HUMIDITY; TRANSITIONS; TOMOGRAPHY; PARTICLES; AEROSOLS; BEHAVIOR;
D O I
10.1149/2.0021911jes
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Atmospheric corrosion of stainless steel can take place when airborne salt particles deposit on the metal surface, forming droplets when the relative humidity (RH) reaches a critical value: the deliquescence relative humidity of the salt. Most work to date has focused on single salts such as MgCl2 or NaCl. In the present work, the effect of mixed salts is investigated at 45% RH, above the deliquescence relative humidity of MgCl2 but below that of NaCl. Dish-shaped pits were found in pure MgCl2 solutions and mixed solutions. Crevice corrosion takes place under NaCl crystals. This is shown both with ex situ measurements and in situ time-dependent measurements using X-ray microtomography, where pit growth was also monitored. (c) The Author(s) 2019. Published by ECS.
引用
收藏
页码:C3010 / C3014
页数:5
相关论文
共 50 条
  • [31] Corrosion potential of 304 stainless steel in sulfuric acid
    Jegdic, Bore
    Drazic, Dragutin M.
    Popic, Jovan P.
    JOURNAL OF THE SERBIAN CHEMICAL SOCIETY, 2006, 71 (05) : 543 - 551
  • [32] Tribological properties of 304 stainless steel with rainwater corrosion
    Pang, Ming-hua
    Zhai, Shuai-jie
    Hu, Yi-kun
    Zhang, Qiu-chen
    Ma, Li-jie
    Feng, Qi-gao
    MATERIALS CHEMISTRY AND PHYSICS, 2023, 297
  • [33] Inhibition of Pitting Corrosion on Type 304 Stainless Steel
    Lian, Zhouyang
    MATERIALS PERFORMANCE, 2017, 56 (12) : 54 - 56
  • [34] Initiation of corrosion pits at inclusions on 304 stainless steel
    Ke, RR
    Alkire, R
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (12) : 4056 - 4062
  • [35] Corrosion behavior of 304 stainless steel in supercritical water
    Zhang, Xiaohui
    Fan, Jingjing
    Krolczyk, Grzegorz M.
    Zhang, Xiaoyu
    Ren, Lu
    Gupta, Munish Kumar
    Chen, Siyu
    Li, Zhixiong
    JOURNAL OF SUPERCRITICAL FLUIDS, 2024, 206
  • [36] CORROSION OF AISI TYPE 304 AUSTENITIC STAINLESS STEEL
    GOOCH, TG
    BRITISH WELDING JOURNAL, 1968, 15 (07): : 345 - &
  • [37] Metal dusting corrosion of austenitic 304 stainless steel
    Chun, CM
    Ramanarayanan, TA
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (05) : B169 - B177
  • [38] Stress Corrosion Cracking of a 304 Stainless Steel Elbow
    Guo, Weimin
    Ding, Ning
    Liu, Long
    Xu, Na
    Li, Nan
    Zhang, Feng
    Chen, Lizong
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2020, 20 (02) : 483 - 493
  • [39] Corrosion Resistance of Kolsterised Austenitic 304 Stainless Steel
    Abudaia, F. B.
    Khalil, E. O.
    Esehiri, A. F.
    Daw, K. E.
    4TH INTERNATIONAL CONGRESS IN ADVANCES IN APPLIED PHYSICS AND MATERIALS SCIENCE (APMAS 2014), 2015, 1653
  • [40] Influence of Lactoserum on the corrosion of 'AISI 304' stainless steel
    Zumelzu, E.
    Cabezas, C.
    Matamala, R.
    Journal of Food Science and Technology, 2001, 38 (02) : 145 - 148