Effects of He ion irradiation on the microstructures and mechanical properties of t′ phase yttria-stabilized zirconia ceramics

被引:19
|
作者
Pu, Guo [1 ]
Zou, Jianxiong [1 ]
Lin, Liwei [1 ]
Zhang, Kun [1 ]
Liu, Bo [1 ]
Ma, Fei [2 ]
Wang, Qiangbing [3 ]
Li, Qiran [4 ]
机构
[1] Sichuan Univ, Inst Nucl Sci & Technol, Key Lab Radiat Phys & Technol, Minist Educ, Chengdu 610064, Sichuan, Peoples R China
[2] Xi An Jiao Tong Univ, State Key Lab Mech Behav Mat, Xian 710049, Shaanxi, Peoples R China
[3] Northwest Inst Nonferrous Met Res, State Key Lab Porous Met Mat, Xian, Shaanxi, Peoples R China
[4] INNOVICES SARL, 1 Pl Paul Verlaine, F-92100 Boulogne Billancourt, France
基金
中国国家自然科学基金;
关键词
Yttria-stabilized zirconia ceramic; Spark plasma sintering; Mechanical properties; Phase transformation; Helium ion irradiation; INERT MATRIX; FRACTURE-TOUGHNESS; TRANSFORMATION; BEHAVIOR; ELECTRON; XENON;
D O I
10.1016/j.jallcom.2018.08.259
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The dense ZrO2-8 wt.% Y2O3 ceramics with tetragonal (t') phase were prepared by spark plasma sintering (SPS). The micro-structure modification in poly-crystalline t' phase YSZ ceramics irradiated with 60 KeV He ions over a wide fluence range were studied. It is found that, the t' -> t + c phase transformation was detected for the samples irradiated at the fluence above 2 x 10(17) cm(-2). In addition, a three-steep model for damage stages has been proposed and discussed for interpreting the evolution of mechanical properties of t'-YSZ ceramics after irradiated, mainly revealed by the analysis from HRTEM results. Firstly, as the He+ fluences range from 0.5 x 10(17) cm(-2) to 1 x 10(17) cm(-2), the hardening effects were confirmed in t'-YSZ owing to the irradiation induced defects serve as obstacles to resist slipping of dislocations. As the fluence was increased to 2 x 10(17) cm(-2), the degradation of mechanical properties was evidenced, which could be ascribed to the deterioration effect of aggregated He bubbles inside t' YSZ grains. While the fluence increased to 10 x 10(17) cm(-2), a seriously damaged region was approximately located at 250 nm in depth, at which a great number of He bubbles with different shape and dislocation loops were evidenced, leading to a further reduction of hardness and elastic modulus. No micro-cracks emerge even for He+ fluences as high as 10 x 10(17) cm(-2), indicating high irradiation stability and resistance to micro-crack propagation in t'-YSZ. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:777 / 783
页数:7
相关论文
共 50 条
  • [31] Effects of specimen size and yttria concentration on mechanical properties of single crystalline yttria-stabilized tetragonal zirconia nanopillars
    Zhang, Ning
    Zaeem, Mohsen Asle
    JOURNAL OF APPLIED PHYSICS, 2017, 122 (01)
  • [32] Photoluminescence in yttria-stabilized zirconia of aging effects
    Hachiya, K
    Oku, H
    Kondoh, J
    PHYSICAL REVIEW B, 2005, 71 (06):
  • [33] High temperature mechanical properties of zirconia metastable t′-Phase degraded yttria stabilized zirconia
    Wang, Kai
    Zhao, Meng
    Ren, Xiaorui
    Pan, Wei
    CERAMICS INTERNATIONAL, 2019, 45 (14) : 17376 - 17381
  • [34] THE TRANSPORTED ENTROPY OF OXYGEN ION IN YTTRIA-STABILIZED ZIRCONIA
    RATKJE, SK
    FORLAND, KS
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1991, 138 (08) : 2374 - 2376
  • [35] Preparation of yttria-stabilized tetragonal zirconia ceramics for optical ferrule
    Yang, SH
    Kim, SB
    Kang, BA
    Yun, YH
    Kim, YH
    Hwang, KS
    JOURNAL OF MATERIALS SYNTHESIS AND PROCESSING, 2001, 9 (05) : 275 - 279
  • [36] Synthesis and structural studies of microporous yttria-stabilized zirconia ceramics
    Srinivasan, R
    Sparks, DE
    Milburn, DR
    Davis, BH
    MICROPOROUS AND MACROPOROUS MATERIALS, 1996, 431 : 279 - 284
  • [37] Nanocrystalline Yttria-Stabilized Zirconia Ceramics for Cranial Window Applications
    Xu, Changlu
    Uahengo, Gottlieb
    Rudnicki, Christopher
    Hung, Chengi
    Huang, Aaron
    Xu, Queenie
    Chen, Yiqing
    Halaney, David L.
    Garay, Javier E.
    Mangolini, Lorenzo
    Aguilar, Guillermo
    Liu, Huinan Hannah
    ACS APPLIED BIO MATERIALS, 2022, 5 (06) : 2664 - 2675
  • [38] MECHANICAL LOSS MEASUREMENTS ON YTTRIA-STABILIZED AND CALCIA-STABILIZED ZIRCONIA
    WELLER, M
    JOURNAL OF ALLOYS AND COMPOUNDS, 1994, 211 : 66 - 70
  • [39] Effects of Fe doping on crystalline and optical properties of yttria-stabilized zirconia
    Nakajima, H.
    Itoh, K.
    Kaneko, H.
    Tamaura, Y.
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2007, 68 (10) : 1946 - 1950
  • [40] Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications
    Camposilvan, E.
    Leone, R.
    Gremillard, L.
    Sorrentino, R.
    Zarone, F.
    Ferrari, M.
    Chevalier, J.
    DENTAL MATERIALS, 2018, 34 (06) : 879 - 890