A practical methodology to select fretting palliatives: Application to shot peening, hard chromium and WC-Co coatings

被引:24
|
作者
Kubiak, K
Fouvry, S
Marechal, AM
机构
[1] Ecole Cent Lyon, CNRS, UMR 5513, Lab Tribol & Dynam Syst, F-69134 Ecully, France
[2] SNCF, F-94407 Vitry Sur Seine, France
关键词
fretting; fatigue; Cr; WC-Co; friction; cracking; wear;
D O I
10.1016/j.wear.2005.01.030
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Considered as a plague for numerous industrial assemblies, fretting, associated to slight oscillatory displacement, is encountered in all quasi-static contacts subjected to vibration. Depending on sliding conditions, cracking or wear damage can be observed. During the past three decades there has been a huge development in surface treatments. Thousands of new surface treatments and coatings are now available. The critical challenge is to evaluate such treatments against fretting loadings. To achieve this objective, a fast fretting methodology has been developed. It consists in quantifying the palliative friction, cracking and wear responses through a very small number of fretting tests. By defining quantitative variables. a normalized polar fretting damage chart approach is introduced. Applied to shot peening, chromium coatings and WC-Co coatings, it demonstrates the potential benefit of a thermal sprayed WC-Co coating. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:367 / 376
页数:10
相关论文
共 27 条
  • [21] Plateholder design for deposition of uniform diamond coatings on WC-Co substrates by microwave plasma CVD for efficient turning application
    Ashkihazi, E. E.
    Sedov, V. S.
    Sovyk, D. N.
    Khomich, A. A.
    Bolshakov, A. P.
    Ryzhkov, S. G.
    Khomich, A. V.
    Vinogradov, D. V.
    Ralchenko, V. G.
    Konova, V. I.
    DIAMOND AND RELATED MATERIALS, 2017, 75 : 169 - 175
  • [22] Comparison of high temperature wear behaviour of plasma sprayed WC-Co coated and hard chromium plated AISI 304 austenitic stainless steel
    Balamurugan, G. M.
    Duraiselvam, Muthukannan
    Anandakrishnan, V.
    MATERIALS & DESIGN, 2012, 35 : 640 - 646
  • [23] Hard and wear-resistant niobium, molybdenum carbide layered coatings on WC-Co tools produced by ion bombardment and cathodic vacuum arc deposition
    Kuleshov, A. K.
    Uglov, V. V.
    Rusalsky, D. P.
    SURFACE & COATINGS TECHNOLOGY, 2020, 395
  • [24] Deposition and characterization of WC-Co hard-metal coatings by high velocity oxy-fuel process combined with dry-ice blasting
    Dong, Shujuan
    Zeng, Jinyan
    Liao, Hanlin
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2017, 64 : 151 - 159
  • [25] Murakami and H2SO4/H2O2 pretreatment of WC-Co hard metal substrates to increase the adhesion of CVD diamond coatings
    Haubner, R.
    Kubelka, S.
    Lux, B.
    Griesser, M.
    Grasserbauer, M.
    Journal De Physique, 1995, 5 (06) : 5 - 753
  • [26] MURAKAMI AND H2SO4/H2O2 PRETREATMENT OF WC-CO HARD METAL SUBSTRATES TO INCREASE THE ADHESION OF CVD DIAMOND COATINGS
    HAUBNER, R
    KUBELKA, S
    LUX, B
    GRIESSER, M
    GRASSERBAUER, M
    JOURNAL DE PHYSIQUE IV, 1995, 5 (C5): : 753 - 760
  • [27] Evaluating the Effect of HVOF Sprayed WC-10Co-4Cr and Hard Chromium Electroplated Coatings on Fatigue Strength of Axle-Shaped Machine Parts
    Phoi Nguyen Vinh
    Ngon Dang Thien
    Cuong Le Chi
    ADVANCES IN ENGINEERING RESEARCH AND APPLICATION, 2019, 63 : 309 - 317