Hydrogen Evolution and Absorption in an API X100 Line Pipe Steel Exposed to Near-Neutral pH Solutions

被引:20
|
作者
Ha, Hung M. [1 ]
Gadala, Ibrahim M. [1 ]
Alfantazi, Akram [1 ,2 ]
机构
[1] Univ British Columbia, Dept Mat Engn, Corros Grp, Vancouver, BC V5Z 1M9, Canada
[2] Petr Inst, Dept Chem Engn, Abu Dhabi, U Arab Emirates
关键词
stress corrosion cracking; line pipe steel; hydrogen embrittlement; hydrogen evolution; hydrogen permeation; STRESS-CORROSION CRACKING; CARBON-DIOXIDE CORROSION; C-MN STEEL; ELECTROCHEMICAL POLARIZATION; CO2-HCO3--CO32-SOLUTIONS; DISSOCIATION-CONSTANTS; CALCAREOUS DEPOSITS; STRAIN-RATE; MILD-STEEL; BEHAVIOR;
D O I
10.1016/j.electacta.2016.03.167
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Hydrogen evolution kinetics and hydrogen absorption in an API X100 line pipe steel exposed to near-neutral pH solutions is studied in this work. At the corrosion potential, dissolved CO2 in the solution accelerates the hydrogen evolution kinetics through the carbonic acid discharge reaction. At potentials more negative than the corrosion potential, hydrogen evolution due to bicarbonate discharge dominates the other cathodic reactions occurring at the ocp. The hydrogen diffusivity in the API X100 steel is found to be approximately 4.4 x 10 x (7) cm(2)/s. A measurable amount of diffusible hydrogen of approximately 1 appm is detected in the steel at the freely corroding condition using an electrochemical hydrogen permeation technique. Higher concentration of diffusible hydrogen is observed at more negative applied potentials as well as at higher CO2 partial pressures. The results in this paper support the attribution of stress corrosion cracking of pipelines in near-neutral pH trapped water environments to hydrogen embrittlement. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:18 / 30
页数:13
相关论文
共 50 条
  • [41] Crack propagation of pipeline steel exposed to a near-neutral pH environment under variable pressure fluctuations
    Yu, Mengshan
    Chen, Weixing
    Kania, Richard
    Van Boven, Greg
    Been, Jenny
    INTERNATIONAL JOURNAL OF FATIGUE, 2016, 82 : 658 - 666
  • [42] Corrosion of X100 pipeline steel under plastic strain in a neutral pH bicarbonate solution
    Xu, L. Y.
    Cheng, Y. F.
    CORROSION SCIENCE, 2012, 64 : 145 - 152
  • [43] Revisiting basic assumptions of the hydrogen evolution reaction (HER) for water electrolysis at near-neutral pH
    Sun, Junzhe
    Etcheverry, Luc
    Bergel, Alain
    CHEMICAL ENGINEERING JOURNAL, 2025, 507
  • [44] Evaluation of electrochemical hydrogen absorption in welded pipe with steel API X52
    Capelle, J.
    Dmytrakh, I.
    Azari, Z.
    Pluvinage, G.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (33) : 14356 - 14363
  • [45] Ductile burst behavior of high pressure X100 steel pipe considering hydrogen damage
    Wang, Huakun
    Wang, Tongyao
    Yang, Sheng
    Gao, Jing
    Yu, Yang
    Tao, Hua-Bing
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2024, 58 : 362 - 379
  • [46] Electrochemical corrosion behavior of X80 pipeline steel in a near-neutral pH solution
    Xue, H. B.
    Cheng, Y. F.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2010, 61 (09): : 756 - 761
  • [47] Mechanical and environmental influences on stress corrosion cracking of an X-70 pipeline steel in dilute near-neutral pH solutions
    Fang, B.
    Han, E.-H.
    Wang, J.
    Ke, W.
    CORROSION, 2007, 63 (05) : 419 - 432
  • [48] Microstructure dependence of stress corrosion cracking initiation in X-65 pipeline steel exposed to a near-neutral pH soil environment
    Chu, R
    Chen, W
    Wang, SH
    King, F
    Jack, TR
    Fessler, RR
    CORROSION, 2004, 60 (03) : 275 - 283
  • [49] Corrosion fatigue and near-neutral pH stress corrosion cracking of pipeline steel and the effect of hydrogen sulfide
    Eadie, RL
    Szklarz, KE
    Sutherby, RL
    CORROSION, 2005, 61 (02) : 167 - 173
  • [50] Fundamentals of hydrogen evolution reaction and its implications on near-neutral pH stress corrosion cracking of pipelines
    Cheng, Y. F.
    ELECTROCHIMICA ACTA, 2007, 52 (07) : 2661 - 2667